期刊文献+

高硫非调质钢38MnVS6纯净度控制 被引量:2

PURITY CONTROL OF HIGH SULFUR NON QUENCHED AND TEMPERED STEEL 38MnVS6
下载PDF
导出
摘要 介绍了38MnVS6钢的生产工艺流程,针对生产过程中夹杂物超标的问题,进行了一系列的工艺优化。通过优化转炉冶炼工艺、采用合适的精炼渣系、优化钢水增氮工艺、完善连铸保护浇注等措施,38MnVS6钢的纯净度得到大幅提升,夹杂物合格率达到了99.2%,满足了客户的需求。 The production process of 38MnVS6 steel was introduced.Aiming at the excessive inclusions in the production process,a series of process optimization were carried out.By optimizing converter smelting process,adopting appropriate refining slag system,optimizing molten steel nitrogen increasing process and continuous casting protective pouring,the purity of 38MnVS6 steel has been greatly improved,and the qualified rate of inclusions has reached 99.2%,meeting the needs of customers.
作者 莫丹 Mo Dan(HBIS Group Shisteel Company, Shijiazhuang 050031,Hebei)
出处 《河北冶金》 2021年第12期47-50,共4页 Hebei Metallurgy
关键词 38MnVS6 非调质钢 高硫 纯净度 精炼渣 增氮 保护浇注 38MnVS6 non quenched and tempered steel high sulfur purity refining slag nitrogen increasing protective pouring
  • 相关文献

参考文献10

二级参考文献83

共引文献90

同被引文献18

引证文献2

二级引证文献1

相关作者

内容加载中请稍等...

相关机构

内容加载中请稍等...

相关主题

内容加载中请稍等...

浏览历史

内容加载中请稍等...
;
使用帮助 返回顶部