比较个性化钛网与传统钛网在引导骨再生后暴露的系统综述 被引量:4

A systematic review comparing the exposure of customized titanium mesh and conventional titanium mesh after guided bone regeneration
下载PDF
导出
摘要 目的探讨个性化钛网和传统钛网在引导骨再生(guided bone regeneration,GBR后暴露率以及软组织裂开发生的时间点,为GBR提供临床参考。方法由2名独立研究员通过计算机检索PubMed、EMbase、Web of Science和Cochrane 4个数据库所有公开发表的有关GBR术后钛网暴露的文章。本研究选取2011年1月1日至2021年12月31日发表的英文文章。应用Stata16.0对最终符合纳入标准的研究数据进行系统分析。结果共找到962篇文章,对其中9篇进行了定量分析。钛网总暴露率的组合值为0.37(95%CI=0.31~0.42)。亚组分析结果显示,个性化钛网暴露率的组合值为0.20(95%CI=0.13~0.27),传统钛网暴露率的组合值为0.60(95%CI=0.52~0.68)。结论个性化钛网的暴露率低于传统钛网,对GBR精确骨增量提供足够植入空间具有重要意义。 Objective To explore the exposure rate of customized titanium mesh and traditional titanium mesh after guided bone regeneration(GBR)and the time point of soft tissue dehiscence,and to provide clinical reference for GBR.Methods Databases,including PubMed,EMbase,Web of Science and Cochrane Central Register Controlled Trials,were searched by two independent researchers,for published articles on titanium mesh exposure after GBR.This study selected English articles published from January 1st,2011to December 31th,2021.Stata 16.0 software was used to systematically analyze the research data that finally met the inclusion criteria.Results A total of 962 articles were found,and 9 of which were quantitatively analysed.The combined value of the total exposure rate of titanium mesh was 0.37(95%CI=0.31~0.42).The result of subgroup analysis showed that the combined value of the customized titanium mesh exposure rate was 0.20(95%CI=0.13~0.27)and the combined value of the traditional titanium mesh exposure rate was 0.60(95%CI=0.52~0.68).Conclusion The exposure rate of customized titanium mesh is lower than that of traditional titanium mesh,which is of great significance to provide sufficient grafting space for accurate bone reconstruction in GBR.
作者 周立波 宿玉成 李昕茹 张立强 陈德平 Zhou Libo;Su Yucheng;Li Xinru;Zhang Liqiang;Chen Deping(Affiliated stomatological hospital,Jiamusi University,Jiamusi 154000,Heilongjiang,China;Heilongjiang Key Lab of Oral Biomedicine Materials and Clinical Application,Heilongjiang Jiamusi,Experimental Center for Stomatological Engineering,Heilongjiang 154000,China;Beijing Implant Training College,Beijing 100032,China;Dental Implant Center,Peking Union Medical College Hospital,Chinese Academy Of Medical Sciences,Beijing 100032,China;Digital Mesh Beijing Technology Co.,LtD,Shunyi,Beijing 101312,China;Beijing Citident Hospital of Stomatology,Beijing 100032,China)
出处 《中国口腔种植学杂志》 2022年第2期112-118,共7页 Chinese Journal of Oral Implantology
基金 黑龙江省自然科学基金项目(LH2021H108) 黑龙江省教育厅青年人才创新计划项目(UNPYSCT-2020057) 佳木斯大学青年创新人才培养计划项目(JMSUQP2020020)。
关键词 钛网 计算机辅助设计 3D打印 骨增量 暴露 Titanium mesh Computer-aided design Three-dimensional printing Bone regeneration Exposure