摘要
The phosphors of KY_(1-x)(MoO_(4))_(2-y)(WO_(4))y:xLn^(3+)(Ln^(3+)=Tm^(3+),Dy^(3+),Eu^(3+))were synthesized by using a sol-gel method.Then,the crystal structure,luminescence properties,energy transfer,and white emission of the prepared materials were researched.The molar ratio of the anion group on the photoluminescence(PL)emission and excitation intensity were investigated,revealing that the optimum intensity could be obtained by using=3:1.The optimal Dy^(3+) doping concentration of KY(MoO_(4))1.5(WO4)0.5was obtained.In addition,the color-tunable emissions of Dy^(3+)/Eu^(3+)-codoped KY(MoO_(4))1.5(WO4)0.5phosphors were observed because of the effective energy transfer(ET)from Dy^(3+)to Eu^(3+)ions.Finally,by doping appropriate concentrations of Tm^(3+),Dy^(3+),and Eu^(3+)and different concentrations of(WO_(4))^(2-),white light emitting phosphors KY_(0.92)(WO_(4))2:0.01Tm^(3+),0.06Dy^(3+),0.01Eu^(3+)with excellent color-rending properties were obtained.The chromaticity coordinate was calculated as(x=0.3238,y=0.3173),closing to the artificial daylight(D65,x=0.313,y=0.329)illuminant,and which indicates the potential application of near ultraviolet White light-emitting diodes(WLEDs).