SrBi2-χNdχNb2O9(χ=0,0.1,0.2 and 0.4)bismuth layer-structured ferroelectric ceramics were prepared by the solid-state reaction sintering method.The accurate position of Nd element in SrBi2-χNdχNb2O9 ceramics was d...SrBi2-χNdχNb2O9(χ=0,0.1,0.2 and 0.4)bismuth layer-structured ferroelectric ceramics were prepared by the solid-state reaction sintering method.The accurate position of Nd element in SrBi2-χNdχNb2O9 ceramics was determined by the X-ray Rietveld method and Synchrotron radiation X-ray absorption fine structure(XAFS)technology.The partial substitution of Nd 3+ for Bi 3+ leads to the decrease in the distortion of NbO6 octahedron for SrBi2-χNdχNb2O9 ceramics and also lowers the piezoelectric properties of SrBi2-χNdχNb2O9 ceramics.Meanwhile,the temperature coefficient of resonant frequency(TCF)decreases when Nd element partially replaces Bi element in SrBi2-χNdχNb2O9 ceramics.展开更多
基金Project(20080440083)supported by China Postdoctoral Science FoundationProject(2007CB924901)supported by the National Basic Research Program of China+1 种基金Project(60677022)supported by the National Natural Science Foundation of ChinaProject(09ZR1409200)supported by the Natural Science Foundation of Shanghai,China
文摘SrBi2-χNdχNb2O9(χ=0,0.1,0.2 and 0.4)bismuth layer-structured ferroelectric ceramics were prepared by the solid-state reaction sintering method.The accurate position of Nd element in SrBi2-χNdχNb2O9 ceramics was determined by the X-ray Rietveld method and Synchrotron radiation X-ray absorption fine structure(XAFS)technology.The partial substitution of Nd 3+ for Bi 3+ leads to the decrease in the distortion of NbO6 octahedron for SrBi2-χNdχNb2O9 ceramics and also lowers the piezoelectric properties of SrBi2-χNdχNb2O9 ceramics.Meanwhile,the temperature coefficient of resonant frequency(TCF)decreases when Nd element partially replaces Bi element in SrBi2-χNdχNb2O9 ceramics.