Understanding the corrosion of Mg alloys in in vitro urinary tract conditions: A step forward towards a biodegradable metallic ureteral stent
1
作者 Margarida Pacheco ivo m.aroso +7 位作者 Joana M.Silva Sviatlana V.Lamaka Jan Bohlen Maria Nienaber Dietmar Letzig Estêvão Lima Alexandre A.Barros Rui L.Reis 《Journal of Magnesium and Alloys》 SCIE EI CAS CSCD 2023年第11期4301-4324,共24页
Ureteral stents play a fundamental role in modern time urology. However, following the deployment, stent-related symptoms are frequent and affect patient health and quality of life. Using biodegradable metals as urete... Ureteral stents play a fundamental role in modern time urology. However, following the deployment, stent-related symptoms are frequent and affect patient health and quality of life. Using biodegradable metals as ureteral stent materials have emerged as a promising strategy, mainly due to the improved radial force and slower degradation rate expected. Therefore, this study aimed to characterize different biodegradable metals in urinary tract environment to understand their propensity for future utilization as base materials for ureteral stents. The corrosion of 5 Mg alloys - AZ31, Mg-1Zn, Mg-1Y, pure Mg, and Mg-4Ag - under simulated urinary tract conditions was accessed. The corrosion layer of the different alloys presented common elements, such as Mg(OH)_(2), MgO, and phosphate-containing products, but slight variations in their chemical compositions were detected. The corrosion rate of the different metals varied, which was expected given the differences in the corrosion layers. On top of this, the findings of this study highlighted the significant differences in the samples' corrosion and corrosion layers when in stagnant and flowing conditions. With the results of this study, we concluded that Mg-1Zn and Mg-4Ag presented a higher propensity for localized corrosion, probably due to a less protective corrosion layer;Mg-4Ag corroded faster than all the other four alloys,and Mg-1Y stood out due to its distinct corrosion pattern, that showed to be more homogeneous than all the other four samples, making this one more attractive for the future studies on biodegradable metals. 展开更多
关键词 Biodegradable metals Magnesium alloys Localized corrosion Biodegradable metallic ureteral stent
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部