作者 pan jin-qi ZHANG Wen-cong +2 位作者 YANG Jian-lei CHEN Wen-zhen CUI Guo-rong 《Journal of Central South University》 SCIE EI CAS CSCD 2021年第8期2307-2319,共13页
In this paper,the 2.6 vol%TiBw/Ti6Al4V composites with network architecture were fabricated by hot press sintering(HPS)at 1100℃ for 1 h,and the quantitative relationships between phases and heat treatment temperature... In this paper,the 2.6 vol%TiBw/Ti6Al4V composites with network architecture were fabricated by hot press sintering(HPS)at 1100℃ for 1 h,and the quantitative relationships between phases and heat treatment temperatures were established.The results showed that the volume fraction phases changed linearly with a range of solution temperature(930-1010℃)and aging temperature(400-600℃).Moreover,the composites with equiaxed microstructure were obtained due to the static recrystallization after solution treated at 950℃ for 1 h and aging treated at 600℃ for 12 h.The ultimate high temperature tensile strengths were 772,658,392 and 182 MPa,and the elongations were 9.1%,12.5%,28.6%and 35.3%at 400,500,600 and 700℃,respectively.In addition,fractured morphology analysis indicated the excellent strengthening effect of TiBw at a temperature below 600℃.However,the strengthening effect was significantly reduced due to the debonding of matrix and TiBw at 700℃ and caused the cracks to propagate along the grain boundary. 展开更多
关键词 titanium matrix composites(TMCs) heat treatment mechanical properties microstructure evolution
下载PDF
上一页 1 下一页 到第
使用帮助 返回顶部