Relaxor ferroic dielectrics have garnered increasing attention in the past decade as promising materials for energy storage.Among them,relaxor antiferroelectrics(AFEs)and relaxor ferroelectrics(FEs)have shown great pr...Relaxor ferroic dielectrics have garnered increasing attention in the past decade as promising materials for energy storage.Among them,relaxor antiferroelectrics(AFEs)and relaxor ferroelectrics(FEs)have shown great promise in term of high energy storage density and efficiency,respectively.In this study,a unique phase transition from relaxor AFE to relaxor FE was achieved for the first time by introducing strong-ferroelectricity BaTiO_(3)into NaNbO_(3)-BiFeO_(3)system,leading to an evolution from AFE R hierarchical nanodomains to FE polar nanoregions.A novel medium state,consisting of relaxor AFE and relaxor FE,was identified in the crossover of 0.88NaNbO_(3)–0.07BiFeO_(3)–0.05BaTiO_(3)ceramic,exhibiting a distinctive core-shell grain structure due to the composition segregation.By harnessing the advantages of high energy storage density from relaxor AFE and large efficiency from relaxor FE,the ceramic showcased excellent overall energy storage properties.It achieved a substantial recoverable energy storage density W_(rec)~13.1 J/cm^(3)and an ultrahigh efficiencyη~88.9%.These remarkable values shattered the trade-off relationship typically observed in most dielectric capacitors between W_(rec)andη.The findings of this study provide valuable insights for the design of ceramic capacitors with enhanced performance,specifically targeting the development of next generation pulse power devices.展开更多
基金financially supported by the National Natural Science Foundation of China(Nos.52172181,22105017)Interdisciplinary Research Project for Young Teachers of USTB(No.FRFIDRY-21–002)。
文摘Relaxor ferroic dielectrics have garnered increasing attention in the past decade as promising materials for energy storage.Among them,relaxor antiferroelectrics(AFEs)and relaxor ferroelectrics(FEs)have shown great promise in term of high energy storage density and efficiency,respectively.In this study,a unique phase transition from relaxor AFE to relaxor FE was achieved for the first time by introducing strong-ferroelectricity BaTiO_(3)into NaNbO_(3)-BiFeO_(3)system,leading to an evolution from AFE R hierarchical nanodomains to FE polar nanoregions.A novel medium state,consisting of relaxor AFE and relaxor FE,was identified in the crossover of 0.88NaNbO_(3)–0.07BiFeO_(3)–0.05BaTiO_(3)ceramic,exhibiting a distinctive core-shell grain structure due to the composition segregation.By harnessing the advantages of high energy storage density from relaxor AFE and large efficiency from relaxor FE,the ceramic showcased excellent overall energy storage properties.It achieved a substantial recoverable energy storage density W_(rec)~13.1 J/cm^(3)and an ultrahigh efficiencyη~88.9%.These remarkable values shattered the trade-off relationship typically observed in most dielectric capacitors between W_(rec)andη.The findings of this study provide valuable insights for the design of ceramic capacitors with enhanced performance,specifically targeting the development of next generation pulse power devices.