The effect and uptake of copper ion on SBR(sequence batch reactor) biological treatment system was studied. Special nutrient and powder activated carbon(PAC) additive were tested as uptake stimulation technique. Resul... The effect and uptake of copper ion on SBR(sequence batch reactor) biological treatment system was studied. Special nutrient and powder activated carbon(PAC) additive were tested as uptake stimulation technique. Results showed that copper ion had higher effect on unacclimated activated sludge system than on acclimated one. The special nutrient adding could enhance the uptake of copper significantly, while PAC adding could improve the sludge settling and decrease the turbidity of effluent. The variation of bacterial community analyzed by 16S rDNA method showed the acclimation of copper could increase copper resistance species, and excess accumulation could cause some species diminish. It was confirmed that acclimation could improve the resistance and uptake ability of microorganism to heavy metal. 展开更多
关键词 copper ion UPTAKE NUTRIENTS powder activated carbon (PAC) 16S rDNA length polymorphism (LPM)
下载PDF
Effects of continuous casting mould fluxes on reducing longitudinal and star cracks on a slab surface 被引量:1
2
作者 WANGQian WANGYu +4 位作者 CHIJinghao xiebing HEYuming ZHUBing CHENWenman 《Journal of Chongqing University》 CAS 2004年第1期65-68,共4页
In the continuous casting production of medium carbon steel (whose mass fraction of carbon is 0.09 % to 0.16 %) and high strength low alloy steel (whose mass fraction of Mn is 0.90 % to 1.40 %), flecks occurring the m... In the continuous casting production of medium carbon steel (whose mass fraction of carbon is 0.09 % to 0.16 %) and high strength low alloy steel (whose mass fraction of Mn is 0.90 % to 1.40 %), flecks occurring the most often are usually longitudinal and star cracks. In additional to the employment of a galvanized plate mould, two kinds of fluxes with special properties were studied and used to harmonize the conflicts between the function of heat transfer and lubrication. An industrial application revealed that the crystallizing temperature (Tc) and crystal ratio (R) of fluxes have a crucible effect on impeding the occurrence of above defects on a slab surface. In the case of slab section (180 to 240) mm(1000 to 1400) mm and casting speed Vc of (0.7 to 1.2) m/min, the optimized parameters of fluxes are Tc of (1170 to 1190) ℃, R of 80 % to 95 % for medium carbon steel, and Tc of (1100 to 1150) ℃, plus R of 40 % to 60 % for high strength low alloy steel. 展开更多
关键词 continuous casting mould flux star crack longitudinal crack