Al2O3 dispersion-strengthened copper alloy was prepared by reactive synthesis and spark plasma sintering(SPS) process. Studies show that nano-sized c-Al2O3 particles with 27.4 nm mean size and 50-nm interval are hom...Al2O3 dispersion-strengthened copper alloy was prepared by reactive synthesis and spark plasma sintering(SPS) process. Studies show that nano-sized c-Al2O3 particles with 27.4 nm mean size and 50-nm interval are homogeneously distributed in copper matrix. The density of SPS alloy is about 99 %, meanwhile, the electrical conductivity of sintered alloy is 72 % IACS and the Rockwell hardness can reach to HRB 91.展开更多
基金financially supported by the National Natural Science Foundation of China (No. 5043202)
文摘Al2O3 dispersion-strengthened copper alloy was prepared by reactive synthesis and spark plasma sintering(SPS) process. Studies show that nano-sized c-Al2O3 particles with 27.4 nm mean size and 50-nm interval are homogeneously distributed in copper matrix. The density of SPS alloy is about 99 %, meanwhile, the electrical conductivity of sintered alloy is 72 % IACS and the Rockwell hardness can reach to HRB 91.