Si调控Cu-20Sn-15Ti钎料显微组织与性能的演变行为
1
作者 张黎燕 杜全斌 +5 位作者 毛望军 崔冰 李昂 王蕾 纠永涛 梁杰 《金刚石与磨料磨具工程》 CAS 北大核心 2024年第3期309-318,共10页
为通过成分调控改善Cu-Sn-Ti钎料的显微组织及性能,采用扫描电子显微镜、X射线衍射仪及EDS能谱分析等设备,研究了Si对Cu-20Sn-15Ti钎料显微组织与性能的影响规律。结果表明:Cu-20Sn-15Ti钎料的显微组织为大尺寸多边形状CuSn_(3)Ti_(5)... 为通过成分调控改善Cu-Sn-Ti钎料的显微组织及性能,采用扫描电子显微镜、X射线衍射仪及EDS能谱分析等设备,研究了Si对Cu-20Sn-15Ti钎料显微组织与性能的影响规律。结果表明:Cu-20Sn-15Ti钎料的显微组织为大尺寸多边形状CuSn_(3)Ti_(5)相、共晶组织和α-Cu相。添加少量的Si(质量分数≤2.0%)可细化钎料中多边形状CuSn_(3)Ti_(5)相,并生成小尺寸Si_(3)Ti_(5)相,较多的Si(质量分数≥3.0%)会造成多边形状CuSn_(3)Ti_(5)相分化离散、共晶组织粗化减少,Si_(3)Ti_(5)相含量增加且粗化,当Si含量增至5.0%时,钎料不再生成多边形状CuSn_(3)Ti_(5)相和共晶组织,Ti主要用于生成Ti_(5)Si_(3)相,显微组织主要为Ti_(5)Si_(3)相、α-Cu相、Cu41Sn11相和少量条状CuSn_(3)Ti_(5)相;与Cu、Sn相比,Si与Ti具有更强的化学亲和力,Si优先与Ti反应生成Ti_(5)Si_(3)相;Ti_(5)Si_(3)相的三维组织形貌为棱柱状,且呈团聚附生特征,粗条状Ti_(5)Si_(3)相具有中心或侧面孔洞缺陷,孔洞的形成主要与其生长机制有关;随着Si含量的增加,钎料的剪切强度呈“升高-降低-升高”的趋势,断口形貌由准解理断裂和解理断裂的混合形态向解理断裂转变;CuSn_(3)Ti_(5)相易破碎开裂成为起裂源,不同粗大状态CuSn_(3)Ti_(5)相的存在均在一定程度上恶化钎料剪切强度。 展开更多
关键词 Cu-Sn-ti钎料 金刚石 显微组织 CuSn_(3)ti_(5)相
下载PDF
退火工艺对Ti-Ni-V形状记忆合金相变和形变行为的影响
2
作者 张伟 贺志荣 安明宇 《材料热处理学报》 CAS CSCD 北大核心 2024年第7期60-68,共9页
利用差示扫描量热仪和拉伸试验研究了400℃×10~120 min和500℃×10~120 min退火态Ti-50.8Ni-0.5V合金的相变行为、拉伸性能和形状记忆行为。结果表明:随退火温度和时间变化,合金的相变类型、R相变温度T_(R)和热滞ΔT_(R)、马... 利用差示扫描量热仪和拉伸试验研究了400℃×10~120 min和500℃×10~120 min退火态Ti-50.8Ni-0.5V合金的相变行为、拉伸性能和形状记忆行为。结果表明:随退火温度和时间变化,合金的相变类型、R相变温度T_(R)和热滞ΔT_(R)、马氏体相变温度T_(M)和热滞ΔT_(M)、抗拉强度R_(m)、伸长率A、应力诱发马氏体相变临界应力σ_(M)、加载-卸载残余应变ε_(R)和能耗W_(D)的变化规律如下:400和500℃退火态Ti-50.8Ni-0.5V合金皆发生B2→R→B19’/B19’→R→B2(B2-母相,CsCl型结构;R-R相,菱方结构;B19’-马氏体相,单斜结构)型相变;T_(R)^(400℃)>T_(R)^(500℃),T_(M)^(500℃)>T_(M)^(400℃),ΔT_(M)^(400℃)>ΔT_(M)^(500℃)≥ΔT_(R)^(400℃)≈ΔT_(R)^(500℃)≈4℃;R_(m)^(400℃)>R_(m)^(500℃),A^(500℃)>A^(400℃);400℃退火态合金的超弹性(SE)稳定性高于500℃退火态合金。随退火时间延长,T_(R)^(400℃)、T_(R)^(500℃)、T_(M)^(400℃)和T_(M)^(500℃)升高,ΔT_(M)^(400℃)和ΔT_(M)^(500℃)减小,ΔT_(R)^(400℃)和ΔT_(R)^(500℃)在3.5~4.6℃之间变化;400℃退火态合金保持SE,500℃退火态合金由SE向SE+SME(形状记忆效应)转变;σ_(M)^(400℃)和σ_(M)^(500℃)降低;W_(D)^(400℃)和W_(D)^(500℃)增加;ε_(R)^(500℃)先降后升;ε_(R)^(400℃)在0.64%~1.36%之间变化。要使Ti-50.8Ni-0.5V合金获得较高的T_(R),可对其进行400℃退火;要使该合金获得较高的T_(M),可对其进行500℃退火;要使该合金在室温下获得超弹性,可对其进行400℃×10~120 min或500℃×10~60 min退火。 展开更多
关键词 ti-Ni-V合金 形状记忆合金 退火工艺 相变 形变
原文传递
烧结法制备Al-Ti-B中间合金粉体
3
作者 王开 张念炳 +1 位作者 甄晓峰 曾令鹤 《有色金属(冶炼部分)》 CAS 北大核心 2024年第5期100-104,共5页
采用TiO_(2)粉、CaO、Al粉和B_(2)O_(3)为原料,经混匀、压片、烧结后,制备出了Al-Ti-B中间合金粉末。利用XRD、SEM-EDS、XPS等表征手段,对烧结产物的物相组成、微观形貌和原子价态进行分析。结果表明,在钙铝比1.6、钛硼比5、1485℃烧结2... 采用TiO_(2)粉、CaO、Al粉和B_(2)O_(3)为原料,经混匀、压片、烧结后,制备出了Al-Ti-B中间合金粉末。利用XRD、SEM-EDS、XPS等表征手段,对烧结产物的物相组成、微观形貌和原子价态进行分析。结果表明,在钙铝比1.6、钛硼比5、1485℃烧结20 min的条件下,烧结产物的主要物相为Al_(3)Ti、TiB_(2)、Al、CaAl_(4)O_(7)和CaAl_(2)O_(4);烧结产物中Al_(3)Ti呈块状,TiB_(2)呈小颗粒状,两者均匀分布在铝基体中;TiO_(2)在反应中存在逐级还原的现象。烧结法可以制备出Al-Ti-B中间合金粉体。 展开更多
关键词 AL-ti-B中间合金 Al_(3)ti tiB_(2)相 烧结法
下载PDF
铸态Ti-6Al-xMo合金的微观组织和力学性能
4
作者 郭依航 景然 +4 位作者 刘以柔 吴倩 刘禹驰 李江华 炊鹏飞 《材料热处理学报》 CAS CSCD 北大核心 2024年第10期42-49,共8页
通过非自耗真空电弧熔炼炉制备了铸态Ti-6Al-xMo(x=0、4、8、12、16和20 mass%)合金,采用X射线衍射仪(XRD)、光学显微镜(OM)、扫描电镜(SEM)、硬度测试和压缩实验等研究了不同Mo元素含量的Ti-6Al-xMo合金的微观组织和力学性能。结果表明... 通过非自耗真空电弧熔炼炉制备了铸态Ti-6Al-xMo(x=0、4、8、12、16和20 mass%)合金,采用X射线衍射仪(XRD)、光学显微镜(OM)、扫描电镜(SEM)、硬度测试和压缩实验等研究了不同Mo元素含量的Ti-6Al-xMo合金的微观组织和力学性能。结果表明:随着Mo元素含量的增加,合金发生了α→α′+β→α″+β→β的相变过程。Ti-6Al合金显微组织由分布不均匀的片状α相组成。当Mo元素含量为4 mass%时,合金中出现明显的β晶界和细针状的α′马氏体相;当Mo元素含量增加至12 mass%时,合金中出现细针状的α″马氏体相和不连续的亚晶界;当Mo元素含量增加至16 mass%以上时,合金组织由粗大等轴β晶粒组成。铸态Ti-6Al合金的应力-应变曲线呈现“PLC效应”;Ti-6Al-16Mo和Ti-6Al-20Mo合金的压缩塑性超过50%仍未断裂,表现出良好的塑性;断口形貌表明添加Mo元素后所有合金均为韧性断裂。 展开更多
关键词 ti-6Al-xMo合金 相结构 显微组织 力学性能
原文传递
增材制造Ti基复合材料的研究进展
5
作者 宫书林 张煜 +2 位作者 宋美慧 李岩 李艳春 《黑龙江科学》 2024年第16期27-31,共5页
随着航空航天、汽车工业等领域的快速发展,Ti基复合材料(TMCs)因其高强度、低密度、高温耐久性和优异的耐磨性而受到广泛的关注,通过增材制造技术制备的Ti基复合材料有着广泛的应用前景。在Ti基材料中添加合适的强化相可改变复合材料的... 随着航空航天、汽车工业等领域的快速发展,Ti基复合材料(TMCs)因其高强度、低密度、高温耐久性和优异的耐磨性而受到广泛的关注,通过增材制造技术制备的Ti基复合材料有着广泛的应用前景。在Ti基材料中添加合适的强化相可改变复合材料的微观结构和性能。介绍了几种常用的增材制造方法及其特点,包括选区激光熔化(SLM)、激光金属沉积技术(LMD)、电子束熔化技术(EBM)和激光近净成形技术(LENS),综述了通过原位反应生成和直接添加强化相对Ti基复合材料的影响,为进一步研究增材制造增强钛合金及复合材料性能提供了理论依据。 展开更多
关键词 增材制造 ti基复合材料 强化相 力学性能
下载PDF
等温温度对Ti-Mo微合金高强双相钢相变及组织性能的影响
6
作者 何平 王巍 +3 位作者 李群芳 王礼凡 党正卓 胡海江 《材料热处理学报》 CAS CSCD 北大核心 2024年第8期146-153,共8页
采用热模拟实验、光学显微镜、显微硬度仪和透射电镜等研究了等温温度对Ti-Mo微合金高强双相钢相变、组织及性能的影响。结果表明:当等温温度在750~725℃时,实验钢组织主要为马氏体+少量贝氏体或铁素体,随着等温温度降低(≤700℃),铁素... 采用热模拟实验、光学显微镜、显微硬度仪和透射电镜等研究了等温温度对Ti-Mo微合金高强双相钢相变、组织及性能的影响。结果表明:当等温温度在750~725℃时,实验钢组织主要为马氏体+少量贝氏体或铁素体,随着等温温度降低(≤700℃),铁素体含量增多,排碳行为增加了过冷奥氏体的稳定性,抑制了中低温区贝氏体相变,在随后的冷却阶段,过冷奥氏体更倾向转变为马氏体。铁素体与马氏体的显微硬度均随等温温度降低而增加,但进一步降低温度,马氏体硬度基本保持稳定(361 HV0.1);650℃时铁素体显微硬度最高(242 HV0.1),这主要是由于铁素体内部产生了大量细小的相间析出,同时析出强化作用减小了铁素体与马氏体的硬度差异,降低了双相钢强度对马氏体体积分数的依赖性,等温温度较高时,相间析出形成被抑制。 展开更多
关键词 铁素体/马氏体双相钢 ti-Mo微合金钢 等温相变 相间析出 显微硬度
原文传递
Ti对复杂锰黄铜TL-084组织及性能的影响
7
作者 周冠斌 金勃含 +3 位作者 魏作山 张潇 祁复功 丁海民 《机电工程技术》 2024年第7期112-118,共7页
以TL-084锰黄铜为研究对象,在原有黄铜生产工艺的基础上引入不同含量的Ti,结合金相分析、XRD分析和SEM分析等手段对其微观组织进行分析,主要探究不同含量Ti的引入对合金基体及基体中硬质相的形貌、尺寸、分布的影响。同时根据对不同Ti含... 以TL-084锰黄铜为研究对象,在原有黄铜生产工艺的基础上引入不同含量的Ti,结合金相分析、XRD分析和SEM分析等手段对其微观组织进行分析,主要探究不同含量Ti的引入对合金基体及基体中硬质相的形貌、尺寸、分布的影响。同时根据对不同Ti含量TL-084锰黄铜的硬度、抗拉强度、耐磨性的测试,探究Ti的引入对合金力学性能的影响。研究发现TL-084黄铜组织的基体为β相,粗大的初生相[Mn(Fe)]_(5)Si_(3)、细小的共晶相Mn_(5)Si_(3)以及在基体中均匀分布的小颗粒状富铅相。在引入Ti元素后,在基体中生成了富Ti相以及以富Ti相为核心的3层核壳结构,对基体中的初生相起到了细化作用,但是基体晶粒反而粗化,随着Ti含量增加到0.3%,基体中产生富Ti相团聚。同时在力学性能上硬度随着Ti元素含量的上升呈先升高后降低的趋势,在添加量为0.2%时其维氏硬度为HV287.2,提升了8.5%;抗拉强度随着随Ti含量的增加也呈现先上升后下降的趋势,其中添加w_(Ti)=0.1%的黄铜棒材的抗拉强度最高,约744.5 MPa,上升了6.75%。 展开更多
关键词 TL-084黄铜 ti 硬质相 力学性能
下载PDF
一种针对TI-ADC的采样时钟相位失配数字校准技术
8
作者 黄尚恩 施娟 +1 位作者 蒋丽 韦雪明 《桂林电子科技大学学报》 2024年第2期174-180,共7页
针对采样时钟偏移失配对多相时间交织采样模数转换器(TI-ADC)性能影响很大的问题,将采样通道输出进行互相关,并利用一阶泰勒展开式进行自适应补偿校准的相位误差提取技术,有效补偿了多通道时序失配。基于65 nm CMOS工艺设计了一种12 bit... 针对采样时钟偏移失配对多相时间交织采样模数转换器(TI-ADC)性能影响很大的问题,将采样通道输出进行互相关,并利用一阶泰勒展开式进行自适应补偿校准的相位误差提取技术,有效补偿了多通道时序失配。基于65 nm CMOS工艺设计了一种12 bit 1.6 GS/s八相TI-ADC的采样相位失配校准电路。当输入信号频率为626.5625 MHz时,校准后的TIADC有效位数提升了6.29 bit,信噪失真比提升38.1 dB,无杂散动态范围提升44.44 dB。设计结果表明,本技术结构简单,硬件资源消耗少,能够显著提高TI-ADC系统采样性能。 展开更多
关键词 ti-ADC 相位偏移失配 互相关 一阶泰勒 自适应校准
下载PDF
Ti-Si-Fe添加量与氮气压强对BN/SiC/Si_(3)N_(4)复相陶瓷材料的影响
9
作者 李立倍 张锦化 +6 位作者 冯邻江 张祖力 龙图 陈祥惠 周寻 徐晟 李灵转 《陶瓷学报》 CAS 北大核心 2024年第3期575-583,共9页
以BN粉、Si粉、SiC粉、Ti-Si-Fe合金、助烧剂B_(2)O_(3)及外加结合剂酚醛树脂(PFF)为原料,采用原位氮化反应烧结制备BN/SiC/Si_(3)N_(4)复相陶瓷材料。探讨了在氮气气氛中添加不同含量Ti-Si-Fe合金部分替代硅粉及不同的气压下制得试样... 以BN粉、Si粉、SiC粉、Ti-Si-Fe合金、助烧剂B_(2)O_(3)及外加结合剂酚醛树脂(PFF)为原料,采用原位氮化反应烧结制备BN/SiC/Si_(3)N_(4)复相陶瓷材料。探讨了在氮气气氛中添加不同含量Ti-Si-Fe合金部分替代硅粉及不同的气压下制得试样的力学性能差异。结果表明,Ti-Si-Fe合金中的Fe、Mn等元素促进了硅粉的氮化和氮化硅晶须的生长,所有的氮化产物均可以更好地填充气孔并提高试样的致密化程度以及调控材料的力学性能。当Ti-Si-Fe合金添加量为1.5 wt.%时,常压下试样的显气孔率最低为25.3%、体积密度最高为1.97 g·cm^(-3),常温抗弯强度最高为33.8 MPa;气压下试样的显气孔率最低为20.8%,体积密度最高为2.15 g·cm^(-3),常温抗弯强度最高为43.4 MPa。与常压相比,2 MPa气氛压力烧成的试样,纤维状的Si_(3)N_(4)晶须明显偏少,柱状的Si_(3)N_(4)晶须明显偏多。 展开更多
关键词 氮化硅 ti-Si-Fe合金 反应烧结 显微结构 物相组成
下载PDF
Metallurgical Microstructure Complexity in the Electron Beam Welding (EBW) Joint of Ti6246
10
作者 Daniel Moreno Yohanan Nachmana +5 位作者 Roei Saraga Tal Rokah Denis Panchenco Michael Mansano Elinor Itzhaky Moshe Shapira 《Journal of Minerals and Materials Characterization and Engineering》 2024年第2期100-111,共12页
Electron Beam Welding (EBW) is employed to both melt and unite materials, influencing their thermal history and subsequently determining the microstructure and properties of the welded joint. Welding Titanium alloys i... Electron Beam Welding (EBW) is employed to both melt and unite materials, influencing their thermal history and subsequently determining the microstructure and properties of the welded joint. Welding Titanium alloys involves undergoing local melting and rapid solidification, subjecting the material to thermal stresses induced by a thermal expansion coefficient of 9.5 × 10 m/m°C. This process, reaching range temperatures from the full melting alloy to room temperature, results in phase formation dictated by the thermodynamic preferences of the alloyed elements, posing a significant challenge. Recent efforts in simulation and calculations have been undertaken elsewhere to address this challenge. This study focuses on a joint of two plates with differing cross-sectional areas, influencing heat transfer during welding. This report presents a case study focusing on the metallurgical changes observed in the microstructure within the welded zone, emphasizing alterations in the cooling rate of the welded joint. The investigation utilizes optical metallography, Vickers’s Hardness testing, and SEM (scanning electron microscopy) to comprehensively characterize the observed changes in addition to heat transfer simulation of the welded zone. 展开更多
关键词 ti Alloys WELDING phase Formation HARDNESS METALLOGRAPHY
下载PDF
冷轧Ti-50.8Ni-0.4V形状记忆合金相变和超弹性研究
11
作者 石海洋 张青来 +2 位作者 韩伟东 柏秋生 刘志强 《热加工工艺》 北大核心 2024年第17期101-106,共6页
利用金相显微镜、示差量热分析法和拉伸试验对比研究了冷轧和退火态Ti-50.8Ni-0.4V合金的相变及超弹性。结果表明:退火处理对冷轧合金的相变和超弹性(SE)特性具有显著的影响。具有大量位错塞积的冷轧态合金表现为线性SE,而退火态合金呈... 利用金相显微镜、示差量热分析法和拉伸试验对比研究了冷轧和退火态Ti-50.8Ni-0.4V合金的相变及超弹性。结果表明:退火处理对冷轧合金的相变和超弹性(SE)特性具有显著的影响。具有大量位错塞积的冷轧态合金表现为线性SE,而退火态合金呈非线性SE,350~550℃退火态合金表现为两步相变(A→R→M/M→R→A),形状回复率Rr达到96%,具有优异SE特性。600℃和650℃退火态合金发生完全再结晶,随温度的升高R相逐渐消失,其相变分别为(A→R→M)/(M→A)和(A→M)/(M→A),形状回复率Rr值<29%,其SE特性明显变差。 展开更多
关键词 ti-50.8Ni-0.4V合金 冷轧 力学性能 超弹性 相变 退火
原文传递
层间孔道扩张结构Ti-MWW分子筛的合成及其在环己烯环氧化反应中的应用
12
作者 郭舒隽 李欣澳 +2 位作者 胡元 郑笑笑 李德晶 《井冈山大学学报(自然科学版)》 2024年第4期27-34,共8页
制备具有更大反应通道的Ti-MWW分子筛,可以极大地解决大分子化合物在孔道中的扩散问题,进而提高催化反应的活性。目前通过研究开发了一种新的合成方法,用于合成具有层间孔道扩张结构的Ti-MWW分子筛,将气相二氧化硅、硼酸、六氟钛酸/过... 制备具有更大反应通道的Ti-MWW分子筛,可以极大地解决大分子化合物在孔道中的扩散问题,进而提高催化反应的活性。目前通过研究开发了一种新的合成方法,用于合成具有层间孔道扩张结构的Ti-MWW分子筛,将气相二氧化硅、硼酸、六氟钛酸/过氧化氢和四乙基氢氧化铵溶液混合后蒸干制备干凝胶。用干凝胶转换法合成出Ti-MWW前驱体,通过酸洗焙烧得到Ti-MWW分子筛。使用XRD、TEM及BET的表征手段确定Ti-MWW层间扩张结构和额外的介孔结构的存在,原位生成的MWW片状前驱体上层间的硅羟基与过氧钛酸物种的缩合是形成扩张结构的原因。主要是具有更大的反应通道,相比于传统的Ti-MWW,其在使用过氧化氢为氧化剂的环己烯环氧化中转化率从5.46%增加至12.7%,环氧环己烷的选择性也增加至49.5%。尤其是使用TBHP为氧化剂时,环氧环己烷的选择性进一步提高至80.5%。 展开更多
关键词 层间修饰 液相环氧化 ti-MWW分子筛
下载PDF
热处理对富锆α型TiZrAl合金组织和性能的影响
13
作者 傅霄云 武保林 +3 位作者 徐再东 万刚 李洲 李健博 《材料工程》 EI CAS CSCD 北大核心 2024年第10期106-116,共11页
针对2种富锆α型钛合金(Ti_(60)Zr_(40))_(97)Al_(3)(质量分数/%,下同)和(Ti_(50))Zr_(50)_(97)Al_(3),利用光学显微镜(OM)、差示扫描量热仪(DSC)、X射线衍射仪(XRD)、扫描电子显微镜(SEM)及室温拉伸等实验手段,分析研究了不同热处理工... 针对2种富锆α型钛合金(Ti_(60)Zr_(40))_(97)Al_(3)(质量分数/%,下同)和(Ti_(50))Zr_(50)_(97)Al_(3),利用光学显微镜(OM)、差示扫描量热仪(DSC)、X射线衍射仪(XRD)、扫描电子显微镜(SEM)及室温拉伸等实验手段,分析研究了不同热处理工艺下2种合金的组织和性能。结果表明,经850℃/40 min退火后,合金为α网篮组织,并在α相间留有少量网状β相;经850℃/40 min水冷淬火,形成细针状α'马氏体;经850℃/40 min淬火+600℃/4h时效后,在淬火中形成的细小针状α'马氏体转变成α相,然而马氏体转变不完全,形成α+α'_(remain)组织。T40Z3A合金的拉伸屈服强度可达1100 MPa,并具有7%良好的伸长率;T50Z3A合金虽然具有更高的强度,但其塑性较差。分析表明,由于更高的Zr含量,T50Z3A合金在退火后具有更多的网状β相、淬火时效后具有更多残留α'马氏体相,导致其抗拉强度较高、塑性较差。 展开更多
关键词 钛锆合金 退火 淬火时效 相转变 组织 力学性能
下载PDF
时效处理对Ni-Ti-La合金微结构、相变及力学性能的影响
14
作者 王晶 李维雅 赵春旺 《内蒙古工业大学学报(自然科学版)》 2024年第1期18-22,共5页
时效处理是调节合金微结构,影响合金性能的有效方法。用实验的方法分析了Ni-Ti-La合金的微结构,研究了合金的相变行为,测定了合金的维氏硬度。实验结果表明,用La元素替代Ni元素形成的Ti_(50)Ni_(49.5)La_(0.5)合金,经时效处理后合金由N... 时效处理是调节合金微结构,影响合金性能的有效方法。用实验的方法分析了Ni-Ti-La合金的微结构,研究了合金的相变行为,测定了合金的维氏硬度。实验结果表明,用La元素替代Ni元素形成的Ti_(50)Ni_(49.5)La_(0.5)合金,经时效处理后合金由NiTi基体、NiLa沉淀相和Ti_(2)Ni沉淀相组成,并且沉淀相的数量随着时效温度升高而减少,合金在加热和冷却的过程中均为一步相变B2↔B19',合金相变开始温度随时效温度的升高而增大,合金的硬度随时效温度的升高而增大。用La元素替代Ti元素形成的Ti_(49.5)Ni_(50)La_(0.5)合金,经时效处理后合金由NiTi基体、NiLa沉淀相组成,并且沉淀相的数量随时效温度的升高而增加,合金在加热和冷却的过程中呈现一步相变B2↔B19',相变开始温度随时效温度的升高而增大,合金的维氏硬度随时效温度的升高而减小。时效处理对Ti_(50)Ni_(49.5)La_(0.5)合金和Ti_(49.5)Ni_(50)La_(0.5)合金的微结构产生了影响,进而影响了合金的相变行为和力学性能。 展开更多
关键词 Ni-ti-La合金 微观结构 相变行为 维氏硬度 时效处理
下载PDF
高熵合金/陶瓷在Ti(C,N)基金属陶瓷中的研究现状与展望
15
作者 刘超 姚兴旺 +4 位作者 董涛 龙宁华 张卫兵 李剑峰 曾瑞霖 《硬质合金》 CAS 2024年第4期267-275,共9页
Ti(C,N)基金属陶瓷因其具有良好的硬度、耐磨性和化学稳定性,成为制造业中不可或缺的关键材料,进一步提高金属陶瓷材料的强韧性对扩大其应用领域和应用规模具有十分重要的意义。本文阐述了Ti(C,N)基金属陶瓷的相结构特点,并重点综述了... Ti(C,N)基金属陶瓷因其具有良好的硬度、耐磨性和化学稳定性,成为制造业中不可或缺的关键材料,进一步提高金属陶瓷材料的强韧性对扩大其应用领域和应用规模具有十分重要的意义。本文阐述了Ti(C,N)基金属陶瓷的相结构特点,并重点综述了高熵合金/陶瓷在Ti(C,N)基金属陶瓷的黏结相和添加相成分设计和制备中的应用。对高熵合金/陶瓷在金属陶瓷的主要研究方向进行了总结展望:在Ti(C,N)基金属陶瓷中加入高熵合金黏结相后组织的演变和对材料性能的影响机理需进一步研究;同时高熵陶瓷添加相在Ti(C,N)基金属陶瓷中的作用及机理也是一个重要的研究方向。 展开更多
关键词 ti(C N)基金属陶瓷 高熵合金/陶瓷 黏结相 添加相
原文传递
中碳CrMo钢中Ti、Nb液析形貌及生成机理分析 被引量:1
16
作者 蒋乔 张健 倪燕红 《特殊钢》 2024年第2期18-23,共6页
通过观察微合金Ti、Nb、V在42CrMo钢连铸坯中的液析形貌,以及液析经加热轧制后的变化,同时,采用热力学计算的方式推导液析生成机理。结果表明,在含w[Ti]0.012%、w[Nb]0.030%、w[V]0.030%、w[N]0.003 5%的42CrMo钢410 mm×530 mm连... 通过观察微合金Ti、Nb、V在42CrMo钢连铸坯中的液析形貌,以及液析经加热轧制后的变化,同时,采用热力学计算的方式推导液析生成机理。结果表明,在含w[Ti]0.012%、w[Nb]0.030%、w[V]0.030%、w[N]0.003 5%的42CrMo钢410 mm×530 mm连铸坯中,可观察到Ti、Nb以复合碳氮化物的形式析出,形成微米级液析,w[Ti]较高(70%~83%)的多呈多边形块状,w[Nb]较高(70%~85%)的多呈薄膜状或不规则块状,液析中基本不含V元素;Ti和Nb的碳氮化物液析可互溶并共同生长,Nb含量较高的液析以Ti含量较高的液析为核心长大为块状,部分液析以含硫夹杂物为核心形核并长大;连铸坯心部的碳氮化物液析较多,并且尺寸较大(最长达35μm),连铸坯表面的数量较少,尺寸较小(10μm以下);连铸坯经1 200℃加热并轧制后,液析可部分回溶,数量减少,尺寸减小,并且在轧制过程中破碎。 展开更多
关键词 ti NB CrMo 微合金 中碳钢 液析
下载PDF
冷轧变形对亚稳β型Ti-B20钛合金低温相变行为的影响
17
作者 冀宣名 《材料热处理学报》 CAS CSCD 北大核心 2024年第6期42-52,共11页
采用光学显微镜(OM)、扫描电镜(SEM)、X射线衍射仪(XRD)和透射电镜(TEM)研究了不同状态Ti-B20钛合金在低温时效过程中的相组成及微观组织演变规律,分析了低温时效过程中ω相的形成规律。结果表明:固溶态Ti-B20合金在低温时效时,亚稳β... 采用光学显微镜(OM)、扫描电镜(SEM)、X射线衍射仪(XRD)和透射电镜(TEM)研究了不同状态Ti-B20钛合金在低温时效过程中的相组成及微观组织演变规律,分析了低温时效过程中ω相的形成规律。结果表明:固溶态Ti-B20合金在低温时效时,亚稳β相中优先析出两种取向的等温ω相,时效温度升高至450℃时,ω相消失;合金在冷轧变形过程中形成的位错等晶体缺陷,降低了合金相变的所需能量,促进了ω相形成,缩小了ω相存在温度区间,且变形量越大,促进效果越大。ST试样、CR10试样、CR50试样在350℃时效1 h后的相组成分别为β+ω、β+ω+α和β+α。当β、ω、α同时存在时,它们之间的取向关系为:[011]β∥[2110]ω∥[0001]α。 展开更多
关键词 ti-B20钛合金 冷轧变形 等温ω相 相变行为
原文传递
电子束选区熔化增材制造Ti-55531合金的凝固及相变行为研究
18
作者 张林嘉 张安琴 +2 位作者 常玥莹 高军 邓浩 《大型铸锻件》 2024年第4期28-32,共5页
通过电子束选区熔化(EBM)技术制造了Ti-5Al-5Mo-5V-3Cr-1Zr(Ti-55531)合金,研究了打印过程中的凝固及相变行为。首先样品沿构筑方向形成了粗大的柱状晶,这是因为EBM过程中熔池凝固前沿较低的形核能垒,将导致晶粒的临界形核半径r*趋于0,... 通过电子束选区熔化(EBM)技术制造了Ti-5Al-5Mo-5V-3Cr-1Zr(Ti-55531)合金,研究了打印过程中的凝固及相变行为。首先样品沿构筑方向形成了粗大的柱状晶,这是因为EBM过程中熔池凝固前沿较低的形核能垒,将导致晶粒的临界形核半径r*趋于0,无法生成等轴晶粒。同时凝固方式由平面凝固转为枝晶凝固,较低的等轴枝晶比例使得无法发生柱状晶向等轴晶的转变,在重熔区和定向热流的影响下,晶粒沿构筑方向发生跨层生长成柱状晶。并且沿构筑方向样品的微观组织呈现梯度结构,随着沉积高度的增加,片层初生αp的比例降低,宽度增加,而次生αs的比例升高,这是沿构筑方向的热量累积和基板加热的原位热处理共同作用的结果。 展开更多
关键词 电子束选区熔化 ti55531合金 凝固行为 相变
下载PDF
Ti-48Al-2Cr-2Nb合金在流动电解液中的钝化行为及非线性动力学分析
19
作者 唐卿 王鑫 +2 位作者 李凌 陈年 廖翠姣 《机电工程技术》 2024年第9期275-281,共7页
探究Ti-48Al-2Cr-2Nb合金钝化膜的稳定性和形成过程以提高电解加工中的抗杂散腐蚀。通过循环伏安曲线确定了Ti-48Al-2Cr-2Nb合金的钝化电位,通过相空间重构、递归图及其定量分析确定系统的波动程度和稳定性,并运用形核曲线和功率谱密度... 探究Ti-48Al-2Cr-2Nb合金钝化膜的稳定性和形成过程以提高电解加工中的抗杂散腐蚀。通过循环伏安曲线确定了Ti-48Al-2Cr-2Nb合金的钝化电位,通过相空间重构、递归图及其定量分析确定系统的波动程度和稳定性,并运用形核曲线和功率谱密度分析钝化膜的形成过程。结果表明,Ti-48Al-2Cr-2Nb合金在20% NaNO_(3)溶液中的钝化区间为0~1.8 V,进而依次选取0.8、1.0、1.2、1.4、1.6 V这5个电位的钝化区间,分析动态流场下形核曲线,发现钝化膜的成膜过程主要是扩散的方式控制瞬间形核以及三维生长方式进行,然后通过功率谱密度发现钝化膜的生长过程受到粒子的分形布朗扩散影响。通过分析钝化过程的非线性动力学行为,发现相空间重构的吸引子整体波动程度较小的电位有1.2V和1.4V,且通过递归定量分析,发现1.2V电位下系统具有很强的周期性。 展开更多
关键词 ti-48Al-2Cr-2Nb合金 形核曲线 功率谱密度 相空间重构 递归图
下载PDF
基于TI DSP的永磁同步电机三电阻电流采样的实现
20
作者 侯勇 沈敬祖 《天津科技大学学报》 CAS 2023年第4期35-40,共6页
为实现永磁同步电机(PMSM)的高性能、低成本矢量控制,改进三电阻电流采样法。针对三电阻电流采样法存在非观测区的问题,提出了根据脉冲宽度调制(pulse width modulation,PWM)波形动态设置电流采样点、对PWM进行移相重构电机电流的方法,... 为实现永磁同步电机(PMSM)的高性能、低成本矢量控制,改进三电阻电流采样法。针对三电阻电流采样法存在非观测区的问题,提出了根据脉冲宽度调制(pulse width modulation,PWM)波形动态设置电流采样点、对PWM进行移相重构电机电流的方法,提高母线电压利用率,提升电机控制系统的输出能力。基于德州仪器公司的数字信号处理器(TI DSP)平台实现该方法的软件算法,通过实验验证本文方法的正确性和可靠性。 展开更多
关键词 永磁同步电机控制系统 三电阻电流采样 脉冲宽度调制移相 ti数字信号处理器
下载PDF