Synergistic Use of CO_(2) Pretreatment and Accelerated Carbonation Curing for Maximum Recycling of Steel Slag
1
作者 刘姚君 AN Xiaopeng +2 位作者 LIANG Huichao YU Kexiao WANG Lan 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS CSCD 2023年第3期530-537,共8页
Two carbonation approaches are considered for studying the effects on the hardening mechanisms of slurries made of 100 wt%electric arc furnace steel slag (EAF) slag or 80 wt%EAF slag incorporating 20 wt% of Portland c... Two carbonation approaches are considered for studying the effects on the hardening mechanisms of slurries made of 100 wt%electric arc furnace steel slag (EAF) slag or 80 wt%EAF slag incorporating 20 wt% of Portland cement,which are applied during the hot-stage pretreatment with simulated gas for raw steel slag or the accelerated carbonation curing of slurry.The mechanical strengths,carbonate products,microstructures and CO_(2) uptakes were quantitatively investigated.Results manifest that accelerated carbonation curing increases the compressive strengths of steel slag slurry,from 17.1 MPa (binder of 80 wt% EAF and 20 wt%cement under standard moisture curing) to 36.0 MPa (binder of 80 wt%EAF and 20 wt%cement under accelerated carbonation curing),with a CO_(2) uptake of 52%.In contrast,hot-stage carbonation applied during the pretreatment of steel slag increases the compressive strengths to 43.7 MPa (binder of 80 wt%carbonated EAF and 20 wt%cement under accelerated carbonation curing),with a CO_(2) uptake of 67%.Hotstage carbonation of steel slag is found for particle agglomeration,minerals remodeling and calcite formed,thus causing an activated steel slag with a dense structure and more active components.Accelerated carbonation curing of steel slag slurry paste results in the newly formed amorphous CaCO_(3),calcite crystalline and silica gels that covered the pores of the matrix,facilitating microstructure densification and strength improvement.Adopting the combinative methods of the hot-stage CO_(2) pretreatment and accelerated carbonation curing creates a promising high-volume steel slag-based binder with high strengths and CO_(2) storage. 展开更多
关键词 high-volume steel slag binders hot-stage CO_(2)pretreatment accelerated carbonation curing CO_(2)storage
原文传递
上一页 1 下一页 到第
使用帮助 返回顶部