Greatly enhanced corrosion/wear resistances of epoxy coating for Mg alloy through a synergistic effect between functionalized graphene and insulated blocking layer
1
作者 Z.Y.Xue X.J.Li +3 位作者 J.H.Chu M.M.Li D.N.Zou L.B.Tong 《Journal of Magnesium and Alloys》 SCIE EI CAS CSCD 2024年第1期332-344,共13页
The poor corrosion and wear resistances of Mg alloys seriously limit their potential applications in various industries.The conventional epoxy coating easily forms many intrinsic defects during the solidification proc... The poor corrosion and wear resistances of Mg alloys seriously limit their potential applications in various industries.The conventional epoxy coating easily forms many intrinsic defects during the solidification process,which cannot provide sufficient protection.In the current study,we design a double-layer epoxy composite coating on Mg alloy with enhanced anti-corrosion/wear properties,via the spin-assisted assembly technique.The outer layer is functionalized graphene(FG)in waterborne epoxy resin(WEP)and the inner layer is Ce-based conversion(Ce)film.The FG sheets can be homogeneously dispersed within the epoxy matrix to fill the intrinsic defects and improve the barrier capability.The Ce film connects the outer layer with the substrate,showing the transition effect.The corrosion rate of Ce/WEP/FG composite coating is 2131 times lower than that of bare Mg alloy,and the wear rate is decreased by~90%.The improved corrosion resistance is attributed to the labyrinth effect(hindering the penetration of corrosive medium)and the obstruction of galvanic coupling behavior.The synergistic effect derived from the FG sheet and blocking layer exhibits great potential in realizing the improvement of multi-functional integration,which will open up a new avenue for the development of novel composite protection coatings of Mg alloys. 展开更多
关键词 Mg alloy Functionalized graphene Epoxy coating Corrosion/wear resistance Blocking layer
下载PDF
Adhesive and corrosive wear at microscales in different vapor environments 被引量:3
2
作者 Sihan SHEN Yonggang MENG 《Friction》 SCIE EI CAS 2013年第1期72-80,共9页
Adhesive and corrosive wear at microscales are quantitatively distinguished in lifetime tests of resonant bulk-fabricated silicon microelectromechanical systems(MEMS).By analyzing the oscillation decay characteristics... Adhesive and corrosive wear at microscales are quantitatively distinguished in lifetime tests of resonant bulk-fabricated silicon microelectromechanical systems(MEMS).By analyzing the oscillation decay characteristics in different vapor environments,we find that wear is dominated by asperity adhesion during the initial stages of rubbing in dry N2 or O2/N2 mixtures;in these situations the transient wear rate is inversely proportional to the wear depth.But in water or ethanol vapors,chemical reactions between the corrosive adsorbed layer and the silicon substrate limit the wear rate to a constant.These observations are consistent with atomic explanations.The differences between adhesive and corrosive wear explain the advantages offered by lubricating with alcohol vapors rather than using dry environments for tribo-MEMS devices.Compared to ethanol,the relatively poor anti-wear effect of water vapor is explained by aggressive and rapid tribo-reactions. 展开更多
关键词 adhesive wear corrosive wear microelectromechanical systems(MEMS)
原文传递
Corrosive-wear and Electrochemical Performance of Laser Thermal Sprayed Co30Cr8W1.6C3Ni1.4Si Coating on Ti6Al4V Alloy 被引量:2
3
作者 徐健晏 孔德军 《Journal of Wuhan University of Technology(Materials Science)》 SCIE EI CAS 2020年第4期812-819,共8页
Co30Cr8W1.6C3Ni1.4Si coatings were fabricated on Ti6Al4V alloy using a laser thermal spraying(LTS).The surface and cross-section morphologies,phases and bonding strength of obtained coatings were investigated using sc... Co30Cr8W1.6C3Ni1.4Si coatings were fabricated on Ti6Al4V alloy using a laser thermal spraying(LTS).The surface and cross-section morphologies,phases and bonding strength of obtained coatings were investigated using scanning electronic microscopy(SEM),X-ray diffraction(XRD),and scratch test,respectively.The effects of laser power on the coefficients of friction(COFs)and corrosive-wear behaviors of Co30Cr8W1.6C3Ni1.4Si coatings were investigated using a wear tester in 3.5%NaCl solution,and the electrochemical corrosion performance was analyzed using an electrochemical workstation.The experimental results show that the Co30Cr8W1.6C3Ni1.4Si coating is bonded with the substrate in the metallurgical form,and the bonding strengths of Co30Cr8W1.6C3Ni1.4Si coatings fabricated at the laser power of 1000,1200,and 1400 W are 76.5,56.5,and 55.6 N,respectively.The average COFs of Co30Cr8W1.6C3Ni1.4Si coatings fabricated at the laser power of 1000,1200,and 1400 W are 0.769,0.893,and 0.941,respectively;and the corresponding wear rates are 0.267×105,0.3178×105,and 0.325×105μm3/Nm,respectively,which increases with the increase of laser power,the wear mechanism is primarily abrasive wear.The corrosion potential of Co30Cr8W1.6C3Ni1.4Si coatings fabricated at the laser power of 1000,1200,and 1400 W is-0.05,-0.25,and-0.31 V,respectively,higher than-0.45 V of substrate which enhances the electrochemical corrosion resistance of substrate. 展开更多
关键词 laser thermal spraying(LTS) laser power Co30Cr8W1.6C3Ni1.4Si coating corrosive wear electrochemical corrosion
原文传递
Corrosion and wear properties of in situ(TiB+TiC)/TA15 composites with a high volume percentage of reinforcement
4
作者 Wei-long Wang Kun Shi +5 位作者 Jun Zhao Shi-bing Liu Jiao-jiao Cheng Wei-chen Qiu Tian-yu Liu Zhi-yong Zhang 《China Foundry》 SCIE CAS CSCD 2023年第5期423-431,共9页
The in situ(TiC+TiB)/TA15 composites with different volume percentages of reinforcement(10%,15%,20%and 25%)were prepared by water-cooled copper crucible vacuum suspension melting technology.The structures and composit... The in situ(TiC+TiB)/TA15 composites with different volume percentages of reinforcement(10%,15%,20%and 25%)were prepared by water-cooled copper crucible vacuum suspension melting technology.The structures and compositions of the TA15 alloy and its composites were analyzed by XRD and EDS,and their electrochemical corrosion behaviors in the 3.5%NaCl solution were studied.Corrosion wear testing was conducted using a reciprocating ball-on-disc wear tester under a 10 N load.Results show that the in situ fibrous TiB phase and the granular TiC phase are uniformly distributed on the composite matrix.The microhardness can reach up to 531 HV as 25vol.%TiC+TiB reinforcement is added.Compared with the TA15 alloy,the volume wear rate decreases from(2.21±0.07)×10^(-4)to(1.75±0.07)×10^(-4)mm^(3)·N^(-1)·m^(-1)by adding 15vol.%TiC+TiB reinforcement,and the wear mechanism is adhesive wear.When the volume percentage of the reinforcement phase reaches 25%,the volume wear rate increases from(1.75±0.07)×10^(-4)to(2.41±0.07)×10^(-4)mm^(3)·N^(-1)·m^(-1),and the wear mechanism changes into abrasive wear.The volume loss resulted by the interaction between corrosion and wear accounts for more than 27%of the total wear volume.The volume loss due to wear-induced corrosion changes from 1.94%to 4.06%with different additions of reinforcement.The volume loss caused by corrosion-induced wear initially increases from 24.08%to 26.90%as the reinforcement increases from 0 to 15%due to the increase of corrosion potential,and then decreases from 26.90%to 25.68%as the reinforcement increases from 15%to 25%due to the peeling of TiC phase. 展开更多
关键词 titanium matrix composites high volume percentage corrosion wear wear mechanism
下载PDF
Rietveld refinement of powder X-ray diffraction,microstructural and mechanical studies of magnesium matrix composites processed by high energy ball milling 被引量:1
5
作者 T.Ramkumar M.Selvakumar +3 位作者 R.Vasanthsankar A.S.Sathishkumar P.Narayanasamy G.Girija 《Journal of Magnesium and Alloys》 SCIE EI CAS 2018年第4期390-398,共9页
This research reports the processing of magnesium matrix composites reinforced with silicon carbide(SiC)and aluminium oxide(Al_(2)O_(3))using powder metallurgy technique through high energy milling.Samples of Mg-SiC a... This research reports the processing of magnesium matrix composites reinforced with silicon carbide(SiC)and aluminium oxide(Al_(2)O_(3))using powder metallurgy technique through high energy milling.Samples of Mg-SiC and Mg-Al_(2)O_(3)composites subjected to high energy ball milling for different vol%of secondary particles 20,30 and 40%of SiC and Al_(2)O_(3)are studied by X-Ray diffraction technique.The rietveld method as implemented in the Fullprof program is applied in order to determine the quantities of the resulting crystalline phases and amorphous phases at each stage of the mechanical treatment.Microstructural examination is carried out using Scanning Electron Microscope(SEM).In addition,crystal structural analysis using appropriate size and strain models is performed in order to handle the distinctive anistrophy that is observed in convinced crystallographic directions for the magnesium composite.The results are furnished in terms of crystalline domains size enlargement of the magnesium composites phases upon prolonged milling duration and discussed in the light of up to date views and theories on crystal growth of nanocrystaline materials.The hardness of the composite samples is calculated by Vickers’s Hardness tester.Further,dry sling wear test and corrosion test are performed for the fabricated composites.Composite with 30%secondary particles incorporated magnesium composites exhibits better wear and corrosion resistance than the other composites. 展开更多
关键词 Rietveld refinement X-ray diffraction Crystal structure Micro structure wear and corrosion
下载PDF
Process-structure-property relationship for plasma-sprayed iron-based amorphous/crystalline composite coatings
6
作者 Abhishek Pathak Biswajyoti Mukherjee +5 位作者 Krishna Kant Pandey Aminul Islam Pavan Bijalwan Monojit Dutta Atanu Banerjee Anup Kumar Keshri 《International Journal of Minerals,Metallurgy and Materials》 SCIE EI CAS CSCD 2022年第1期144-152,共9页
This study explores the fabrication of Fe-based amorphous/crystalline coating by air plasma spraying and its dependency on the coating parameters(plasma power,primary gas flow rate,powder feed rate,and stand-off dista... This study explores the fabrication of Fe-based amorphous/crystalline coating by air plasma spraying and its dependency on the coating parameters(plasma power,primary gas flow rate,powder feed rate,and stand-off distance).X-ray diffraction of the coatings deposited at optimized spray parameters showed the presence of amorphous/crystalline phase.Coatings deposited at a lower plasma power and highest gas flow rate exhibited better density,hardness,and wear resistance.All coatings demonstrated equally good resistance against the corrosive environment(3.5wt%NaCl solution).Mechanical,wear,and tribological studies indicated that a single process parameter optimization cannot provide good coating performance;instead,all process parameters have a unique role in defining better properties for the coating by con-trolling the in-flight particle temperature and velocity profile,followed by the cooling pattern of molten droplet before impingement on the substrate. 展开更多
关键词 Fe-based alloys amorphous alloys plasma spray coating mechanical corrosion and wear
下载PDF
Hierarchical Ti_(3)C_(2)T_(x)@MoS_(2) heterostructures:A first principles calculation and application in corrosion/wear protection 被引量:1
7
作者 Meng Cai Peng Feng +6 位作者 Han Yan Yuting Li Shijie Song Wen Li Hao Li Xiaoqiang Fan Minhao Zhu 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2022年第21期151-160,共10页
Surface and interface engineering plays a crucial role in modulating the properties of materials,especially two-dimensional(2D)materials.Hence,a strategy,forming heterostructures with MoS_(2),is proposed to overcome t... Surface and interface engineering plays a crucial role in modulating the properties of materials,especially two-dimensional(2D)materials.Hence,a strategy,forming heterostructures with MoS_(2),is proposed to overcome the natural agglomeration of Ti_(3)C_(2)T_(x) MXene nanosheets.Most importantly,the interactions between Ti_(3)C_(2)Tx and MoS_(2) were elaborately investigated by first-principles calculations based on density functional theory(DFT)for the first time.The calculations demonstrate that van der Waals forces dominate the interface interactions of Ti_(3)C_(2)T_(x) and MoS_(2),rendering Ti_(3)C_(2)T_(x)@MoS_(2) heterostructures favorable stability.The Ti_(3)C_(2)T_(x)@MoS_(2) heterostructure composites were synthesized through a facile one-step hydrothermal method and exhibit a 2D hierarchical structure.Furthermore,the corrosion and tribological properties of epoxy composite coatings with varying proportions of Ti_(3)C_(2)T_(x)@MoS_(2) composites were studied in detail.As a result,the epoxy composite coating with 0.1 wt.%Ti_(3)C_(2)T_(x)@MoS_(2) composites(Ti_(3)C_(2)T_(x)@MoS_(2)-0.1)exhibits excellent corrosion protection and antiwear performances.The Ti_(3)C_(2)T_(x)@MoS_(2)-0.1 keeps the largest low-frequency impedance modulus(|Z|_(0.)01 Hz)and coating resistance(R_(c))during the whole immersion period.Its wear rate is 0.09μm^(3)/(Nμm)under the load of 10 N,one half of that of pure epoxy coating(EP).This work further broadens the application of MXene-based heterostructure composites. 展开更多
关键词 First-principles calculations Ti_(3)C_(2)T_(x)MXene MoS_(2) Heterostructure Corrosion/wear
原文传递
Mitigation of tribocorrosion of metals in aqueous solutions by potential-enhanced adsorption of surfactants
8
作者 Chenxu LIU Yu TIAN +1 位作者 Zulfiqar A.KHAN Yonggang MENG 《Friction》 SCIE EI CAS CSCD 2023年第5期801-819,共19页
Corrosion and corrosive wear occur commonly on metals surface in aqueous solutions.External electric field is usually considered as one of the factors to accelerate corrosion or corrosive wear of materials in the pres... Corrosion and corrosive wear occur commonly on metals surface in aqueous solutions.External electric field is usually considered as one of the factors to accelerate corrosion or corrosive wear of materials in the presence of conventional electrolytes.This work aims to reposition widely believed perspective by experimental justification which have been conducted in aqueous solutions containing surfactants.Electric potential of metal surfaces was modulated externally within the electrochemical potential window of the metal electrode-solution-counter electrode system,which actively regulated the adsorption or desorption of surfactant molecule in the aqueous solution over the electrodes to form a molecular barrier of electron transportation across the electrode–electrolyte interface.The advantage of the approach over the anodic passivation is negligible redox reactions on the protected electrode surface while a better lubricious and wear resistant film than oxide is maintained in the meantime.Tribopairs of several metal/metal and metal/ceramic were tested by employing a ball-on-disc tribometer with anionic and cationic surfactants solutions.For anionic surfactant as the modifier,positive surface potential enables coefficient of friction to be decreased by promoting the formation of adsorption film on metal surface in aqueous solutions.For cationic surfactant,negative surface potential plays a role in decreasing the coefficient of friction.Phase diagrams of friction and wear in wide ranges of surfactant concentration and surface potential were plotted for the tested metal/metal and metal/ceramic tribopairs.These results indicate that the adsorption behavior of molecules or ions at the metal–aqueous interface can be well regulated when an external electric field is present without inducing corrosion or corrosive wear. 展开更多
关键词 corrosive wear metal electric field SURFACTANT ADSORPTION
原文传递
Tribo-corrosion interaction of the parallel steel wires in the suspension bridges
9
作者 Bo WANG Dagang WANG +3 位作者 Hailang CHONG Guozheng XIE Dekun ZHANG Shirong GE 《Friction》 SCIE EI CAS CSCD 2023年第12期2221-2237,共17页
The effect of contact load and relative displacement on tribo-corrosion interaction of parallel steel wires of main cable in the suspension bridge was investigated in this study.A self-made tribo-corrosion test bench ... The effect of contact load and relative displacement on tribo-corrosion interaction of parallel steel wires of main cable in the suspension bridge was investigated in this study.A self-made tribo-corrosion test bench was employed to conduct tribo-corrosion tests of parallel steel wires in 3.5%(wt%)NaCl solution and deionized water under different contact loads and different relative displacements.The friction coefficient and wear coefficient of wires were presented.Electrochemical corrosion behavior(Tafel polarization curves,Nyquist diagram,and equivalent circuit diagram)was characterized by electrochemical analyzer.Wear morphology was observed by scanning electron microscope.Wear volume loss and corrosion‒wear interaction were quantitatively demonstrated by high-precision weighing balance.The results show that the electrochemical corrosion ability of the steel wires increases with the increase of the contact load or relative displacement.The increased contact load or relative displacement increases the volume loss of corrosion‒wear and pure wear,but decreases the wear coefficient.The wear mechanisms in 3.5%NaCl solution are adhesive wear,abrasive wear,and corrosive wear as compared to adhesive wear and abrasive wear in deionized water under different contact loads.The wear mechanisms of parallel steel wires are slightly different under different relative displacements.But the main wear mechanisms are similar to that under different contact loads.The interaction effects of corrosion and wear produced by the contact load and relative displacement are all the synergistic effects. 展开更多
关键词 main cable parallel steel wires FRICTION corrosion‒wear INTERACTION
原文传递
Effect of environments and normal loads on tribological properties of nitrided Ni(45)(FeCoCr)(40)(AlTi)(15)high-entropy alloys 被引量:4
10
作者 L.W.Lan X.J.Wang +2 位作者 R.P.Guo H.J.Yang J.W.Qiao 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2020年第7期85-96,共12页
The tribological properties of nitrided Ni(45)(FeCoCr)(40)(AlTi)(15)high-entropy alloys(HEAs)were investigated in air and simulated acid rain under different normal loads(5,7,10,and 12 N)at ambient temperature.The res... The tribological properties of nitrided Ni(45)(FeCoCr)(40)(AlTi)(15)high-entropy alloys(HEAs)were investigated in air and simulated acid rain under different normal loads(5,7,10,and 12 N)at ambient temperature.The results revealed that as-cast HEAs were only composed of FCC phase,while the volume fraction of FCC phase in the nitrided alloys was significantly reduced.Moreover,the hard phases of AIN,CrN,Fe4 N,and TiN phases were formed in the nitrided alloys.The thickness of the nitriding layer was about 8.4μm.The hardness increased from 8.7 GPa in as-cast alloys to 14.5 GPa in the nitrided alloys.In addition,under the same conditions,the friction coefficient of the nitrided alloys was higher than that of as-cast alloys,but the wear rate was generally lower than that of as-cast alloys.Furthermore,the wear rate of the nitrided alloys was the lowest in acid rain due to the lubrication,cleaning,and cooling in the liquid environment.In air,dominating wear mechanisms in as-cast and nitrided alloys were abrasive,delamination,and adhesive wears.And,the wear mechanism of as-cast and nitrided alloys in acid rain was mainly abrasive and corrosion wears. 展开更多
关键词 Abrasive wear HARDNESS corrosive wear MICROSTRUCTURE wear mechanism
原文传递
Corrosion and impact-abrasion-corrosion behaviors of quenching- tempering martensitic Fe-Cr alloy steels 被引量:4
11
作者 Zhi-bin Zheng Jun Long +3 位作者 Yi Guo Hui Li Kai-hong Zheng Yan-xin Qiao 《Journal of Iron and Steel Research(International)》 SCIE EI CAS CSCD 2022年第11期1853-1863,共11页
The corrosion and impact-abrasion-corrosion behaviors of quenching-tempering Fe-Cr martensitic steels for ball mill liner were investigated in the corrosive slurry of a copper mine compared with high manganese steel.I... The corrosion and impact-abrasion-corrosion behaviors of quenching-tempering Fe-Cr martensitic steels for ball mill liner were investigated in the corrosive slurry of a copper mine compared with high manganese steel.It is found that the corrosion resistance and the protectiveness of the passive film of Fe-Cr martensitic steels became worse when the carbon content increased.The quenching-tempering Fe-Cr martensitic steel showed better impact-abrasion-corrosion resistance in the corrosive slurry compared with the high manganese steel,especially the alloy steel with the carbon content of 0.3 wt.%.The synergistic effect between mechanics and corrosion has also been analyzed to further reveal the impact-abrasion-corrosion mechanism of the steels.The damage from pure mechanics accounted for the largest percentage(over 65%)for all steels,demonstrating that mechanical damage played the most important role in the impact-abrasion-corrosion behaviors of the steels.The impact and cracking resistance of the steel should also be paid special attention during the development of new materials for ball mill liner. 展开更多
关键词 MINING Abrasive wear corrosive wear Impact wear Martensitic steel
原文传递
Enamel coating for protection of the 316 stainless steel against tribo-corrosion in molten zinc alloy at 460℃
12
作者 Zhongdi Yu Minghui Chen +3 位作者 Jinlong Wang Fengjie Li Shenglong Zhu Fuhui Wang 《Journal of Materials Science & Technology》 SCIE EI CAS CSCD 2021年第6期126-136,共11页
Hot-dip galvanizing provides excellent corrosion and wear resistance for steels.However,the equipment itself,such as the steel roller,immerged in corrosive molten zinc suffers serious material loss during steel's ... Hot-dip galvanizing provides excellent corrosion and wear resistance for steels.However,the equipment itself,such as the steel roller,immerged in corrosive molten zinc suffers serious material loss during steel's production.Its protection has become the main technique problem in modern galvanizing line.In this study,an enamel coating was designed and prepared.Its tribo-corrosion in molten zinc alloy(Zn-0.2 wt%Al)at 460℃was investigated in comparison with the traditional WC-12 Co composite coating and the 316 stainless steel.Results indicate that the steel suffers serious material damage.Various corrosion products of Fe_(2) Al_(5) Znx form at the worn surface and the wear scar has reached 200μm deep after merely 5 h tribo-corrosion.Though the two coatings provide an improved tribo-corrosion resistance,for the WC-12 Co coating,its chemical reaction with the molten zinc increases brittleness and promotes cracking.The synergistic wear and corrosion cause its degradation.The enamel coating performs better during tribo-corrosion.It is chemically stable in molten zinc thus able to provide high corrosion resistance.In addition,the amorphous[Si04]network and the self-lubricating CaF_(2) crystallite help it to build up an intact amorphous glaze layer readily at surface on sliding,leading to a reduced wear loss.During the whole tribo-corrosion process,the enamel coating is completely free of cracking,and the Zn penetration is inhibited. 展开更多
关键词 Enamel coating High temperature corrosion Liquid alloy corrosive wear
原文传递
Two material removal modes in chemical mechanical polishing:mechanical plowing vs.chemical bonding
13
作者 Yuan WU Liang JIANG +3 位作者 Wenhui LI Jiaxin ZHENG Yushan CHEN Linmao QIAN 《Friction》 SCIE EI CAS 2024年第5期897-905,共9页
With the rapid development of semiconductors,the number of materials needed to be polished sharply increases.The material properties vary significantly,posing challenges to chemical mechanical polishing(CMP).According... With the rapid development of semiconductors,the number of materials needed to be polished sharply increases.The material properties vary significantly,posing challenges to chemical mechanical polishing(CMP).Accordingly,the study aimed to classify the material removal mechanism.Based on the CMP and atomic force microscopy results,the six representative metals can be preliminarily classified into two groups,presumably due to different material removal modes.From the tribology perspective,the first group of Cu,Co,and Ni may mainly rely on the mechanical plowing effect.After adding H_(2)O_(2),corrosion can be first enhanced and then suppressed,affecting the surface mechanical strength.Consequently,the material removal rate(MRR)and the surface roughness increase and decrease.By comparison,the second group of Ta,Ru,and Ti may primarily depend on the chemical bonding effect.Adding H_(2)O_(2)can promote oxidation,increasing interfacial chemical bonds.Therefore,the MRR increases,and the surface roughness decreases and levels off.In addition,CMP can be regulated by tuning the synergistic effect of oxidation,complexation,and dissolution for mechanical plowing,while tuning the synergistic effect of oxidation and ionic strength for chemical bonding.The findings provide mechanistic insight into the material removal mechanism in CMP. 展开更多
关键词 Chemical mechanical polishing corrosion wear material removal mode mechanical plowing chemical bonding