In order to improve the bioactivity of 316L stainless steel,a titanium layer was prepared on the surface of 316L by laser cladding(LC),followed by plasma electrolytic oxidation(PEO)to form a porous ceramic coating on ...In order to improve the bioactivity of 316L stainless steel,a titanium layer was prepared on the surface of 316L by laser cladding(LC),followed by plasma electrolytic oxidation(PEO)to form a porous ceramic coating on titanium layer.The morphologies,microstructure and compositions of the coated samples were characterized by 3D surface profiler,SEM,EDS,XRD and XPS.The corrosion resistance and bioactivity of the coatings were evaluated by potentiodynamic polarization and immersion test in simulated body fluid(SBF),respectively.The results showed that the porous ceramic coating mainly consisted of anatase and rutile,and highly crystalline HA was also detected.The main elements of the PEO coating are Ca,P,Ti and O.The LC+PEO composite bio-coating has more excellent corrosion resistance than the 316L substrate in simulated body fluid.Furthermore,the composite coating could effectively improve the bioactivity of 316L stainless steel.展开更多
基金financial support from the National Natural Science Foundation of China (No. 51975533)National Safety Academic Fund, China (No. U2130122)Public Projects of Zhejiang Province, China (Nos. LGJ22E050002, LGJ20E050002)
文摘In order to improve the bioactivity of 316L stainless steel,a titanium layer was prepared on the surface of 316L by laser cladding(LC),followed by plasma electrolytic oxidation(PEO)to form a porous ceramic coating on titanium layer.The morphologies,microstructure and compositions of the coated samples were characterized by 3D surface profiler,SEM,EDS,XRD and XPS.The corrosion resistance and bioactivity of the coatings were evaluated by potentiodynamic polarization and immersion test in simulated body fluid(SBF),respectively.The results showed that the porous ceramic coating mainly consisted of anatase and rutile,and highly crystalline HA was also detected.The main elements of the PEO coating are Ca,P,Ti and O.The LC+PEO composite bio-coating has more excellent corrosion resistance than the 316L substrate in simulated body fluid.Furthermore,the composite coating could effectively improve the bioactivity of 316L stainless steel.