载纳米银海藻酸钙敷料的制备及体外细胞毒性、抗菌性能的检测 被引量:7
1
作者 林志群 赵大川 +4 位作者 郎敏 柳学文 陈瀛 陈飞 黄宗海 《生物医学工程研究》 北大核心 2016年第2期113-117,共5页
以湿法纺丝法制得的海藻酸钙羧甲基纤维复合物作为敷料载体,再利用浸渍法将纳米银粒子搭载于敷料之上,制备质量分数为0.5、1、2、4%的载纳米银海藻酸钙抗菌敷料。采用紫外-可见光分光光度计和扫描电子显微镜检测敷料的物理学表征,并检... 以湿法纺丝法制得的海藻酸钙羧甲基纤维复合物作为敷料载体,再利用浸渍法将纳米银粒子搭载于敷料之上,制备质量分数为0.5、1、2、4%的载纳米银海藻酸钙抗菌敷料。采用紫外-可见光分光光度计和扫描电子显微镜检测敷料的物理学表征,并检测抗菌敷料的细胞毒性及抗菌性能。结果表明载纳米银海藻酸钙抗菌敷料表面可见纳米银均匀附着,于去离子水中可释放纳米银粒子,而载银量1%的海藻酸钙敷料无明显细胞毒性且对常见四种菌株均有良好的抗菌性能,是一个理想的载银浓度。 展开更多
关键词 纳米银 海藻酸钙 物理学表征 细胞毒性 抗菌性能
下载PDF
Characterization of semi-coke generated by coal-based direct reduction process of siderite
2
作者 朱德庆 罗艳红 +1 位作者 潘建 周仙霖 《Journal of Central South University》 SCIE EI CAS CSCD 2015年第8期2914-2921,共8页
Solid wastes derived from metallurgical industries pose a significant threat to environment. The utilization and disposal of these solid wastes are the major concern in the world. Semi-coke generated in coal-based dir... Solid wastes derived from metallurgical industries pose a significant threat to environment. The utilization and disposal of these solid wastes are the major concern in the world. Semi-coke generated in coal-based direct reduction process of iron ore is a by-product and its suitable utilization is not available so far. In order to handle it properly, the characteristics of this by-product were comprehensively investigated. A series of analysis methods were used to demonstrate its mineral compositions, petrography and physico-chemical properties. The results reveal that the semi-coke has poor washability. The fixed carbon content of semi-coke reaches 76.11% and the gross calorific value is 28.10 MJ/kg, both of which are similar to those of traditional sinter coke breeze. Also, semi-coke ash possesses lower content of SiO2, Al2O3, S and higher content of CaO and MgO, which could improve the strength of sinter ore when partially substituting for coke breeze in sintering. Semi-coke features well-development porous structure and higher reaction activity, which predicts that the sintering speed could be elevated to some extent when employing it as a partial replacement of coke breeze, so the studies further suggest that the potential adverse effect of the high reactivity on sintering process could be weakened by adequately coarsening the semi-coke's particle size. 展开更多
关键词 SEMI-COKE coal-based direct reduction non-magnetic product sinter fuel