Manganese-based material is a prospective cathode material for aqueous zinc ion batteries(ZIBs)by virtue of its high theoretical capacity,high operating voltage,and low price.However,the manganese dissolution during t...Manganese-based material is a prospective cathode material for aqueous zinc ion batteries(ZIBs)by virtue of its high theoretical capacity,high operating voltage,and low price.However,the manganese dissolution during the electrochemical reaction causes its electrochemical cycling stability to be undesirable.In this work,heterointerface engineering-induced oxygen defects are introduced into heterostructure MnO_(2)(δa-MnO_(2))by in situ electrochemical activation to inhibit manganese dissolution for aqueous zinc ion batteries.Meanwhile,the heterointerface between the disordered amorphous and the crystalline MnO_(2)ofδa-MnO_(2)is decisive for the formation of oxygen defects.And the experimental results indicate that the manganese dissolution ofδa-MnO_(2)is considerably inhibited during the charge/discharge cycle.Theoretical analysis indicates that the oxygen defect regulates the electronic and band structure and the Mn-O bonding state of the electrode material,thereby promoting electron transport kinetics as well as inhibiting Mn dissolution.Consequently,the capacity ofδa-MnO_(2)does not degrade after 100 cycles at a current density of 0.5 Ag^(-1)and also 91%capacity retention after 500cycles at 1 Ag^(-1).This study provides a promising insight into the development of high-performance manganese-based cathode materials through a facile and low-cost strategy.展开更多
To clarify the formation and distribution of feldspar dissolution pores and predict the distribution of high-quality reservoir in gravity flow sandstone of the 7^(th) member of Triassic Yanchang Formation(Chang 7 Memb...To clarify the formation and distribution of feldspar dissolution pores and predict the distribution of high-quality reservoir in gravity flow sandstone of the 7^(th) member of Triassic Yanchang Formation(Chang 7 Member)in the Ordos Basin,thin sections,scanning electron microscopy,energy spectrum analysis,X-ray diffraction whole rock analysis,and dissolution experiments are employed in this study to investigate the characteristics and control factors of feldspar dissolution pores.The results show that:(1)Three types of diagenetic processes are observed in the feldspar of Chang 7 sandstone in the study area:secondary overgrowth of feldspar,replacement by clay and calcite,and dissolution of detrital feldspar.(2)The feldspar dissolution of Chang 7 tight sandstone is caused by organic acid,and is further affected by the type of feldspar,the degree of early feldspar alteration,and the buffering effect of mica debris on organic acid.(3)Feldspars have varying degrees of dissolution.Potassium feldspar is more susceptible to dissolution than plagioclase.Among potassium feldspar,orthoclase is more soluble than microcline,and unaltered feldspar is more soluble than early kaolinized or sericitized feldspar.(4)The dissolution experiment demonstrated that the presence of mica can hinder the dissolution of feldspar.Mica of the same mass has a significantly stronger capacity to consume organic acids than feldspar.(5)Dissolution pores in feldspar of Chang 7 Member are more abundant in areas with low mica content,and they improve the reservoir physical properties,while in areas with high mica content,the number of feldspar dissolution pores decreases significantly.展开更多
Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonethel...Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonetheless,the intricate energy storage mechanisms in aqueous electrolytes place stringent require-ments on the host materials.Prussian blue analogs(PBAs),with their open three-dimensional framework and facile synthesis,stand out as leading candidates for aqueous energy storage.However,PBAs possess a swift capacity fade and limited cycle longevity,for their structural integrity is compromised by the pronounced dis-solution of transition metal(TM)ions in the aqueous milieu.This manuscript provides an exhaustive review of the recent advancements concerning PBAs in ASIBs and APIBs.The dissolution mechanisms of TM ions in PBAs,informed by their structural attributes and redox processes,are thoroughly examined.Moreover,this study delves into innovative design tactics to alleviate the dissolution issue of TM ions.In conclusion,the paper consolidates various strategies for suppressing the dissolution of TM ions in PBAs and posits avenues for prospective exploration of high-safety aqueous sodium-/potassium-ion batteries.展开更多
To investigate the dissolution behaviors of Al_(2)O_(3)inclusions in CaO-5wt%MgO-SiO_(2)-30wt%Al_(2)O_(3)-TiO_(2)system ladle slags,confocal scanning laser microscopy was conducted on the slags with different TiO_(2)c...To investigate the dissolution behaviors of Al_(2)O_(3)inclusions in CaO-5wt%MgO-SiO_(2)-30wt%Al_(2)O_(3)-TiO_(2)system ladle slags,confocal scanning laser microscopy was conducted on the slags with different TiO_(2)contents(0-10wt%),and scanning electron microscopy was performed to study the interfacial reaction between Al_(2)O_(3)and this slag system.The results disclose that the dissolution of Al_(2)O_(3)inclusions does not result in the formation of new phases at the boundary between the slag and the inclusions.In TiO_(2)-bearing and TiO_(2)-free ladle slags,there is no difference in the dissolution mechanism of Al_(2)O_(3)inclusions at steelmaking temperatures.Boundary layer diffusion is found as the controlling step of the dissolution of Al_(2)O_(3),and the diffusion coefficient is in the range of 4.18×10^(-10)to 2.18×10^(-9)m^(2)/s at 1450-1500℃.Compared with the solubility of Al_(2)O_(3)in the slags,slag viscosity and temperature play a more profound role in the dissolution of Al_(2)O_(3)inclusions.A lower viscosity and a lower melting point of the slags are beneficial for the dissolution.Suitable addition of TiO_(2)(e.g.,5wt%)in ladle slags can enhance the dissolution of Al_(2)O_(3)inclusions because of the low viscosity and melting point of the slags,while excessive addition of TiO_(2)(e.g.,10wt%)shows the opposite trend.展开更多
In this study,ZnO formation during the dissolution-passivation process of Zn anodes is observed via in situ Raman and optical characterization.The Zn passivation during galvanostatic anodization merely follows the dis...In this study,ZnO formation during the dissolution-passivation process of Zn anodes is observed via in situ Raman and optical characterization.The Zn passivation during galvanostatic anodization merely follows the dissolution-precipitation model,whereas that of potentiodynamic polarization exhibits different behaviors in different potential ranges.Initially,the Zn electrode is gradually covered by a ZnO precipitation film and then undergoes solid-state oxidation at~255 mV.The starting point of solid-state oxidation is well indicated by the abrupt current drop and yellow coloration of the electrode surface.During the pseudo passivation,an intense current oscillation is observed.Further,blink-like color changes between yellow and dark blue are revealed for the first time,implying that the oscillation is caused by the dynamic adsorption and desorption of OH groups.The as-formed ZnOs then experience a dissolution-reformation evolution,during which the crystallinity of the primary ZnO film is improved but the solid-state-formed ZnO layer becomes rich in oxygen vacancies.Eventually,oxide densification is realized,contributing to the Zn passivation.This study provides new insights into the Zn dissolution-passivation behavior,which is critical for the future optimization of Zn batteries.展开更多
Alumina is one of the crucial and extensively utilized refractory components.As the refractory wear due to dissolution at elevated temperatures during operation is a major threat to refractory lifespan,quantifying dis...Alumina is one of the crucial and extensively utilized refractory components.As the refractory wear due to dissolution at elevated temperatures during operation is a major threat to refractory lifespan,quantifying dissolution is important for developing cost-effective and resource-efficient refractories.This study investigated the dissolution of alumina particles in two silicate and one calcium aluminate slags at 1450,1500,and 1550°C using high-temperature confocal laser scanning microscopy(HT-CLSM).Dissolution was quantified in terms of diffusivity,with all influencing factors,including Stefan flow and bath movement,incorporated into the determination process.The trends observed in total dissolution time and diffusivity in three slags at three experimental temperatures could not be explained solely on the basis of slag basicity.Two parameters,considering the influencing factors,were introduced to explain these trends.Furthermore,the linear trend observed in Arrhenius plots of diffusivities supports the diffusivity results.Additionally,good agreement between the diffusivities of alumina in one silicate slag obtained via CLSM and rotating finger test investigations verified the reliability of the results.展开更多
The phenomenon of marital dissolution in later life,also referred to as“gray divorce”,is described on the rise in contemporary Western societies.This article contributes to the study of marriage breakdown in older a...The phenomenon of marital dissolution in later life,also referred to as“gray divorce”,is described on the rise in contemporary Western societies.This article contributes to the study of marriage breakdown in older age,with a specific focus on Italian society.First,the temporal trends of this phenomenon are reconstructed using official statistics.The data reveal that,although still relatively rare,the dissolution of marriage in later life is expanding in Italy.The analysis of the period from 1974 to 2015 indicates a rise in the average age at separation,a higher percentage of spouses over 50 years on the total number of couples obtaining legal separation,and an increase in the proportion of Italian spouses separating after many years of marriage.Furthermore,data from the national survey“Family and Social Subjects”,conducted in 2016 by the Italian National Institute of Statistics,are utilized to explore the relationship between specific traits of those who separated and their tendency to dissolve marriages before or after the age of 50.The data suggest that individuals with characteristics such as lower educational attainment,residence in the South and Islands,and adherence to more traditional family models are more likely to experience separation in later life.展开更多
基金funds from the National Natural Science Foundation of China(51772082 and 51804106)the Natural Science Foundation of Hunan Province(2023JJ10005)
文摘Manganese-based material is a prospective cathode material for aqueous zinc ion batteries(ZIBs)by virtue of its high theoretical capacity,high operating voltage,and low price.However,the manganese dissolution during the electrochemical reaction causes its electrochemical cycling stability to be undesirable.In this work,heterointerface engineering-induced oxygen defects are introduced into heterostructure MnO_(2)(δa-MnO_(2))by in situ electrochemical activation to inhibit manganese dissolution for aqueous zinc ion batteries.Meanwhile,the heterointerface between the disordered amorphous and the crystalline MnO_(2)ofδa-MnO_(2)is decisive for the formation of oxygen defects.And the experimental results indicate that the manganese dissolution ofδa-MnO_(2)is considerably inhibited during the charge/discharge cycle.Theoretical analysis indicates that the oxygen defect regulates the electronic and band structure and the Mn-O bonding state of the electrode material,thereby promoting electron transport kinetics as well as inhibiting Mn dissolution.Consequently,the capacity ofδa-MnO_(2)does not degrade after 100 cycles at a current density of 0.5 Ag^(-1)and also 91%capacity retention after 500cycles at 1 Ag^(-1).This study provides a promising insight into the development of high-performance manganese-based cathode materials through a facile and low-cost strategy.
基金Supported by the National Natural Science Foundation of China(42202176)CNPC-Southwest University of Petroleum Innovation Consortium Cooperation Project(2020CX050103).
文摘To clarify the formation and distribution of feldspar dissolution pores and predict the distribution of high-quality reservoir in gravity flow sandstone of the 7^(th) member of Triassic Yanchang Formation(Chang 7 Member)in the Ordos Basin,thin sections,scanning electron microscopy,energy spectrum analysis,X-ray diffraction whole rock analysis,and dissolution experiments are employed in this study to investigate the characteristics and control factors of feldspar dissolution pores.The results show that:(1)Three types of diagenetic processes are observed in the feldspar of Chang 7 sandstone in the study area:secondary overgrowth of feldspar,replacement by clay and calcite,and dissolution of detrital feldspar.(2)The feldspar dissolution of Chang 7 tight sandstone is caused by organic acid,and is further affected by the type of feldspar,the degree of early feldspar alteration,and the buffering effect of mica debris on organic acid.(3)Feldspars have varying degrees of dissolution.Potassium feldspar is more susceptible to dissolution than plagioclase.Among potassium feldspar,orthoclase is more soluble than microcline,and unaltered feldspar is more soluble than early kaolinized or sericitized feldspar.(4)The dissolution experiment demonstrated that the presence of mica can hinder the dissolution of feldspar.Mica of the same mass has a significantly stronger capacity to consume organic acids than feldspar.(5)Dissolution pores in feldspar of Chang 7 Member are more abundant in areas with low mica content,and they improve the reservoir physical properties,while in areas with high mica content,the number of feldspar dissolution pores decreases significantly.
基金This work was supported by the National Natural Science Foundation of China(52373306,52172233,and 51832004)the Natural Science Foundation of Hubei Province(2023AFA053)the Hainan Provincial Joint Project of Sanya Yazhou Bay Science and Technology City(2021CXLH0007).
文摘Aqueous sodium-ion batteries(ASIBs)and aqueous potassium-ion batteries(APIBs)present significant potential for large-scale energy storage due to their cost-effectiveness,safety,and environmental compatibility.Nonetheless,the intricate energy storage mechanisms in aqueous electrolytes place stringent require-ments on the host materials.Prussian blue analogs(PBAs),with their open three-dimensional framework and facile synthesis,stand out as leading candidates for aqueous energy storage.However,PBAs possess a swift capacity fade and limited cycle longevity,for their structural integrity is compromised by the pronounced dis-solution of transition metal(TM)ions in the aqueous milieu.This manuscript provides an exhaustive review of the recent advancements concerning PBAs in ASIBs and APIBs.The dissolution mechanisms of TM ions in PBAs,informed by their structural attributes and redox processes,are thoroughly examined.Moreover,this study delves into innovative design tactics to alleviate the dissolution issue of TM ions.In conclusion,the paper consolidates various strategies for suppressing the dissolution of TM ions in PBAs and posits avenues for prospective exploration of high-safety aqueous sodium-/potassium-ion batteries.
基金financially supported by the National Natural Science Foundation of China(Nos.U20A20272 and52074073)the Fundamental Research Funds for the Central Universities(No.2325035)。
文摘To investigate the dissolution behaviors of Al_(2)O_(3)inclusions in CaO-5wt%MgO-SiO_(2)-30wt%Al_(2)O_(3)-TiO_(2)system ladle slags,confocal scanning laser microscopy was conducted on the slags with different TiO_(2)contents(0-10wt%),and scanning electron microscopy was performed to study the interfacial reaction between Al_(2)O_(3)and this slag system.The results disclose that the dissolution of Al_(2)O_(3)inclusions does not result in the formation of new phases at the boundary between the slag and the inclusions.In TiO_(2)-bearing and TiO_(2)-free ladle slags,there is no difference in the dissolution mechanism of Al_(2)O_(3)inclusions at steelmaking temperatures.Boundary layer diffusion is found as the controlling step of the dissolution of Al_(2)O_(3),and the diffusion coefficient is in the range of 4.18×10^(-10)to 2.18×10^(-9)m^(2)/s at 1450-1500℃.Compared with the solubility of Al_(2)O_(3)in the slags,slag viscosity and temperature play a more profound role in the dissolution of Al_(2)O_(3)inclusions.A lower viscosity and a lower melting point of the slags are beneficial for the dissolution.Suitable addition of TiO_(2)(e.g.,5wt%)in ladle slags can enhance the dissolution of Al_(2)O_(3)inclusions because of the low viscosity and melting point of the slags,while excessive addition of TiO_(2)(e.g.,10wt%)shows the opposite trend.
基金supported by the Research and Development Initiative for Scientific Innovation of New Generation Batteries(RISING)Projects,RISING2[JPNP16001]and RISING3[JPNP21006],commissioned by of the New Energy and Industrial Technology Development Organization(NEDO),Japanthe State Scholarship Fund of the China Scholarship Council[No.201906230294]for their support
文摘In this study,ZnO formation during the dissolution-passivation process of Zn anodes is observed via in situ Raman and optical characterization.The Zn passivation during galvanostatic anodization merely follows the dissolution-precipitation model,whereas that of potentiodynamic polarization exhibits different behaviors in different potential ranges.Initially,the Zn electrode is gradually covered by a ZnO precipitation film and then undergoes solid-state oxidation at~255 mV.The starting point of solid-state oxidation is well indicated by the abrupt current drop and yellow coloration of the electrode surface.During the pseudo passivation,an intense current oscillation is observed.Further,blink-like color changes between yellow and dark blue are revealed for the first time,implying that the oscillation is caused by the dynamic adsorption and desorption of OH groups.The as-formed ZnOs then experience a dissolution-reformation evolution,during which the crystallinity of the primary ZnO film is improved but the solid-state-formed ZnO layer becomes rich in oxygen vacancies.Eventually,oxide densification is realized,contributing to the Zn passivation.This study provides new insights into the Zn dissolution-passivation behavior,which is critical for the future optimization of Zn batteries.
基金funded by the COMET program within the K2 Center “Integrated Computational MaterialProcess and Product Engineering (IC-MPPE)”, Project No. 859480+7 种基金supported by the Austrian Federal Ministries for TransportInnovationand Technology (BMVIT)Digital and Economic Affairs (BMDW)represented by the Austrian Research Funding Association (FFG)the federal states of StyriaUpper Austriaand Tyrol
文摘Alumina is one of the crucial and extensively utilized refractory components.As the refractory wear due to dissolution at elevated temperatures during operation is a major threat to refractory lifespan,quantifying dissolution is important for developing cost-effective and resource-efficient refractories.This study investigated the dissolution of alumina particles in two silicate and one calcium aluminate slags at 1450,1500,and 1550°C using high-temperature confocal laser scanning microscopy(HT-CLSM).Dissolution was quantified in terms of diffusivity,with all influencing factors,including Stefan flow and bath movement,incorporated into the determination process.The trends observed in total dissolution time and diffusivity in three slags at three experimental temperatures could not be explained solely on the basis of slag basicity.Two parameters,considering the influencing factors,were introduced to explain these trends.Furthermore,the linear trend observed in Arrhenius plots of diffusivities supports the diffusivity results.Additionally,good agreement between the diffusivities of alumina in one silicate slag obtained via CLSM and rotating finger test investigations verified the reliability of the results.
文摘The phenomenon of marital dissolution in later life,also referred to as“gray divorce”,is described on the rise in contemporary Western societies.This article contributes to the study of marriage breakdown in older age,with a specific focus on Italian society.First,the temporal trends of this phenomenon are reconstructed using official statistics.The data reveal that,although still relatively rare,the dissolution of marriage in later life is expanding in Italy.The analysis of the period from 1974 to 2015 indicates a rise in the average age at separation,a higher percentage of spouses over 50 years on the total number of couples obtaining legal separation,and an increase in the proportion of Italian spouses separating after many years of marriage.Furthermore,data from the national survey“Family and Social Subjects”,conducted in 2016 by the Italian National Institute of Statistics,are utilized to explore the relationship between specific traits of those who separated and their tendency to dissolve marriages before or after the age of 50.The data suggest that individuals with characteristics such as lower educational attainment,residence in the South and Islands,and adherence to more traditional family models are more likely to experience separation in later life.