Au nanorods have been successfully synthesized at 90 ℃ by using hexadecyltrimethylammonium bromide (CTAB) and benzyldimethylammoniumchloride hydrate (BDAC) co-surfactant. At 90 ℃, the reaction time was less than...Au nanorods have been successfully synthesized at 90 ℃ by using hexadecyltrimethylammonium bromide (CTAB) and benzyldimethylammoniumchloride hydrate (BDAC) co-surfactant. At 90 ℃, the reaction time was less than 10 s, and the longitudinal surface plasmon absorption band could vary between 680 and 770 nm by adjusting the molar ratio of BDAC to CTAB from 2 to 0.5. At 90 ℃, nanorods with a longitudinal surface plasmon absorption peak of 770 nm can be obtained when the molar ratio of BDAC to CTAB was 3:2.展开更多
文摘Au nanorods have been successfully synthesized at 90 ℃ by using hexadecyltrimethylammonium bromide (CTAB) and benzyldimethylammoniumchloride hydrate (BDAC) co-surfactant. At 90 ℃, the reaction time was less than 10 s, and the longitudinal surface plasmon absorption band could vary between 680 and 770 nm by adjusting the molar ratio of BDAC to CTAB from 2 to 0.5. At 90 ℃, nanorods with a longitudinal surface plasmon absorption peak of 770 nm can be obtained when the molar ratio of BDAC to CTAB was 3:2.