Mesoporous silica nanoparticles (MSNs) are promising for drug delivery and other biomedical applications owing to their excellent chemical stability and biocompatibility. For these applications, a hollow morphology ...Mesoporous silica nanoparticles (MSNs) are promising for drug delivery and other biomedical applications owing to their excellent chemical stability and biocompatibility. For these applications, a hollow morphology with thin shell and open mesopores is preferred for MSNs in order to maximize the loading capacity of drugs. Herein we report a novel and direct synthesis of such an ideal drug delivery system in a dilute and alkaline solution of benzylcetyl- dimethylammonium chloride and diethylene glycol hexadecyl ether. The mixed surfactants can guide the formation of MSNs with cubic Ia3d mesostructure, and at a concentration of sodium hydroxide between 9.8 and 13.5 mM, hollow MSNs with uniform sizes of 90-120 nm and a single-unit-cell-thick shell are formed. A mechanism for the formation of the hollow Ia3d MSNs, designated as MMT-2, is proposed based on in situ small-angle X-ray scattering measurements and other analyses. MMT-2 exhibits much higher loading capacity of ibuprofen and degrades faster in simulated body fluid and phosphate buffered saline than non-hollow MSNs. The degradation of MMT-2 can be significantly retarded by modification with polyethylene glycol. More interestingly, the degradation of MMT-2 involves fragmentation instead of void formation, a phenomenon beneficial for their elimination. The results demonstrate the uniqueness of the hollow Ia3d MSNs and the great potential of the material for drug delivery and biomedical applications.展开更多
1 Introduction Since its first discovery in 1992, ordered mesoporous silica material with large pore size, high surface area, and high pore volume has attracted great attention for the potentially wide application in...1 Introduction Since its first discovery in 1992, ordered mesoporous silica material with large pore size, high surface area, and high pore volume has attracted great attention for the potentially wide application in catalysis, adsorption, separation, and ion exchange, etc. However, the poor hydrothermal stability of mesoporous silica has limited its wide application in industry. Therefore, in the last 10 years, many studies have been dedicated to improving the hydrothermal stability of mesoporous silica. Xiao et al.展开更多
文摘Mesoporous silica nanoparticles (MSNs) are promising for drug delivery and other biomedical applications owing to their excellent chemical stability and biocompatibility. For these applications, a hollow morphology with thin shell and open mesopores is preferred for MSNs in order to maximize the loading capacity of drugs. Herein we report a novel and direct synthesis of such an ideal drug delivery system in a dilute and alkaline solution of benzylcetyl- dimethylammonium chloride and diethylene glycol hexadecyl ether. The mixed surfactants can guide the formation of MSNs with cubic Ia3d mesostructure, and at a concentration of sodium hydroxide between 9.8 and 13.5 mM, hollow MSNs with uniform sizes of 90-120 nm and a single-unit-cell-thick shell are formed. A mechanism for the formation of the hollow Ia3d MSNs, designated as MMT-2, is proposed based on in situ small-angle X-ray scattering measurements and other analyses. MMT-2 exhibits much higher loading capacity of ibuprofen and degrades faster in simulated body fluid and phosphate buffered saline than non-hollow MSNs. The degradation of MMT-2 can be significantly retarded by modification with polyethylene glycol. More interestingly, the degradation of MMT-2 involves fragmentation instead of void formation, a phenomenon beneficial for their elimination. The results demonstrate the uniqueness of the hollow Ia3d MSNs and the great potential of the material for drug delivery and biomedical applications.
基金Supported by the National Natural Science Foundation of China(Nos.20401015 and 50574082)Beijing(China) Municipal Natural Science Foundation(No.2082022)the Innovation Project of the Chinese Academy of Sciences(Nos.CXJJ-171 and CXJJ-210)
文摘1 Introduction Since its first discovery in 1992, ordered mesoporous silica material with large pore size, high surface area, and high pore volume has attracted great attention for the potentially wide application in catalysis, adsorption, separation, and ion exchange, etc. However, the poor hydrothermal stability of mesoporous silica has limited its wide application in industry. Therefore, in the last 10 years, many studies have been dedicated to improving the hydrothermal stability of mesoporous silica. Xiao et al.