To achieve the resource utilization of solid waste phosphogypsum(PG)and tackle the problem of utilizing potassium feldspar(PF),a coupled synergistic process between PG and PF is proposed in this paper.The study invest...To achieve the resource utilization of solid waste phosphogypsum(PG)and tackle the problem of utilizing potassium feldspar(PF),a coupled synergistic process between PG and PF is proposed in this paper.The study investigates the features of P and F in PG,and explores the decomposition of PF using hydrofluoric acid(HF)in the sulfuric acid system for K leaching and leaching of P and F in PG.The impact factors such as sulfuric acid concentration,reaction temperature,reaction time,material ratio(PG/PF),liquid–solid ratio,PF particle size,and PF calcination temperature on the leaching of P and K is systematically investigated in this paper.The results show that under optimal conditions,the leaching rate of K and P reach more than 93%and 96%,respectively.Kinetics study using shrinking core model(SCM)indicates two significant stages with internal diffusion predominantly controlling the leaching of K.The apparent activation energies of these two stages are 11.92 kJ·mol^(-1)and 11.55 kJ·mol^(-1),respectively.展开更多
The proper recycling of spent lithium-ion batteries(LIBs)can promote the recovery and utilization of valuable resources,while also negative environmental effects resulting from the presence of toxic and hazardous subs...The proper recycling of spent lithium-ion batteries(LIBs)can promote the recovery and utilization of valuable resources,while also negative environmental effects resulting from the presence of toxic and hazardous substances.In this study,a new environmentally friendly hydro-metallurgical process was proposed for leaching lithium(Li),nickel(Ni),cobalt(Co),and manganese(Mn)from spent LIBs using sulfuric acid with citric acid as a reductant.The effects of the concentration of sulfuric acid,the leaching temperature,the leaching time,the solid-liquid ratio,and the reducing agent dosage on the leaching behavior of the above elements were investigated.Key parameters were optimized using response surface methodology(RSM)to maximize the recovery of metals from spent LIBs.The maxim-um recovery efficiencies of Li,Ni,Co,and Mn can reach 99.08%,98.76%,98.33%,and 97.63%.under the optimized conditions(the sulfuric acid concentration was 1.16 mol/L,the citric acid dosage was 15wt%,the solid-liquid ratio was 40 g/L,and the temperature was 83℃ for 120 min),respectively.It was found that in the collaborative leaching process of sulfuric acid and citric acid,the citric acid initially provided strong reducing CO_(2)^(-),and the transition metal ions in the high state underwent a reduction reaction to produce transition metal ions in the low state.Additionally,citric acid can also act as a proton donor and chelate with lower-priced transition metal ions,thus speeding up the dissolution process.展开更多
To realize the resource utilization of the valuable metals in the titanium-containing blast furnace slag,the process route of “hydrochloric acid leaching-electrolysis-carbonization and carbon dioxide capture-preparat...To realize the resource utilization of the valuable metals in the titanium-containing blast furnace slag,the process route of “hydrochloric acid leaching-electrolysis-carbonization and carbon dioxide capture-preparation of calcium carbonate” was proposed.In this study,the influences of process conditions on the leaching rates of calcium,magnesium,aluminum,and iron and the phases of the leaching residue were investigated for the leaching process.The experimental results show that the HCl solution could selectively leach the elements from the titanium-containing blast furnace slag.The better leaching conditions are the HCl solution concentration of 4 mol/L,the leaching time of 30 min,the ratio of liquid volume to solid gas of 10 mL/g,and the stirring paddle speed of 300 r/min.Under the conditions,the leaching rates of calcium,magnesium,aluminum,and iron can reach 85.87%,73.41%,81.35%,and 59.08%,and the leaching rate of titanium is 10.71%.The iron and the aluminum are removed from the leachate to obtain iron-aluminum water purification agents,and the magnesium is removed from the leachate to obtain magnesium hydroxide.The leaching residue phase is dominated by perovskite,followed by magnesium silicate and tricalcium aluminate,and the titaniumrich material could be obtained from the leaching residue by desiliconization.展开更多
The preparation process of sodium molybdate has the disadvantages of high energy consumption,low thermal efficiency,and high raw material requirement of molybdenum trioxide,in order to realize the green and efficient ...The preparation process of sodium molybdate has the disadvantages of high energy consumption,low thermal efficiency,and high raw material requirement of molybdenum trioxide,in order to realize the green and efficient development of molybdenum concentrate resources,this paper proposes a new process for efficient recovery of molybdenum from molybdenum concentrate and preparation of sodium molybdate by microwave-enhanced roasting and alkali leaching.Thermodynamic analysis indicated the feasibility of oxidation roasting of molybdenum concentrate.The effects of roasting temperature,holding time,and power-to-mass ratio on the oxidation product and leaching product sodium molybdate (Na_(2)MoO_(4)·2H_(2)O) were investigated.Under the optimal process conditions:roasting temperature of 700℃,holding time of 110 min,and power-to-mass ratio of 110 W/g,the molybdenum state of existence was converted from MoS_(2) to Mo O3.The process of preparing sodium molybdate by alkali leaching of molybdenum calcine was investigated,the optimal leaching conditions include a solution concentration of 2.5 mol/L,a liquid-to-solid ratio of 2 mL/g,a leaching temperature of 60℃,and leaching solution termination at pH 8.The optimum conditions result in a leaching rate of sodium molybdate of 96.24%.Meanwhile,the content of sodium molybdate reaches 94.08wt%after leaching and removing impurities.Iron and aluminum impurities can be effectively separated by adjusting the pH of the leaching solution with sodium carbonate solution.This research avoids the shortcomings of the traditional process and utilizes the advantages of microwave metallurgy to prepare high-quality sodium molybdate,which provides a new idea for the highvalue utilization of molybdenum concentrate.展开更多
The necessity to saline and sodic waters is sometimes used for irrigating agricultural activities under certain circumstances, but it is important to note that the use of these waters comes with specific consideration...The necessity to saline and sodic waters is sometimes used for irrigating agricultural activities under certain circumstances, but it is important to note that the use of these waters comes with specific considerations and limitations. One way to decrease undesirable effects of sodic waters on the physical and chemical properties of soils is to apply organic and chemical amendments within the soil. This study aimed to assess the effectiveness of saline water on soil acidity, alkalinity and nutrients leaching in sandy loamy soil at Bella flower farm, in Rwamagana District, Rwanda. The water used was from the Muhazi Lake which is classified as Class I (Saline water quality). Column leaching experiments using treated soils were then conducted under saturated conditions. The soil under experimental was first analyzed for its textural classification, soil properties and is classified as sandy loamy soil. The t-test was taken at 1%, 5% and 10% levels of statistical significance compared to control soil. The results indicated that the application of saline water to soils caused an increase in some soil nutrients like increase of Phosphorus (P), Potassium (K<sup>+</sup>), Magnesium (Mg2<sup>+</sup>), Sulphur (S), CN ratio and Sodium (Na<sup>+</sup>) and decreased soil texture, physical and chemical properties and remained soil nutrients. Consequently, the intensive addition of saline water leachates to soil in PVC pipes led to decreased of soil EC through leaching and a raiser Soluble Sodium Percentage (SSP). The rate of saline water application affected the increase accumulation of SAR and Na% in the top soil layers. The study indicated that saline water is an inefficient amendment for sandy soil with saline water irrigation. The study recommends further studies with similar topic with saline water irrigation, as it accentuated the alkalinity levels.展开更多
Currently,the process of extracting rubidium from ores has attracted a great deal of attention due to the increasing application of rubidium in high-technology field.A novel process for the comprehensive utilization o...Currently,the process of extracting rubidium from ores has attracted a great deal of attention due to the increasing application of rubidium in high-technology field.A novel process for the comprehensive utilization of rubidium ore resources is proposed in this paper.The process consists mainly of mineral dissociation,selective leaching,and desilication.The results showed that the stable silicon–oxygen tetrahedral structure of the rubidium ore was completely disrupted by thermal activation and the mineral was completely dissociated,which was conducive to subsequent selective leaching.Under the optimal conditions,extractions of 98.67% Rb and 96.23%K were obtained by leaching the rubidium ore.Moreover,the addition of a certain amount of activated Al(OH)_(3) during leaching can effectively inhibit the leaching of silicon.In the meantime,the leach residue was sodalite,which was successfully synthesized to zeolite A by hydrothermal conversion.The proposed process provided a feasible strategy for the green extraction of rubidium and the sustainable utilization of various resources.展开更多
Microwave heating can rapidly and uniformly raise the temperature and accelerate the reaction rate.In this paper,microwave heating was used to improve the acid leaching,and the mechanism was investigated via microscop...Microwave heating can rapidly and uniformly raise the temperature and accelerate the reaction rate.In this paper,microwave heating was used to improve the acid leaching,and the mechanism was investigated via microscopic morphology analysis and numerical simulation by COMSOL Multiphysics software.The effects of the microwave power,leaching temperature,CaF_(2) dosage,H_(2)SO_(4) concentration,and leaching time on the vanadium recovery were investigated.A vanadium recovery of 80.66%is obtained at a microwave power of 550 W,leaching temperature of 95℃,CaF_(2) dosage of 5wt%,H_(2)SO_(4) concentration of 20vol%,and leaching time of 2.5 h.Compared with conventional leaching technology,the vanadium recovery increases by 6.18%,and the leaching time shortens by 79.17%.More obvious pulverization of shale particles and delamination of mica minerals happen in the microwave-assisted leaching process.Numerical simulation results show that the temperature of vanadium shales increases with an increase in electric field(E-field).The distributions of E-field and temperature among vanadium shale particles are relatively uniform,except for the higher content at the contact position of the particles.The analysis results of scaleup experiments and leaching experiments indicate high-temperature hot spots in the process of microwave-assisted leaching,and the local high temperature destroys the mineral structure and accelerates the reaction rate.展开更多
Efficient and low-cost recycling of spent lithium iron phosphate(LiFePO_(4),LFP)batteries has become an inevitable trend.In this study,an integrated closed-loop recycling strategy including isomorphic substitution lea...Efficient and low-cost recycling of spent lithium iron phosphate(LiFePO_(4),LFP)batteries has become an inevitable trend.In this study,an integrated closed-loop recycling strategy including isomorphic substitution leaching and solvent extraction process for spent LFP was proposed.An inexpensive FeCl_(3)was used as leaching agent to directly substitute Fe^(2+)from LFP.99%of Li can be rapidly leached in just 30 min,accompanied by 98%of FePO_(4)precipitated in lixivium.The tri-n-butyl phosphate(TBP)-sulfonated kerosene(SK)system was applied to extract Li from lixivium through a twelve-stage countercurrent process containing synchronous extraction and stepwise stripping of Li^(+)and Fe^(3+).80.81%of Li can be selectively enriched in stripping liquor containing 3.059 mol·L^(-1)of Li^(+)under optimal conditions.And the Fe stripping liquor was recovered for LFP re-leaching,of which,Fe^(2+)was oxidized to Fe^(3+)by appropriate H_(2)O_(2).Raffinate and lixivium were concentrated and entered into extraction process to accomplished closeloop recycling process.Overall,the results suggest that more than 99%of Li was recovered.FeCl_(3)holding in solution was directly regenerated without any pollutant emission.The sustainable mothed would be an alternative candidate for total element recycling of spent LFP batteries with industrial potential.展开更多
Coal gasification slag(CGS)is a type of solid waste produced during coal gasification,in which heavy metals severely restrict its resource utilization.In this work,the mineral occurrence and distribution of typical he...Coal gasification slag(CGS)is a type of solid waste produced during coal gasification,in which heavy metals severely restrict its resource utilization.In this work,the mineral occurrence and distribution of typical heavy metal Cr in CGS is investigated.The leaching behavior of Cr under different conditions is studied in detail.Acid leaching-selective oxidation-coprecipitation method is proposed based on the characteristics of Cr in CGS.The detoxification of Cr in CGS is realized,and the detoxification mechanism is clarified.Results show that Cr is highly enriched in CGS.The speciation of Cr is mainly residual fraction(74.47%-86.12%),which is combined with amorphous aluminosilicate.Cr^(3+)and Cr^(6+)account for 90.93%-94.82%and 5.18%-9.07%of total Cr,respectively.High acid concentration and high liquid-solid ratio are beneficial to destroy the lattice structure of amorphous aluminosilicate,thus improving the leaching efficiency of Cr,which can reach 97.93%under the optimal conditions.Acid leaching-selective oxidation-coprecipitation method can realize the detoxification of Cr in CGS.Under the optimal conditions,the removal rates of Fe^(3+)and Cr^(3+)in the leaching solution are 80.99%-84.79%and 70.58%-71.69%,respectively,while the loss rate of Al^(3+)is only 1.10%-3.35%.Detoxification slag exists in the form of Fe-Cr coprecipitation(Fe_(1-x)Cr_xOOH),which can be used for smelting.The detoxification acid leaching solution can be used to prepare inorganic polymer composite coagulant poly-aluminum chloride(PAC).This study can provide theoretical and data guidance for detoxification of heavy metal Cr in CGS and achieve resource utilization of coal gasification solid waste.展开更多
The purpose of this work was to fabricate three-dimensional porous scaffolds by using the salt leaching technique.This technique is simple and it does not need the pressure or dislike expensive equipment.The study sel...The purpose of this work was to fabricate three-dimensional porous scaffolds by using the salt leaching technique.This technique is simple and it does not need the pressure or dislike expensive equipment.The study selected polycaprolactone blended with carboxymethylcellulose that is the additive.The ratios of them were derived from mixture design in Minitab program that was 98/2(P1),93.5/6.5(P2),89/11(P3),84.5/15.5(P4),and 80/20(P5),respectively.The scanning electron microscopy(SEM)was applied to assess the physical properties and the pore size dimension of the scaffold from SEM micrographs.The results of SEM present the scaffolds happened interconnected porous structures that are found in all of the P1-P5 samples.The pore size dimension of all sample scaffolds is in the range of 264.11-348.28μm.Whereas the largest and the smallest of pore size are the sample of P3 and P2,respectively,while the porosity ranges from 98.06%-98.88%that the sample of P5 is the greatest and the sample of P4 is the slightly lowest.In conclusion,the blended PCL/CMC scaffolds P1-P5 were formed by salt leaching technique suitable to use in tissue engineering application.However,the amount of CMC blended with PCL should be reasonable in order to adjust the hydrophilic of the scaffold.展开更多
The bond film on the surface of the CO_(2) sodium silicate used sands is not easy to decompose,therefore,it is difficult to reclaim used sands.A new reclamation method of CO_(2) sodium silicate used sands was develope...The bond film on the surface of the CO_(2) sodium silicate used sands is not easy to decompose,therefore,it is difficult to reclaim used sands.A new reclamation method of CO_(2) sodium silicate used sands was developed by steam leaching,which can reduce the water consumption of reclamation and improve the removal effect of sodium silicate bond film.Firstly,the leaching effect of the sodium silicate sands after 20/200/400/600/800/1,000°C heat preservation treatment was simulated.Furthermore,the influence of the leaching time on the removal effect of the sodium silicate bond film was studied.Finally,the casting properties of the reclaimed sands after the leaching reclamation treatment were tested.The results show for simulated used sands after 30 min of steam leaching,the removal ratio of the alkali exceeds 84.1%,the removal ratio of silicate is 86.2%,and the removal ratio of carbonate is 93.6%.The removal rate of alkali,silicate and carbonate is relatively low in the leaching time of 30-50 min.Considering the reclamation effect and cost,the leaching time is controlled in 30 min.Water consumption is only 60%of the mass of used sands for 30 min steam leaching,while it is 200%for wet reclamation.Morphological analysis shows that most of the hazardous substances in the used sands are removed in 30 min steam leaching,and the reclaimed sands surface after steam leaching in 50 min is as smooth as new sands.After 30 min of steam leaching,the alkali removal effect of the factory used sands can reach 81.5%,the water consumption by the steam leaching reclamation is 58%of the mass of the used sand,which is similar to the result of simulated used sands.The performance of reclaimed sands obtained after 30 min steam leaching is better than that of new sands when the amount of sodium silicate added is 6%of the mass of the reclaimed sands and the CO_(2) blowing time is 15 s:the 24 h ultimate compressive strength of reclaimed sands is 5.6 MPa(equated with new sands),and the collapsibility compressive strength is 5.2 MPa,which is lower than the collapsibility compressive strength of new sands(7.7 MPa).This indicates that the reclamation of CO_(2) sodium silicate used sands by steam leaching is a feasible method.展开更多
Under the new development philosophy of carbon peaking and carbon neutrality,CO_(2)and O_(2)in situ leaching(ISL)has been identified as a promising technique for uranium mining in China,not only because it solves carb...Under the new development philosophy of carbon peaking and carbon neutrality,CO_(2)and O_(2)in situ leaching(ISL)has been identified as a promising technique for uranium mining in China,not only because it solves carbon dioxide utilization and sequestration,but it also alleviates the environmental burden.However,significant challenges exist in assessment of CO_(2)footprint and water-rock interactions,due to complex geochemical processes.Herein this study conducts a three-dimensional,multicomponent reactive transport model(RTM)of a field-scale CO_(2)and O_(2)ISL process at a typical sandstone-hosted uranium deposit in Songliao Basin,China.Numerical simulations are performed to provide new insight into quantitative interpretation of the greenhouse gas(CO_(2))footprint and environmental impact(SO_(4)^(2–))of the CO_(2)and O_(2)ISL,considering the potential chemical reaction network for uranium recovery at the field scale.RTM results demonstrate that the fate of the CO_(2)could be summarized as injected CO_(2)dissolution,dissolved CO_(2)mineralization and storage of CO_(2)as a gas phase during the CO_(2)and O_(2)ISL process.Furthermore,compared to acid ISL,CO_(2)and O_(2)ISL has a potentially smaller environmental footprint,with 20%of SO_(4)^(2–)concentration in the aquifer.The findings improve our fundamental understanding of carbon utilization in a long-term CO_(2)and O_(2)ISL system and provide important environmental implications when considering complex geochemical processes.展开更多
Soil salinity is a serious land degradation issue in agriculture.It is a major threat to agriculture productivity.Extra irrigation water is applied to leach down the salts from the root zone of the plants in the form ...Soil salinity is a serious land degradation issue in agriculture.It is a major threat to agriculture productivity.Extra irrigation water is applied to leach down the salts from the root zone of the plants in the form of a Leaching fraction(LF)of irrigation water.For the leaching process to be effective,the LF of irriga-tion water needs to be adjusted according to the environmental conditions and soil salinity level in the form of Evapotranspiration(ET)rate.The relationship between environmental conditions and ET rate is hard to be defined by a linear relationship and data-driven Machine learning(ML)based decisions are required to determine the calibrated Evapotranspiration(ETc)rate.ML-assisted ETc is pro-posed to adjust the LF according to the ETc and soil salinity level.A regression model is proposed to determine the ETc rate according to the prevailing tempera-ture,humidity,and sunshine,which would be used to determine the smart LF according to the ETc and soil salinity level.The proposed model is trained and tested against the Blaney Criddle method of Reference evapotranspiration(ETo)determination.The validation of the model from the test dataset reveals the accu-racy of the ML model in terms of Root mean squared errors(RMSE)are 0.41,Mean absolute errors(MAE)are 0.34,and Mean squared errors(MSE)are 0.28 mm day-1.The applications of the proposed solution in a real-time environ-ment show that the LF by the proposed solution is more effective in reducing the soil salinity as compared to the traditional process of leaching.展开更多
Rare earth elements are indispensable raw materials for advanced aero-engines, special optical materials, and high-performance electronic products. With the development of the social economy, the global demand for rar...Rare earth elements are indispensable raw materials for advanced aero-engines, special optical materials, and high-performance electronic products. With the development of the social economy, the global demand for rare earth resources is increasing, and rare earths have become a key metal for the development of new industries and frontier technologies that are highly valued both at home and abroad. Ion-adsorbed rare earth ores are an important source of rare earths, so the efficient green leaching of ion-adsorbed rare earths is important. Researchers found that the selection of an efficient green leaching agent for ion-adsorbed rare earths is based on the zeta potential of tailing clay minerals in addition to leaching efficiency, and both zeta potential and leaching ion concentration are related to mineral acidity and alkalinity, and the pH of tailing water suspension is a direct indicator of environmental water quality requirements. Therefore, the efficiency of the leaching process is closely integrated with the environmental evaluation, and the characteristics and correlation of the changes in zeta potential, pH, conductivity and pollutant concentration of the pulp of clay mineral content during the leaching process of ore leaching and tailings aqueous electrolyte solution leaching are studied by evaluating the leaching system, and a set of correlation leaching efficiency and environmental impact evaluation method is established based on the results of the above analysis, which is of scientific development of ion adsorption rare earth resources. It has important theoretical significance and practical application value.展开更多
Compared with the traditional pyrometallurgical process, copper bioleaching has distinctive advantages of high efficiency and lower cost, enabling efficiently extracts of valuable metal resources from copper sulfides....Compared with the traditional pyrometallurgical process, copper bioleaching has distinctive advantages of high efficiency and lower cost, enabling efficiently extracts of valuable metal resources from copper sulfides. Moreover, during long-term industrial applications of bioleaching, many regulatory enhancements and technological methods are used to accelerate the interfacial reactions. With advances in microbial genetic and sequencing technologies, bacterial communities and their mechanisms in bioleaching systems have been revealed gradually. The bacterial proliferation and dissolution of sulfide ores by a bacterial community depends on the pH, temperature, oxygen, reaction product regulation, additives, and passivation substances, among other factors. The internal relationship among the influencing factors and the succession of microorganism diversity are discussed and reviewed in this paper. This paper is intended to provide a good reference for studies related to enhanced bioleaching.展开更多
Coal gangue is the main pollution source of mining areas.When coal gangue is stacked and recycled,the heavy metal elements contained in it are released by natural weathering and leaching,which causes damage to the sur...Coal gangue is the main pollution source of mining areas.When coal gangue is stacked and recycled,the heavy metal elements contained in it are released by natural weathering and leaching,which causes damage to the surrounding ecological environment.In this study,the leaching and precipitation characteristics of heavy metals in low-sulfur coal gangue under different environmental conditions were simulated by indoor dynamic leaching experiments,which provided a theoretical basis for environmental restoration of the mining area.The conclusions are as follows:higher heavy metal content in low-sulfur coal gangue is associated with greater,leaching of heavy metals;acidic conditions promote the release of heavy metals in low-sulfur coal gangue;and more precipitation is associated with better release of heavy metals from the low-sulfur coal gangue.展开更多
In this work,sodium dicyanamide(SD)was used as a leaching reagent for gold recovery,and the effects of the SD dosage and solution pH on the gold-leaching performance were investigated.A gold recovery of 34.8%was obtai...In this work,sodium dicyanamide(SD)was used as a leaching reagent for gold recovery,and the effects of the SD dosage and solution pH on the gold-leaching performance were investigated.A gold recovery of 34.8%was obtained when SD was used as the sole leaching reagent at a dosage of 15 kg/t.In the presence of a certain amount of potassium ferrocyanide(PF)in the SD solution,the gold recovery was found to increase from 34.8%to 57.08%.Using the quartz crystal microbalance with dissipation(QCM-D)technique,the leaching kinetics of SD with and without PF were studied.The QCM-D results indicate that the gold-leaching rate increased from 4.03 to 39.99 ng·cm^(–2)·min^(–1) when the SD concentration was increased from 0 to 0.17 mol/L,and increased from 39.99 to 272.62 ng·cm^(–2)·min^(–1) when 0.1 mol/L of PF was used in combination with SD.The pregnant solution in the leaching tests was characterized by X-ray photoelectron spectroscopy and electrospray mass spectrometry,which indicated that Au and(N(CN)2)–in the SD solution formed a series of metal complex ions,[AuNax(N(CN)2)x+2]–(x=1,2,3,or 4).展开更多
A laboratory leaching experiment with samples of different grades was carried out, and an analytical method of concentration of leaching solution was put forward. For each sample, respectively, by applying phase space...A laboratory leaching experiment with samples of different grades was carried out, and an analytical method of concentration of leaching solution was put forward. For each sample, respectively, by applying phase space reconstruction for time series of monitoring data, the saturated embedding dimension and the correlation dimension were obtained, and the evolution laws between neighboring points in the reconstructed phase space were revealed. With BP neural network, a prediction model of concentration of leaching solution was set up and the maximum error of which was less than 2%. The results show that there exist chaotic characteristics in leaching system, and samples of different grades have different nonlinear dynamic features; the higher the grade of sample, the smaller the correlation dimension; furthermore, the maximum Lyapunov index, energy dissipation and chaotic extent of the leaching system increase with grade of the sample; by phase space reconstruction, the subtle change features of concentration of leaching solution can be magnified and the inherent laws can be fully demonstrated. According to the laws, a prediction model of leaching cycle period has been established to provide a theoretical foundation for solution mining.展开更多
An ammonia-based system was used to selectively leach cobalt(Co)from an African high-silicon low-grade Co ore,and the other elemental impurities were inhibited from leaching in this process.This process was simple and...An ammonia-based system was used to selectively leach cobalt(Co)from an African high-silicon low-grade Co ore,and the other elemental impurities were inhibited from leaching in this process.This process was simple and environmentally friendly.The results revealed that the leaching ratio of Co can reach up to 95.61%using(NH_(4))_(2)SO_(4)as a leaching agent under the following materials and conditions:(NH_(4))_(2)SO_(4)concentration 300 g/L,reductant dosage 0.7 g,leaching temperature 353 K,reaction time 4 h,and liquid-solid ratio 6 mL/g.The leaching kinetics of Co showed that the apparent activation energy of Co leaching was 76.07 kJ/mol(i.e.,in the range of 40-300 kJ/mol).This indicated that the leaching of Co from the Co ore was controlled by an interfacial chemical reaction,and then the developed leaching kinetics model of the Co can be expressed as 1-(1-α)^(1/3)=28.01×10~3×r_0^(-1)×C_((NH_(4))_(2)SO_(4))^(1.5)×exp(-76073/8.314 T)×t,whereαis the leaching ratio(%)of Co,r_0 is the average radius(m)of the Co ore particles,T is the temperature(K),and C_((NH_(4))_(2)SO_(4))is the initial reactant concentration(kg/m^(3)).展开更多
A mathematical model for heap bioleaching is developed to analyze heat transfer,oxygen flow,target ion distribution and oxidation leaching rate in the heap.The model equations are solved with Comsol Multiphysics softw...A mathematical model for heap bioleaching is developed to analyze heat transfer,oxygen flow,target ion distribution and oxidation leaching rate in the heap.The model equations are solved with Comsol Multiphysics software.Numerical simulation results show the following facts:Concentration of oxygen is relatively high along the boundary of the slope,and low in the center part where leaching rate is slow.Temperature is relatively low along the slope and reaches the highest along the bottom region near the slope,with difference being more than 6 C.Concentration of target mental ions is the highest in the bottom region near the slope.Oxidation leaching rate is relatively large in the bottom and slope part with a fast reaction rate,and small in the other part with low oxygen concentration.展开更多
基金jointly supported by the National Key Research and Development Program of China (2019YFC1905800)the National Key Research & Development Program of China (2018YFC1903500)+4 种基金the commercial project by Beijing Zhong Dian Hua Yuan Environment Protection Technology Co., Ltd. (E01211200005)the Regional key projects of the science and technology service network program (STS program) of the Chinese Academy of Sciences (KFJ-STS-QYZD-153)the Ningbo Science and Technology Innovation Key Projects (2020Z099, 2022Z028)the Ningbo Municipal Commonweal Key Program (2019C10033)the support of Mineral Resources Analytical and Testing Center, Institute of Process Engineering, Chinese Academy of Science
文摘To achieve the resource utilization of solid waste phosphogypsum(PG)and tackle the problem of utilizing potassium feldspar(PF),a coupled synergistic process between PG and PF is proposed in this paper.The study investigates the features of P and F in PG,and explores the decomposition of PF using hydrofluoric acid(HF)in the sulfuric acid system for K leaching and leaching of P and F in PG.The impact factors such as sulfuric acid concentration,reaction temperature,reaction time,material ratio(PG/PF),liquid–solid ratio,PF particle size,and PF calcination temperature on the leaching of P and K is systematically investigated in this paper.The results show that under optimal conditions,the leaching rate of K and P reach more than 93%and 96%,respectively.Kinetics study using shrinking core model(SCM)indicates two significant stages with internal diffusion predominantly controlling the leaching of K.The apparent activation energies of these two stages are 11.92 kJ·mol^(-1)and 11.55 kJ·mol^(-1),respectively.
基金supported by Key R&D Program of Zhejiang Province,China (No.2022C03061)the National Natural Science Foundation of China (No.52074204)the Fundamental Research Funds for the Central Universities (No.2023-vb-032).
文摘The proper recycling of spent lithium-ion batteries(LIBs)can promote the recovery and utilization of valuable resources,while also negative environmental effects resulting from the presence of toxic and hazardous substances.In this study,a new environmentally friendly hydro-metallurgical process was proposed for leaching lithium(Li),nickel(Ni),cobalt(Co),and manganese(Mn)from spent LIBs using sulfuric acid with citric acid as a reductant.The effects of the concentration of sulfuric acid,the leaching temperature,the leaching time,the solid-liquid ratio,and the reducing agent dosage on the leaching behavior of the above elements were investigated.Key parameters were optimized using response surface methodology(RSM)to maximize the recovery of metals from spent LIBs.The maxim-um recovery efficiencies of Li,Ni,Co,and Mn can reach 99.08%,98.76%,98.33%,and 97.63%.under the optimized conditions(the sulfuric acid concentration was 1.16 mol/L,the citric acid dosage was 15wt%,the solid-liquid ratio was 40 g/L,and the temperature was 83℃ for 120 min),respectively.It was found that in the collaborative leaching process of sulfuric acid and citric acid,the citric acid initially provided strong reducing CO_(2)^(-),and the transition metal ions in the high state underwent a reduction reaction to produce transition metal ions in the low state.Additionally,citric acid can also act as a proton donor and chelate with lower-priced transition metal ions,thus speeding up the dissolution process.
基金Funded by the National Natural Science Foundation of China Youth Fund(No.52204419)the Liaoning Provincial Natural Science Foundation(No.2022-BS-076)the Guangxi Science and Technology Major Project(No.2021AA12013)。
文摘To realize the resource utilization of the valuable metals in the titanium-containing blast furnace slag,the process route of “hydrochloric acid leaching-electrolysis-carbonization and carbon dioxide capture-preparation of calcium carbonate” was proposed.In this study,the influences of process conditions on the leaching rates of calcium,magnesium,aluminum,and iron and the phases of the leaching residue were investigated for the leaching process.The experimental results show that the HCl solution could selectively leach the elements from the titanium-containing blast furnace slag.The better leaching conditions are the HCl solution concentration of 4 mol/L,the leaching time of 30 min,the ratio of liquid volume to solid gas of 10 mL/g,and the stirring paddle speed of 300 r/min.Under the conditions,the leaching rates of calcium,magnesium,aluminum,and iron can reach 85.87%,73.41%,81.35%,and 59.08%,and the leaching rate of titanium is 10.71%.The iron and the aluminum are removed from the leachate to obtain iron-aluminum water purification agents,and the magnesium is removed from the leachate to obtain magnesium hydroxide.The leaching residue phase is dominated by perovskite,followed by magnesium silicate and tricalcium aluminate,and the titaniumrich material could be obtained from the leaching residue by desiliconization.
基金financially supported by the National Natural Science Foundation of China (No.51964046)。
文摘The preparation process of sodium molybdate has the disadvantages of high energy consumption,low thermal efficiency,and high raw material requirement of molybdenum trioxide,in order to realize the green and efficient development of molybdenum concentrate resources,this paper proposes a new process for efficient recovery of molybdenum from molybdenum concentrate and preparation of sodium molybdate by microwave-enhanced roasting and alkali leaching.Thermodynamic analysis indicated the feasibility of oxidation roasting of molybdenum concentrate.The effects of roasting temperature,holding time,and power-to-mass ratio on the oxidation product and leaching product sodium molybdate (Na_(2)MoO_(4)·2H_(2)O) were investigated.Under the optimal process conditions:roasting temperature of 700℃,holding time of 110 min,and power-to-mass ratio of 110 W/g,the molybdenum state of existence was converted from MoS_(2) to Mo O3.The process of preparing sodium molybdate by alkali leaching of molybdenum calcine was investigated,the optimal leaching conditions include a solution concentration of 2.5 mol/L,a liquid-to-solid ratio of 2 mL/g,a leaching temperature of 60℃,and leaching solution termination at pH 8.The optimum conditions result in a leaching rate of sodium molybdate of 96.24%.Meanwhile,the content of sodium molybdate reaches 94.08wt%after leaching and removing impurities.Iron and aluminum impurities can be effectively separated by adjusting the pH of the leaching solution with sodium carbonate solution.This research avoids the shortcomings of the traditional process and utilizes the advantages of microwave metallurgy to prepare high-quality sodium molybdate,which provides a new idea for the highvalue utilization of molybdenum concentrate.
文摘The necessity to saline and sodic waters is sometimes used for irrigating agricultural activities under certain circumstances, but it is important to note that the use of these waters comes with specific considerations and limitations. One way to decrease undesirable effects of sodic waters on the physical and chemical properties of soils is to apply organic and chemical amendments within the soil. This study aimed to assess the effectiveness of saline water on soil acidity, alkalinity and nutrients leaching in sandy loamy soil at Bella flower farm, in Rwamagana District, Rwanda. The water used was from the Muhazi Lake which is classified as Class I (Saline water quality). Column leaching experiments using treated soils were then conducted under saturated conditions. The soil under experimental was first analyzed for its textural classification, soil properties and is classified as sandy loamy soil. The t-test was taken at 1%, 5% and 10% levels of statistical significance compared to control soil. The results indicated that the application of saline water to soils caused an increase in some soil nutrients like increase of Phosphorus (P), Potassium (K<sup>+</sup>), Magnesium (Mg2<sup>+</sup>), Sulphur (S), CN ratio and Sodium (Na<sup>+</sup>) and decreased soil texture, physical and chemical properties and remained soil nutrients. Consequently, the intensive addition of saline water leachates to soil in PVC pipes led to decreased of soil EC through leaching and a raiser Soluble Sodium Percentage (SSP). The rate of saline water application affected the increase accumulation of SAR and Na% in the top soil layers. The study indicated that saline water is an inefficient amendment for sandy soil with saline water irrigation. The study recommends further studies with similar topic with saline water irrigation, as it accentuated the alkalinity levels.
基金financially supported by the National Natural Science Foundation of China(Nos.U1802253 and 52034002)the Fundamental Research Funds for the Central Universities,China(No.FRF-TT-19-001)。
文摘Currently,the process of extracting rubidium from ores has attracted a great deal of attention due to the increasing application of rubidium in high-technology field.A novel process for the comprehensive utilization of rubidium ore resources is proposed in this paper.The process consists mainly of mineral dissociation,selective leaching,and desilication.The results showed that the stable silicon–oxygen tetrahedral structure of the rubidium ore was completely disrupted by thermal activation and the mineral was completely dissociated,which was conducive to subsequent selective leaching.Under the optimal conditions,extractions of 98.67% Rb and 96.23%K were obtained by leaching the rubidium ore.Moreover,the addition of a certain amount of activated Al(OH)_(3) during leaching can effectively inhibit the leaching of silicon.In the meantime,the leach residue was sodalite,which was successfully synthesized to zeolite A by hydrothermal conversion.The proposed process provided a feasible strategy for the green extraction of rubidium and the sustainable utilization of various resources.
基金supported by the National Natural Science Foundation of China(No.51904211)the National Natural Science Foundation of China(No.52004187)。
文摘Microwave heating can rapidly and uniformly raise the temperature and accelerate the reaction rate.In this paper,microwave heating was used to improve the acid leaching,and the mechanism was investigated via microscopic morphology analysis and numerical simulation by COMSOL Multiphysics software.The effects of the microwave power,leaching temperature,CaF_(2) dosage,H_(2)SO_(4) concentration,and leaching time on the vanadium recovery were investigated.A vanadium recovery of 80.66%is obtained at a microwave power of 550 W,leaching temperature of 95℃,CaF_(2) dosage of 5wt%,H_(2)SO_(4) concentration of 20vol%,and leaching time of 2.5 h.Compared with conventional leaching technology,the vanadium recovery increases by 6.18%,and the leaching time shortens by 79.17%.More obvious pulverization of shale particles and delamination of mica minerals happen in the microwave-assisted leaching process.Numerical simulation results show that the temperature of vanadium shales increases with an increase in electric field(E-field).The distributions of E-field and temperature among vanadium shale particles are relatively uniform,except for the higher content at the contact position of the particles.The analysis results of scaleup experiments and leaching experiments indicate high-temperature hot spots in the process of microwave-assisted leaching,and the local high temperature destroys the mineral structure and accelerates the reaction rate.
基金financially supported by the National Natural Science Foundation of China(U1707601)project of Youth Innovation Promotion Association,Chinese Academy of Sciences(2021430)+1 种基金project of Innovation Academy for Green Manufacture,Chinese Academy of Sciences(IAGM2020C26)project of Bureau of International Cooperation,Chinese Academy of Sciences(122363KYSB20190033)。
文摘Efficient and low-cost recycling of spent lithium iron phosphate(LiFePO_(4),LFP)batteries has become an inevitable trend.In this study,an integrated closed-loop recycling strategy including isomorphic substitution leaching and solvent extraction process for spent LFP was proposed.An inexpensive FeCl_(3)was used as leaching agent to directly substitute Fe^(2+)from LFP.99%of Li can be rapidly leached in just 30 min,accompanied by 98%of FePO_(4)precipitated in lixivium.The tri-n-butyl phosphate(TBP)-sulfonated kerosene(SK)system was applied to extract Li from lixivium through a twelve-stage countercurrent process containing synchronous extraction and stepwise stripping of Li^(+)and Fe^(3+).80.81%of Li can be selectively enriched in stripping liquor containing 3.059 mol·L^(-1)of Li^(+)under optimal conditions.And the Fe stripping liquor was recovered for LFP re-leaching,of which,Fe^(2+)was oxidized to Fe^(3+)by appropriate H_(2)O_(2).Raffinate and lixivium were concentrated and entered into extraction process to accomplished closeloop recycling process.Overall,the results suggest that more than 99%of Li was recovered.FeCl_(3)holding in solution was directly regenerated without any pollutant emission.The sustainable mothed would be an alternative candidate for total element recycling of spent LFP batteries with industrial potential.
基金finally supported by the National Natural Science Foundation of China(52174390,U1810205)Innovation Academy for Green Manufacture of the Chinese Academy of Sciences China(IAGM2022D04)Strategic Priority Research Program of the Chinese Academy of Sciences China(XDA21040601)。
文摘Coal gasification slag(CGS)is a type of solid waste produced during coal gasification,in which heavy metals severely restrict its resource utilization.In this work,the mineral occurrence and distribution of typical heavy metal Cr in CGS is investigated.The leaching behavior of Cr under different conditions is studied in detail.Acid leaching-selective oxidation-coprecipitation method is proposed based on the characteristics of Cr in CGS.The detoxification of Cr in CGS is realized,and the detoxification mechanism is clarified.Results show that Cr is highly enriched in CGS.The speciation of Cr is mainly residual fraction(74.47%-86.12%),which is combined with amorphous aluminosilicate.Cr^(3+)and Cr^(6+)account for 90.93%-94.82%and 5.18%-9.07%of total Cr,respectively.High acid concentration and high liquid-solid ratio are beneficial to destroy the lattice structure of amorphous aluminosilicate,thus improving the leaching efficiency of Cr,which can reach 97.93%under the optimal conditions.Acid leaching-selective oxidation-coprecipitation method can realize the detoxification of Cr in CGS.Under the optimal conditions,the removal rates of Fe^(3+)and Cr^(3+)in the leaching solution are 80.99%-84.79%and 70.58%-71.69%,respectively,while the loss rate of Al^(3+)is only 1.10%-3.35%.Detoxification slag exists in the form of Fe-Cr coprecipitation(Fe_(1-x)Cr_xOOH),which can be used for smelting.The detoxification acid leaching solution can be used to prepare inorganic polymer composite coagulant poly-aluminum chloride(PAC).This study can provide theoretical and data guidance for detoxification of heavy metal Cr in CGS and achieve resource utilization of coal gasification solid waste.
文摘The purpose of this work was to fabricate three-dimensional porous scaffolds by using the salt leaching technique.This technique is simple and it does not need the pressure or dislike expensive equipment.The study selected polycaprolactone blended with carboxymethylcellulose that is the additive.The ratios of them were derived from mixture design in Minitab program that was 98/2(P1),93.5/6.5(P2),89/11(P3),84.5/15.5(P4),and 80/20(P5),respectively.The scanning electron microscopy(SEM)was applied to assess the physical properties and the pore size dimension of the scaffold from SEM micrographs.The results of SEM present the scaffolds happened interconnected porous structures that are found in all of the P1-P5 samples.The pore size dimension of all sample scaffolds is in the range of 264.11-348.28μm.Whereas the largest and the smallest of pore size are the sample of P3 and P2,respectively,while the porosity ranges from 98.06%-98.88%that the sample of P5 is the greatest and the sample of P4 is the slightly lowest.In conclusion,the blended PCL/CMC scaffolds P1-P5 were formed by salt leaching technique suitable to use in tissue engineering application.However,the amount of CMC blended with PCL should be reasonable in order to adjust the hydrophilic of the scaffold.
基金This work was financially supported by the State Key Laboratory of New Textile Materials and Advanced Processing Technologies(No.FZ2021014)the Wuhan Science and Technology Bureau Application Foundation Frontier Project(2022023988065216)+2 种基金the National Natural Science Foundation of China(J2124010,51405348,51575405)the Educational Commission of Hubei Province of China(D20171604)the Hubei Provincial Natural Science Foundation of China(2018CFB673).
文摘The bond film on the surface of the CO_(2) sodium silicate used sands is not easy to decompose,therefore,it is difficult to reclaim used sands.A new reclamation method of CO_(2) sodium silicate used sands was developed by steam leaching,which can reduce the water consumption of reclamation and improve the removal effect of sodium silicate bond film.Firstly,the leaching effect of the sodium silicate sands after 20/200/400/600/800/1,000°C heat preservation treatment was simulated.Furthermore,the influence of the leaching time on the removal effect of the sodium silicate bond film was studied.Finally,the casting properties of the reclaimed sands after the leaching reclamation treatment were tested.The results show for simulated used sands after 30 min of steam leaching,the removal ratio of the alkali exceeds 84.1%,the removal ratio of silicate is 86.2%,and the removal ratio of carbonate is 93.6%.The removal rate of alkali,silicate and carbonate is relatively low in the leaching time of 30-50 min.Considering the reclamation effect and cost,the leaching time is controlled in 30 min.Water consumption is only 60%of the mass of used sands for 30 min steam leaching,while it is 200%for wet reclamation.Morphological analysis shows that most of the hazardous substances in the used sands are removed in 30 min steam leaching,and the reclaimed sands surface after steam leaching in 50 min is as smooth as new sands.After 30 min of steam leaching,the alkali removal effect of the factory used sands can reach 81.5%,the water consumption by the steam leaching reclamation is 58%of the mass of the used sand,which is similar to the result of simulated used sands.The performance of reclaimed sands obtained after 30 min steam leaching is better than that of new sands when the amount of sodium silicate added is 6%of the mass of the reclaimed sands and the CO_(2) blowing time is 15 s:the 24 h ultimate compressive strength of reclaimed sands is 5.6 MPa(equated with new sands),and the collapsibility compressive strength is 5.2 MPa,which is lower than the collapsibility compressive strength of new sands(7.7 MPa).This indicates that the reclamation of CO_(2) sodium silicate used sands by steam leaching is a feasible method.
基金supported by the National Natural Science Foundation of China(Grant No.U2167212)。
文摘Under the new development philosophy of carbon peaking and carbon neutrality,CO_(2)and O_(2)in situ leaching(ISL)has been identified as a promising technique for uranium mining in China,not only because it solves carbon dioxide utilization and sequestration,but it also alleviates the environmental burden.However,significant challenges exist in assessment of CO_(2)footprint and water-rock interactions,due to complex geochemical processes.Herein this study conducts a three-dimensional,multicomponent reactive transport model(RTM)of a field-scale CO_(2)and O_(2)ISL process at a typical sandstone-hosted uranium deposit in Songliao Basin,China.Numerical simulations are performed to provide new insight into quantitative interpretation of the greenhouse gas(CO_(2))footprint and environmental impact(SO_(4)^(2–))of the CO_(2)and O_(2)ISL,considering the potential chemical reaction network for uranium recovery at the field scale.RTM results demonstrate that the fate of the CO_(2)could be summarized as injected CO_(2)dissolution,dissolved CO_(2)mineralization and storage of CO_(2)as a gas phase during the CO_(2)and O_(2)ISL process.Furthermore,compared to acid ISL,CO_(2)and O_(2)ISL has a potentially smaller environmental footprint,with 20%of SO_(4)^(2–)concentration in the aquifer.The findings improve our fundamental understanding of carbon utilization in a long-term CO_(2)and O_(2)ISL system and provide important environmental implications when considering complex geochemical processes.
基金funded by the Deanship of Scientific Research(DSR),King AbdulAziz University,Jeddah,Saudi Arabia under Grant No.(RG-11-611-43).
文摘Soil salinity is a serious land degradation issue in agriculture.It is a major threat to agriculture productivity.Extra irrigation water is applied to leach down the salts from the root zone of the plants in the form of a Leaching fraction(LF)of irrigation water.For the leaching process to be effective,the LF of irriga-tion water needs to be adjusted according to the environmental conditions and soil salinity level in the form of Evapotranspiration(ET)rate.The relationship between environmental conditions and ET rate is hard to be defined by a linear relationship and data-driven Machine learning(ML)based decisions are required to determine the calibrated Evapotranspiration(ETc)rate.ML-assisted ETc is pro-posed to adjust the LF according to the ETc and soil salinity level.A regression model is proposed to determine the ETc rate according to the prevailing tempera-ture,humidity,and sunshine,which would be used to determine the smart LF according to the ETc and soil salinity level.The proposed model is trained and tested against the Blaney Criddle method of Reference evapotranspiration(ETo)determination.The validation of the model from the test dataset reveals the accu-racy of the ML model in terms of Root mean squared errors(RMSE)are 0.41,Mean absolute errors(MAE)are 0.34,and Mean squared errors(MSE)are 0.28 mm day-1.The applications of the proposed solution in a real-time environ-ment show that the LF by the proposed solution is more effective in reducing the soil salinity as compared to the traditional process of leaching.
文摘Rare earth elements are indispensable raw materials for advanced aero-engines, special optical materials, and high-performance electronic products. With the development of the social economy, the global demand for rare earth resources is increasing, and rare earths have become a key metal for the development of new industries and frontier technologies that are highly valued both at home and abroad. Ion-adsorbed rare earth ores are an important source of rare earths, so the efficient green leaching of ion-adsorbed rare earths is important. Researchers found that the selection of an efficient green leaching agent for ion-adsorbed rare earths is based on the zeta potential of tailing clay minerals in addition to leaching efficiency, and both zeta potential and leaching ion concentration are related to mineral acidity and alkalinity, and the pH of tailing water suspension is a direct indicator of environmental water quality requirements. Therefore, the efficiency of the leaching process is closely integrated with the environmental evaluation, and the characteristics and correlation of the changes in zeta potential, pH, conductivity and pollutant concentration of the pulp of clay mineral content during the leaching process of ore leaching and tailings aqueous electrolyte solution leaching are studied by evaluating the leaching system, and a set of correlation leaching efficiency and environmental impact evaluation method is established based on the results of the above analysis, which is of scientific development of ion adsorption rare earth resources. It has important theoretical significance and practical application value.
基金financially supported by the National Key Research and Development Program of China (No. 2016YFC0600704)the National Science Fund for Excellent Young Scholars of China (No. 51722401)the Key Program of National Natural Science Foundation of China (No. 51734001)
文摘Compared with the traditional pyrometallurgical process, copper bioleaching has distinctive advantages of high efficiency and lower cost, enabling efficiently extracts of valuable metal resources from copper sulfides. Moreover, during long-term industrial applications of bioleaching, many regulatory enhancements and technological methods are used to accelerate the interfacial reactions. With advances in microbial genetic and sequencing technologies, bacterial communities and their mechanisms in bioleaching systems have been revealed gradually. The bacterial proliferation and dissolution of sulfide ores by a bacterial community depends on the pH, temperature, oxygen, reaction product regulation, additives, and passivation substances, among other factors. The internal relationship among the influencing factors and the succession of microorganism diversity are discussed and reviewed in this paper. This paper is intended to provide a good reference for studies related to enhanced bioleaching.
基金the National Natural Science Fund Project of China(41373108)the Mining Group Project of Huaibei(K160139078)。
文摘Coal gangue is the main pollution source of mining areas.When coal gangue is stacked and recycled,the heavy metal elements contained in it are released by natural weathering and leaching,which causes damage to the surrounding ecological environment.In this study,the leaching and precipitation characteristics of heavy metals in low-sulfur coal gangue under different environmental conditions were simulated by indoor dynamic leaching experiments,which provided a theoretical basis for environmental restoration of the mining area.The conclusions are as follows:higher heavy metal content in low-sulfur coal gangue is associated with greater,leaching of heavy metals;acidic conditions promote the release of heavy metals in low-sulfur coal gangue;and more precipitation is associated with better release of heavy metals from the low-sulfur coal gangue.
基金the National Naturel Science Foundation of China(Nos.51974016 and 51204012)for financial support.
文摘In this work,sodium dicyanamide(SD)was used as a leaching reagent for gold recovery,and the effects of the SD dosage and solution pH on the gold-leaching performance were investigated.A gold recovery of 34.8%was obtained when SD was used as the sole leaching reagent at a dosage of 15 kg/t.In the presence of a certain amount of potassium ferrocyanide(PF)in the SD solution,the gold recovery was found to increase from 34.8%to 57.08%.Using the quartz crystal microbalance with dissipation(QCM-D)technique,the leaching kinetics of SD with and without PF were studied.The QCM-D results indicate that the gold-leaching rate increased from 4.03 to 39.99 ng·cm^(–2)·min^(–1) when the SD concentration was increased from 0 to 0.17 mol/L,and increased from 39.99 to 272.62 ng·cm^(–2)·min^(–1) when 0.1 mol/L of PF was used in combination with SD.The pregnant solution in the leaching tests was characterized by X-ray photoelectron spectroscopy and electrospray mass spectrometry,which indicated that Au and(N(CN)2)–in the SD solution formed a series of metal complex ions,[AuNax(N(CN)2)x+2]–(x=1,2,3,or 4).
基金Project(51374035)supported by the National Natural Science Foundation of ChinaProject(2012BAB08B02)supported by the National“Twelfth Five”Science and Technology,ChinaProject(NCET-13-0669)supported by New Century Excellent Talents in University of Ministry of Education of China
文摘A laboratory leaching experiment with samples of different grades was carried out, and an analytical method of concentration of leaching solution was put forward. For each sample, respectively, by applying phase space reconstruction for time series of monitoring data, the saturated embedding dimension and the correlation dimension were obtained, and the evolution laws between neighboring points in the reconstructed phase space were revealed. With BP neural network, a prediction model of concentration of leaching solution was set up and the maximum error of which was less than 2%. The results show that there exist chaotic characteristics in leaching system, and samples of different grades have different nonlinear dynamic features; the higher the grade of sample, the smaller the correlation dimension; furthermore, the maximum Lyapunov index, energy dissipation and chaotic extent of the leaching system increase with grade of the sample; by phase space reconstruction, the subtle change features of concentration of leaching solution can be magnified and the inherent laws can be fully demonstrated. According to the laws, a prediction model of leaching cycle period has been established to provide a theoretical foundation for solution mining.
基金financially supported by the National Nature Science Foundation of China(Nos.51804136,52064021,51974140,and 52064018)the Key Projects of Jiangxi Key R&D Plan,China(No.20192ACB70017)+3 种基金the Jiangxi Provincial Cultivation Program for Academic and Technical Leaders of Major Subjects,China(No.20204 BCJL23031)the Jiangxi Province Science Fund for Distinguished Young Scholars,China(No.20202ACB213002)the Program of Qingjiang Excellent Young Talents,Jiangxi University of Science and Technology,China(JXUSTQJBJ 2020004)the Distinguished Professor Program of Jinggang Scholars in institutions of higher learning,Jiangxi Province,China。
文摘An ammonia-based system was used to selectively leach cobalt(Co)from an African high-silicon low-grade Co ore,and the other elemental impurities were inhibited from leaching in this process.This process was simple and environmentally friendly.The results revealed that the leaching ratio of Co can reach up to 95.61%using(NH_(4))_(2)SO_(4)as a leaching agent under the following materials and conditions:(NH_(4))_(2)SO_(4)concentration 300 g/L,reductant dosage 0.7 g,leaching temperature 353 K,reaction time 4 h,and liquid-solid ratio 6 mL/g.The leaching kinetics of Co showed that the apparent activation energy of Co leaching was 76.07 kJ/mol(i.e.,in the range of 40-300 kJ/mol).This indicated that the leaching of Co from the Co ore was controlled by an interfacial chemical reaction,and then the developed leaching kinetics model of the Co can be expressed as 1-(1-α)^(1/3)=28.01×10~3×r_0^(-1)×C_((NH_(4))_(2)SO_(4))^(1.5)×exp(-76073/8.314 T)×t,whereαis the leaching ratio(%)of Co,r_0 is the average radius(m)of the Co ore particles,T is the temperature(K),and C_((NH_(4))_(2)SO_(4))is the initial reactant concentration(kg/m^(3)).
基金Project supported by the National Natural Science Foundation of China (Nos. 50934002 and 50774011)the Postdoctoral Science Foundation of China (No. 20090450014)the DoctoralNatural Science Foundation of China (No. 20070008038)
文摘A mathematical model for heap bioleaching is developed to analyze heat transfer,oxygen flow,target ion distribution and oxidation leaching rate in the heap.The model equations are solved with Comsol Multiphysics software.Numerical simulation results show the following facts:Concentration of oxygen is relatively high along the boundary of the slope,and low in the center part where leaching rate is slow.Temperature is relatively low along the slope and reaches the highest along the bottom region near the slope,with difference being more than 6 C.Concentration of target mental ions is the highest in the bottom region near the slope.Oxidation leaching rate is relatively large in the bottom and slope part with a fast reaction rate,and small in the other part with low oxygen concentration.