Improvement on the Luminescence Property of Y, Sb Co-doped PbWO_4 Single Crystal
1
作者 杨春晖 Shi Pengfei Chen Gang 《High Technology Letters》 EI CAS 2001年第2期87-88,共2页
The effect of Y and Sb co-doping on the luminescence property of PbWO 4 crystals has been investigated. Compared with undoped PbWO4, the transmittance and emission peak intensity of Y∶Sb∶PbWO 4 crystals were obvious... The effect of Y and Sb co-doping on the luminescence property of PbWO 4 crystals has been investigated. Compared with undoped PbWO4, the transmittance and emission peak intensity of Y∶Sb∶PbWO 4 crystals were obviously improved. In addition, its transmittance cutoff wavelength and emission peak shifted to the shorter one. The mechanism of effect of Y and Sb on the transmittance spectra was briefly discussed. The light yield of Y∶Sb∶PbWO 4 crystals was 25p.e./MeV, which was two times of that of undoped PbWO 4. Our experiments showed that Y and Sb co-doping was a selectable method to improve the luminescence property of PbWO 4. 展开更多
关键词 y∶sb∶pbwo4 crystal TRANSMITTANCE Exicted-emission spectra Light yield
下载PDF
大尺寸Y:PbWO_4晶体的坩埚下降法生长与光学均匀性研究 被引量:1
2
作者 宫波 沈定中 +2 位作者 任国浩 张海斌 殷之文 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2002年第2期215-219,共5页
报道了大尺寸Y:PbWO4晶体的坩埚下降法生长工艺,讨论了影响晶体生长的主要 因素.探讨了消除晶体开裂、抑制晶体组分过冷的工艺措施,成功地生长出无宏观缺陷的大尺 寸Y:PbWO4晶体,尺寸达52min×52mm×... 报道了大尺寸Y:PbWO4晶体的坩埚下降法生长工艺,讨论了影响晶体生长的主要 因素.探讨了消除晶体开裂、抑制晶体组分过冷的工艺措施,成功地生长出无宏观缺陷的大尺 寸Y:PbWO4晶体,尺寸达52min×52mm×250mm.同时,对实验样品沿晶体生长方向不同部 位的横向透过率及发射光谱进行了测试,结果表明,坩埚下降法生长的大尺寸Y:PbWO4晶体 具有较好的光学均匀性. 展开更多
关键词 大尺寸 y:pbwo4晶体 生长 钨酸铅 坩埚下降法 光学均匀性
下载PDF
K_3Sb_(0.3)Y_4O_8·6H_2O新型低温相的水热合成与表征 被引量:1
3
作者 郑文君 徐翊华 庞文琴 《高等学校化学学报》 SCIE EI CAS CSCD 北大核心 1997年第12期1932-1934,共3页
A novel low temperature phase K3Sb0.3Y4O8. 6H2O was synthesized hydrother-mally from K2O-Sb2O3-Y2O3-H2O system, and characterized by means of XRD, SEM, IR,TG, DTA and ICP methods- The unit cell for the product is hexa... A novel low temperature phase K3Sb0.3Y4O8. 6H2O was synthesized hydrother-mally from K2O-Sb2O3-Y2O3-H2O system, and characterized by means of XRD, SEM, IR,TG, DTA and ICP methods- The unit cell for the product is hexagonal with the cell parame-ters a = 1.657 6nm and c= 1.186 5 nm. The volume of the cell is calculated to be 2. 823 3nm3. The product was decomposed into oxides from 310℃ to 390 ℃. 展开更多
关键词 羟基氧化物 低温相 K3sb0.3y4O8
下载PDF
大尺寸PbWO4:Y晶体光谱性能的均匀性研究
4
作者 耿政松 陆少君 +1 位作者 谢建军 廖晶莹 《同济大学学报(自然科学版)》 EI CAS CSCD 北大核心 2008年第1期135-138,共4页
报道了用改进的布里奇曼(Bridgmam)法生长的大尺寸PbWO4:Y晶体光谱性能均匀性的研究.通过对依次切自大尺寸PbWO4:Y毛坯晶体的籽晶端、中间部位和顶端三块晶体(24m×24m×24mm)的透射光谱、X-ray激发发射光谱、发光衰减... 报道了用改进的布里奇曼(Bridgmam)法生长的大尺寸PbWO4:Y晶体光谱性能均匀性的研究.通过对依次切自大尺寸PbWO4:Y毛坯晶体的籽晶端、中间部位和顶端三块晶体(24m×24m×24mm)的透射光谱、X-ray激发发射光谱、发光衰减寿命、光产额和辐照损伤等方面的光谱性能测试,表明了Y掺杂能显著改善PbWO4晶体的光谱性能,使晶体在短波330-420nm范围的透过率明显提高,抗辐照能力增强. 展开更多
关键词 pbwo4 y晶体 改进的Bridgman法 光谱性能
下载PDF
混合溶剂下Y^(3+)-PbWO_4微晶的制备及光致发光性质
5
作者 熊鹰 房刚 周元林 《科技创新导报》 2015年第24期3-4,共2页
以不同比例的乙二醇(EG)和水(H2O)为混合溶剂,通过直接沉淀法在室温条件下成功制备了不同形貌的钇掺杂钨酸铅(Y3+-Pb WO4)微晶,利用X射线衍射(XRD)、扫描电子显微镜(SEM)、光致发光光谱仪(PL)等对微晶的微观结构以及光学性能进行了表征... 以不同比例的乙二醇(EG)和水(H2O)为混合溶剂,通过直接沉淀法在室温条件下成功制备了不同形貌的钇掺杂钨酸铅(Y3+-Pb WO4)微晶,利用X射线衍射(XRD)、扫描电子显微镜(SEM)、光致发光光谱仪(PL)等对微晶的微观结构以及光学性能进行了表征。研究结果表明:混合溶剂中的EG的比例对Y3+-Pb WO4微晶的形貌演变起到了关键的作用;不同形貌的Y3+-Pb WO4微晶表现出不同的光致发光性能,通过高斯拟合发现其发光峰由蓝光峰、绿光峰和黄光峰构成,峰位均随着混合溶剂中EG含量的增加而先红移再蓝移,绿光峰和黄光峰的强度随着混合溶剂中EG含量的增加而分别下降和增加,表明Y3+-Pb WO4微晶的光致发光与其晶粒尺寸、形貌存在密切的联系。 展开更多
关键词 y3+掺杂 pbwo4微晶 直接沉淀法 混合溶剂 光致发光
下载PDF
Y^(3+)掺杂PbWO_4微晶的合成及发光性质研究
6
作者 房刚 熊鹰 周元林 《材料导报》 EI CAS CSCD 北大核心 2011年第22期20-24,共5页
在乙二醇-蒸馏水混合溶剂中,以水热法制备出不同钇(Y3+)掺杂浓度的钨酸铅(PbWO4)微晶,并利用X射线衍射(XRD)、X射线荧光光谱(XRF)和光致发光光谱(PL)分别对样品的结构和发光性能进行了表征。结果显示,Y3+掺杂使PbWO4微晶的发光强度最大... 在乙二醇-蒸馏水混合溶剂中,以水热法制备出不同钇(Y3+)掺杂浓度的钨酸铅(PbWO4)微晶,并利用X射线衍射(XRD)、X射线荧光光谱(XRF)和光致发光光谱(PL)分别对样品的结构和发光性能进行了表征。结果显示,Y3+掺杂使PbWO4微晶的发光强度最大提高了近4倍,且随着Y3+掺杂浓度的增加发光峰位红移近40nm;另外,通过对发光曲线的高斯拟合发现,所有的发光峰都是由蓝光峰、绿光峰、黄光峰和红光峰组成,并分别探讨它们的可能起源及Y3+掺杂对它们所产生的影响。 展开更多
关键词 pbwo4微晶 y3+掺杂 水热法 光致发光
下载PDF
大尺寸PWO:(Sb,Y)晶体光谱特性的表征研究 被引量:1
7
作者 谢建军 袁晖 +5 位作者 杨培志 沈炳孚 曹顿华 廖晶莹 顾牡 殷之文 《无机材料学报》 SCIE EI CAS CSCD 北大核心 2005年第5期1089-1094,共6页
报道了用改进的Bridgmam法生长的大尺寸PbWO4:(Sb,Y)晶体的光谱特性的表征研究.通过对依次切自大尺寸PbWO4:(Sb,Y)毛坯晶体的籽晶端、中间部位和顶端三块晶体(-23mm×23mm×20mm)的透射光谱、X射线激发发射光谱、紫外激发与发... 报道了用改进的Bridgmam法生长的大尺寸PbWO4:(Sb,Y)晶体的光谱特性的表征研究.通过对依次切自大尺寸PbWO4:(Sb,Y)毛坯晶体的籽晶端、中间部位和顶端三块晶体(-23mm×23mm×20mm)的透射光谱、X射线激发发射光谱、紫外激发与发射光谱、发光衰减寿命、光产额和辐照损伤等方面的光谱性能测试,结果表明,Sb、Y双掺杂能显著改善PbWO4晶体的光谱性能,使晶体在短波330-420nm范围的透过率明显提高,光产额增加,抗辐照能力增强.但从籽晶端到顶端的性能存在一定的差异,说明大尺寸的PbWO4:(Sb,Y)晶体的均匀性还有待提高. 展开更多
关键词 改进的Bridgman法 PbW04:(sb y) 光谱性能
下载PDF
大尺寸PWO:(Mo,Y)晶体发光均匀性的研究 被引量:2
8
作者 谢建军 袁晖 +3 位作者 廖晶莹 杨培志 沈炳孚 殷之文 《人工晶体学报》 EI CAS CSCD 北大核心 2005年第3期417-420,共4页
报道了用改进的Bridgman法生长的大尺寸PbWO4:(Mo,Y)晶体发光均匀性的表征研究。通过对大尺寸的PbWO4:(Mo,Y)晶体不同部位的透射光谱、X射线激发发射光谱、光产额和抗辐照损伤能力等光学和闪烁性能的测试,结果表明在实验所涉及的掺杂浓... 报道了用改进的Bridgman法生长的大尺寸PbWO4:(Mo,Y)晶体发光均匀性的表征研究。通过对大尺寸的PbWO4:(Mo,Y)晶体不同部位的透射光谱、X射线激发发射光谱、光产额和抗辐照损伤能力等光学和闪烁性能的测试,结果表明在实验所涉及的掺杂浓度范围,Mo、Y双掺杂能显著改善PbWO4晶体的发光均匀性,增强其抗辐照损伤能力。 展开更多
关键词 pbwo4:(Mo y)晶体 下降法 发光均匀性
下载PDF
三元金属间化合物La_3Cu_3Bi_4的合成、结构与性能研究(英文)
9
作者 鲁玉明 范峰 +2 位作者 蔡传兵 曹世勋 张金仓 《Journal of Shanghai University(English Edition)》 CAS 2008年第6期486-488,共3页
The new intermetallic compound La3Cu3Bi4 was synthesized by arc melting method followed by annealing.The crystal structure refined using the Rietveld method and X-ray powder diffraction data showed to be Y3Au3Sb4 stru... The new intermetallic compound La3Cu3Bi4 was synthesized by arc melting method followed by annealing.The crystal structure refined using the Rietveld method and X-ray powder diffraction data showed to be Y3Au3Sb4 structure type with space group I43D(No.220).The unit cell parameters were a = 0.997 797(7) nm and V = 0.993 41(2) nm3.The structure was characterized by covalent Cu-Bi4 tetrahedron, which formed three-dimensional network by sharing corners and La atoms separated in the space of Cu-Bi4 tetragon.The expansion of La3Cu3Bi4 studied by using low temperature X-ray di?raction showed to be positive expansion and diminished with the temperature rising. 展开更多
关键词 建筑物 La3Ca3Bi4 y3Au3sb4 建筑材料 建筑构成 金属材料
下载PDF
掺Y对PbWO_4闪烁体的热释光影响 被引量:6
10
作者 刘波 施朝淑 +4 位作者 魏亚光 吴灿 李裕熊 胡关钦 沈定中 《物理学报》 SCIE EI CAS CSCD 北大核心 2000年第10期2078-2082,共5页
研究了纯PbWO4 和PbWO4 :Y晶体经γ射线辐照和可见光光照前后室温以上的热释光 .发现大剂量辐照后掺Y可以有效地抑制热释光的强度并使热释光峰移向高温 ,说明掺Y有利于提高光输出的稳定性 .可见光光照也会影响热释光并可以产生新的热释... 研究了纯PbWO4 和PbWO4 :Y晶体经γ射线辐照和可见光光照前后室温以上的热释光 .发现大剂量辐照后掺Y可以有效地抑制热释光的强度并使热释光峰移向高温 ,说明掺Y有利于提高光输出的稳定性 .可见光光照也会影响热释光并可以产生新的热释光峰 ,这可能是由于光释电子 (或空穴 )被浅陷阱重新俘获或是光照后产生了新型色心的结果 . 展开更多
关键词 热释光 钨酸铅 掺杂 闪烁体
原文传递
Sb_2O_3掺杂对提高PbWO_4晶体光学及闪烁性能的作用 被引量:6
11
作者 王绍华 沈定中 +3 位作者 任国浩 倪海洪 蔡晓琳 殷之文 《光学学报》 EI CAS CSCD 北大核心 2000年第8期1122-1127,共6页
采用改进的布里奇曼 (Bridgman)法生长了掺杂Sb2 O3的PbWO4 晶体。基于透射光谱、紫外激发及其发射谱、X射线激发的发射谱、光输出和辐照损伤等方面的测试 ,讨论了Sb2 O3掺杂对提高PbWO4 晶体光学及闪烁性能的作用。
关键词 掺杂 钨酸铅晶体 闪烁性能 sb2O3
原文传递
掺Gd^(3+),Y^(3+)对PbWO_4低温热释光的影响 被引量:3
12
作者 刘波 施朝淑 +3 位作者 周东方 戚泽明 胡关钦 汤洪高 《物理学报》 SCIE EI CAS CSCD 北大核心 2001年第8期1627-1631,共5页
通过热释光方法研究了PbWO4(PWO) ,PWO :Y3+ ,PWO :Gd3+ 多晶粉末及PWO ,PWO :Y单晶的低温 (<30 0K)热释光现象 .多晶粉末中 ,掺杂Y3+ 或Gd3 + 都会大大降低甚至消除 2 0 0K附近的热释光峰 ,同时产生新的热释光峰 ,分别位于 12 5和 1... 通过热释光方法研究了PbWO4(PWO) ,PWO :Y3+ ,PWO :Gd3+ 多晶粉末及PWO ,PWO :Y单晶的低温 (<30 0K)热释光现象 .多晶粉末中 ,掺杂Y3+ 或Gd3 + 都会大大降低甚至消除 2 0 0K附近的热释光峰 ,同时产生新的热释光峰 ,分别位于 12 5和 15 0K(掺Y掺Gd) .这表明掺三价离子除了起到电荷补偿作用以减少Pb3+ ,O- 浓度外 ,还可以产生新的陷阱能级 .对于PWO :Y单晶 ,掺杂Y3 + 可以消除 2 5 3K的热释光峰 ,即消除较深 (~ 0 .89eV)的陷阱 ,但PWO单晶中较浅的陷阱 (~ 0 .42eV)对应 130K热释光峰仍然存在 ,对此进行讨论 ,它最可能源于氧空位缺陷 .根据Pb3+ ,Gd3+ ,Y3 + 的电子库仑势不同 ,在PWO晶体中替代Pb2 + 后形成的电子陷阱深度有别 (EPb>EGd >EY) 。 展开更多
关键词 掺杂 热释光 陷阱 钨酸铅 低温
原文传递
提高PbWO_4晶体光学性能的研究 被引量:6
13
作者 孙尚文 韩爱珍 +1 位作者 李铭华 徐玉恒 《光学学报》 EI CAS CSCD 北大核心 1997年第6期817-819,共3页
钨酸铅(PbWO4)晶体在生长过程中由于缺氧产生了氧空位缺陷和Fe2+杂质缺陷,使晶体着色,光学性能下降。在晶体生长过程中掺进Sb2O3,能消除氧空位,将Fe2+氧化为无色的Fe3+。
关键词 晶体 吸收光谱 光产额 钨酸铅晶体
原文传递
掺钇钨酸铅晶体发光性能和微观缺陷的研究 被引量:1
14
作者 梁玲 顾牡 +2 位作者 段勇 马晓辉 刘峰松 《发光学报》 EI CAS CSCD 北大核心 2003年第1期76-80,共5页
通过透射谱、X射线激发发射谱 (XSL)的测试 ,研究了Bridgman法生长的掺钇钨酸铅晶体的发光性能 ,并利用正电子湮没寿命谱 (PAT)和X光电子能谱 (XPS)实验手段 ,对掺钇钨酸铅晶体的微观缺陷进行研究。实验表明 ,钇掺杂能够提高钨酸铅晶体... 通过透射谱、X射线激发发射谱 (XSL)的测试 ,研究了Bridgman法生长的掺钇钨酸铅晶体的发光性能 ,并利用正电子湮没寿命谱 (PAT)和X光电子能谱 (XPS)实验手段 ,对掺钇钨酸铅晶体的微观缺陷进行研究。实验表明 ,钇掺杂能够提高钨酸铅晶体的发光快成分比例 ,并使得晶体中的正电子俘获中心浓度下降 ,低价氧浓度下降。提出掺钇钨酸铅晶体中钇的掺杂主要以Y3 + 占据VPb的形式存在。Y3 + 占据VPb可能是钨酸铅晶体吸收边得到改善的原因 ,而由于晶体内低价氧浓度的减少 ,作为绿光发光中心的 (WO3 +O-)基团的减少可能会使发光快成分比例有所增加。 展开更多
关键词 发光性能 掺钇 钨酸铅晶体 微观缺陷 正电子湮没寿命谱 X光电子能谱
下载PDF
掺钇钨酸铅晶体的研制
15
作者 倪海洪 蔡晓琳 沈定中 《人工晶体学报》 EI CAS CSCD 北大核心 2000年第S1期73-,共1页
PbWO4晶体已被西欧核子中心确定用于建造大型强子对撞机 (LHC)中的精密电磁量能器 ,并与我所签定生产意向。根据他们对晶体提出的光输出大于 8个光电子 /MeV ,辐照损伤小于 1 0 %等要求 ,我们对掺钇钨酸铅晶体进行了研究。采用高纯原料 ... PbWO4晶体已被西欧核子中心确定用于建造大型强子对撞机 (LHC)中的精密电磁量能器 ,并与我所签定生产意向。根据他们对晶体提出的光输出大于 8个光电子 /MeV ,辐照损伤小于 1 0 %等要求 ,我们对掺钇钨酸铅晶体进行了研究。采用高纯原料 ( 99.99%以上 )PbO∶WO3 =1∶1 (摩尔比 ) ,在原料中掺入质量分数为 1 .5×1 0 -4 的Y2 O3 。将此原料充分混合在一定温度下熔制成多晶 ,用硅碳棒加热 ,采用铂坩埚下降法生长大尺寸PbWO4晶体 ,生长方向为c轴生长 ,生长速度为 1 .0~ 1 .2mm/h。我们发现晶种质量及方向、温度梯度及温场分布对晶体性能有很大影响。我们在实验中选取完好无开裂且与c轴方向一致的晶种 ,并采用计算机多路分别控制 ,消除温场的波动 ,保证生长环境的稳定 ,保持固液界面的稳定。通过实验我们能够生长出 2 8mm× 2 8mm× 2 80mm的晶体 ,晶体内部无开裂、气泡、散射颗粒但晶体顶部略带黄色。过去通常认为PbWO4晶体带黄色是由于晶体内缺氧引起 ,可通过氧退火解决。而我们认为PbWO4晶体在熔晶及生长过程中PbO易挥发故采用偏铅生长 ,在这之后我们得到无色透明的优质PbWO4晶体 ,经测试其性能完全符合西欧核子中心使用要求 ,其中光输出大于 1 2个光电子 /MeV ,辐照损伤小于 5 % ,再由一定的温度退火 ,? 展开更多
关键词 pbwo_4(y_2O_3)晶体 闪烁晶体 布里奇曼法