The subsurface damage(SSD)layers of monocrystalline germanium wafers lapped by three different ways were measured and compared by the method of nanoindentation and micro morphology.Three ways such as ice-fixed abrasiv...The subsurface damage(SSD)layers of monocrystalline germanium wafers lapped by three different ways were measured and compared by the method of nanoindentation and micro morphology.Three ways such as ice-fixed abrasive,thermosetting fixed abrasive and free abrasive lappings are adopted to lap monocrystalline germanium wafers.The SSD depth was measured by a nanoindenter,and the morphology of SSD layer was observed by an atomic force microscopy(AFM).The results show that the SSD layer of monocrystalline germanium wafer is mainly composed of soft corrosion layer and plastic scratch and crack growth layer.Compared with thermosetting fixed abrasive and free abrasive lappings,the SSD depth lapped with ice-fixed abrasive is shallower.Moreover,the SSD morphology of monocrystalline germanium wafer lapped with ice-fixed abrasive is superior to those of two other processing ways.展开更多
基金supported by the National Natural Science Foundation of China(No.51375237)the Postdoctoral Science Foundation of China(No.2015T80547)
文摘The subsurface damage(SSD)layers of monocrystalline germanium wafers lapped by three different ways were measured and compared by the method of nanoindentation and micro morphology.Three ways such as ice-fixed abrasive,thermosetting fixed abrasive and free abrasive lappings are adopted to lap monocrystalline germanium wafers.The SSD depth was measured by a nanoindenter,and the morphology of SSD layer was observed by an atomic force microscopy(AFM).The results show that the SSD layer of monocrystalline germanium wafer is mainly composed of soft corrosion layer and plastic scratch and crack growth layer.Compared with thermosetting fixed abrasive and free abrasive lappings,the SSD depth lapped with ice-fixed abrasive is shallower.Moreover,the SSD morphology of monocrystalline germanium wafer lapped with ice-fixed abrasive is superior to those of two other processing ways.