期刊文献+
共找到607篇文章
< 1 2 31 >
每页显示 20 50 100
Prediction of Burst Pressure of a Radial Truck Tire Using Finite Element Analysis 被引量:4
1
作者 Kyoung Moon Jeong 《World Journal of Engineering and Technology》 2016年第2期228-237,共10页
This paper is concerned with the numerical prediction of the burst pressure of a radial truck tire. Even though relatively rare, the tire fracture or failure brings up a big accident. Especially, the tire burst or rup... This paper is concerned with the numerical prediction of the burst pressure of a radial truck tire. Even though relatively rare, the tire fracture or failure brings up a big accident. Especially, the tire burst or rupture is a rapid loss of inflation pressure of a truck and bus tire leading to an explosion. The tire burst pressure, under this extreme loading condition, can be predicted by identifying the pressure at which the cord breaking force of the composite materials is attained. Recently, the use of finite element analysis in tire optimal design has become widely popular. In order to determine the burst pressure of a radial truck tire, an axisymmetric finite element model has been developed using a commercial finite element code with rebar element. The numerical result shows that the bead wire among the various layers modeled the rebar element breaks off first in the radial truck tire. The finite element modeling with the rebar element on the bead wire of a radial truck tire is able to well predict the tire burst pressure identifying the pressure at which the breaking force of steel bead wires is reached. The model predictions of tire burst pressure should be correlated with test data, in which case the tire is hydro-tested to destruction. The effect of the design change with the different bead structure on the tire burst pressure is discussed. 展开更多
关键词 Burst Pressure radial truck Tire Finite Element Analysis Breaking Force
下载PDF
Computation of rolling resistance caused by rubber hysteresis of truck radial tire 被引量:1
2
作者 MA Gai-ling XU Hong CUI Wen-yong 《Journal of Zhejiang University-Science A(Applied Physics & Engineering)》 SCIE EI CAS CSCD 2007年第5期778-785,共8页
Applying the results of stress and strain calculated by 3D finite element model of truck radial tire 11.00R20, a MATLAB program used to compute rolling resistance of the tire caused by hysteresis rolling resistance (H... Applying the results of stress and strain calculated by 3D finite element model of truck radial tire 11.00R20, a MATLAB program used to compute rolling resistance of the tire caused by hysteresis rolling resistance (HRR) is worked out. The HRR distribution on different part of tire section, and the effects of speed, load, internal pressure and the width of the rim on HRR are analyzed. The analysis results showed that energy loss produced by tread rubber contributes the most part to HRR of the whole tire, and that to decrease the HRR, the hysteresis factor of the tread rubber should be reduced, and the distribution of the stress and strain on the section be optimized. 展开更多
关键词 truck radial tire Hysteresis rolling resistance (HRR) Finite element analysis (FEA) Hysteresis factor Tire structuredesign
下载PDF
生物基白炭黑和生物基油在全钢载重子午线轮胎胎面胶中的应用
3
作者 樊斌斌 刘豫皖 +2 位作者 吕国正 岳艳妮 葛永亮 《橡胶科技》 CAS 2024年第1期20-23,共4页
研究生物基白炭黑和生物基油在全钢载重子午线轮胎胎面胶中的应用。结果表明:使用生物基油等量代替环烷油,胶料的硫化速度略加快,300%定伸应力降低,耐切割、耐低温和耐迁移性能提高,生热略增大,耐磨性能基本相当;在同样采用生物基油的... 研究生物基白炭黑和生物基油在全钢载重子午线轮胎胎面胶中的应用。结果表明:使用生物基油等量代替环烷油,胶料的硫化速度略加快,300%定伸应力降低,耐切割、耐低温和耐迁移性能提高,生热略增大,耐磨性能基本相当;在同样采用生物基油的情况下,使用生物基白炭黑等量代替沉淀法白炭黑,胶料的硫化特性、生热、耐磨和耐切割性能相当,但耐疲劳性能明显降低。 展开更多
关键词 生物基白炭黑 生物基油 全钢载重子午线轮胎 胎面胶
下载PDF
高驱动性能315/80R22.5无内胎全钢载重子午线轮胎的设计
4
作者 周鹏飞 李圆圆 +2 位作者 杜嘉需 刘军鹏 郭玮 《轮胎工业》 CAS 2024年第8期466-469,共4页
介绍高驱动性能315/80R22.5无内胎全钢载重子午线轮胎的设计。结构设计:外直径1093 mm,断面宽314 mm,行驶面宽度275 mm,行驶面弧度高7.5857 mm,胎圈着合直径570.5 mm,胎圈着合宽度240.8 mm,断面水平轴位置(H_(1)/H_(2))0.91,胎面采用泥... 介绍高驱动性能315/80R22.5无内胎全钢载重子午线轮胎的设计。结构设计:外直径1093 mm,断面宽314 mm,行驶面宽度275 mm,行驶面弧度高7.5857 mm,胎圈着合直径570.5 mm,胎圈着合宽度240.8 mm,断面水平轴位置(H_(1)/H_(2))0.91,胎面采用泥地+雪地花纹,花纹深度24 mm,花纹饱和度66.41%,花纹周节数54。施工设计:采用双复合胎面,1^(#)和2^(#)带束层采用0.37+6×0.32ST钢丝帘线,0°带束层由3根3×0.7×0.20HE钢丝帘线压延成的冠带条围绕2#带束层缠绕而成,3#带束层采用5×5.30HI钢丝帘线,胎体采用0.22+6+11×0.205ST钢丝帘线,采用一次法成型机成型、双模蒸锅式硫化机硫化。成品轮胎性能试验结果表明,轮胎的充气外缘尺寸、强度性能、耐久性能和胎圈耐久性能均满足相应设计和标准要求。 展开更多
关键词 无内胎轮胎 全钢载重子午线轮胎 驱动性能 结构设计 施工设计
下载PDF
重卡传动轴用高强7075铝合金热流变行为及径向锻造微观组织演变
5
作者 张超 赵升吨 +3 位作者 邢轲 郑文浩 李坤 王永飞 《西安交通大学学报》 EI CAS CSCD 北大核心 2024年第8期124-135,共12页
为研究重型卡车轻量化传动轴用高强7075铝合金在径向锻造时的热变形行为,将大直径7075铝合金挤压棒料预热退火后,取样进行了不同变形条件下的等温压缩试验。分别考虑温度与应变速率对应变强化及软化的影响,构建了适用于中大型7075铝合... 为研究重型卡车轻量化传动轴用高强7075铝合金在径向锻造时的热变形行为,将大直径7075铝合金挤压棒料预热退火后,取样进行了不同变形条件下的等温压缩试验。分别考虑温度与应变速率对应变强化及软化的影响,构建了适用于中大型7075铝合金传动轴热加工的改进Hansel-Spittel本构模型。根据动态材料模型理论获得了7075铝合金的热加工图,并据此分析了7075铝合金棒料在典型径向锻造工艺中的组织变化。研究结果表明:改进Hansel-Spittel模型能更准确地模拟预热退火态7075铝合金的峰值和稳态流变应力,预测值与试验值的平均相对误差仅为2.71%;7075铝合金在温度为350~450℃、应变速率为0.01~10 s^(-1)范围内具有较高的热加工稳定性,高温及低应变速率的变形条件有利于材料的微观组织演化;预热退火态7075铝合金棒料在经过截面收缩率为55.6%的径向锻造工艺和T6热处理后,原始板条晶粒转变为细化大转角晶粒组织,抗拉强度提高至651 MPa,延伸率提高至12.5%,综合性能得到显著改善。 展开更多
关键词 重型卡车轻量化 7075铝合金 本构模型 热加工图 径向锻造 微观组织演化
下载PDF
全钢载重子午线轮胎胎圈露线的原因分析及解决措施
6
作者 佐家军 陆林 +2 位作者 郑伟 高禄 王皓明 《橡胶科技》 CAS 2024年第6期343-345,共3页
从产品设计和工艺控制方面分析全钢载重子午线轮胎胎圈露线的原因,并提出相应的解决措施。通过适当增大成型平面宽和鼓肩宽,适当减小钢丝圈内侧胎侧厚度和胎趾角度,严格控制胎侧成型定位、胎坯存放、硫化机机械手精度、钢丝圈缠绕工艺... 从产品设计和工艺控制方面分析全钢载重子午线轮胎胎圈露线的原因,并提出相应的解决措施。通过适当增大成型平面宽和鼓肩宽,适当减小钢丝圈内侧胎侧厚度和胎趾角度,严格控制胎侧成型定位、胎坯存放、硫化机机械手精度、钢丝圈缠绕工艺及存放等措施,有效地解决了全钢载重子午线轮胎胎圈露线问题,提高了轮胎的安全性能,降低了生产成本。 展开更多
关键词 全钢载重子午线轮胎 胎圈露线 产品设计 工艺控制
下载PDF
Basic Properties of Pyrolysis Carbon Black of Waste Tyres and Application of Pyrolysis Carbon Black in Transition Layer Rubber of All Steel Radial Tire 被引量:4
7
作者 Qi LIU Hui LI Jian LI 《Research and Application of Materials Science》 2020年第1期39-42,共4页
The main chemical composition of pyrolysis carbon black of waste tires is C,O,Cu,Zn and so on.The content of ash and fine powder in pyrolysis carbon black is high,and the 300%elongation stress is high.The difference b... The main chemical composition of pyrolysis carbon black of waste tires is C,O,Cu,Zn and so on.The content of ash and fine powder in pyrolysis carbon black is high,and the 300%elongation stress is high.The difference between pyrolysis carbon black and furnace black N326,which is commonly used in rubber,is obvious compared with chemical property.The pyrolysis carbon black was used to replace furnace black N326 in the transition layer of all steel load Radial tire rubber through experimental study.It was found that the compression heat generation and dynamic loss(Tanδ)of the blend rubber before and after aging were obviously reduced,the elongation at break and resilience increased,while the tensile stress and tear strength decreased by 100%and 300%,but the hardness and tensile strength changed little before and after aging.According to the latest raw material price calculation,15 used tire pyrolysis carbon black instead of furnace carbon black N326 used in all steel Radial tire transition layer rubber application,excluding labor costs,electricity and equipment depreciation,a ton of blended rubber saves about$22.86 in production costs. 展开更多
关键词 waste tyre pyrolysis carbon black all steel radial truck tire the transition layer formula mixing rubber
下载PDF
双酰肼类材料CSC920在全钢载重子午线轮胎基部胶中的应用
8
作者 吕国正 刘豫皖 刘磊 《轮胎工业》 CAS 2024年第7期408-412,共5页
研究双酰肼类材料CSC920(简称CSC920)对全钢载重子午线轮胎基部胶性能的影响。结果表明:CSC920对天然橡胶有较好的改性效果,能显著加快胶料的硫化反应速度,增大胶料的门尼粘度;加入CSC920后,基部胶的定伸应力、拉伸强度和弹性均有所提升... 研究双酰肼类材料CSC920(简称CSC920)对全钢载重子午线轮胎基部胶性能的影响。结果表明:CSC920对天然橡胶有较好的改性效果,能显著加快胶料的硫化反应速度,增大胶料的门尼粘度;加入CSC920后,基部胶的定伸应力、拉伸强度和弹性均有所提升,滚动阻力和生热明显降低;混炼过程中,CSC920在氧化锌之前加入,基部胶的物理性能较好,压缩生热明显降低,CSC920在氧化锌之后加入,可以起到抗硫化返原作用,基部胶的物理性能有所改善,但降低生热效果不明显。 展开更多
关键词 酰肼材料 全钢载重子午线轮胎 基部胶 物理性能 生热
下载PDF
硫化定型时间对全钢载重子午线轮胎均匀性及动平衡性能的影响 被引量:1
9
作者 丛明辉 聂本梁 +4 位作者 宫璐 崔晓 李超 周鹏程 董凌波 《轮胎工业》 CAS 2024年第2期109-111,共3页
研究硫化定型时间对全钢载重子午线轮胎均匀性及动平衡性能的影响。结果表明:随着硫化定型时间的延长,轮胎的径向力波动和侧向力波动增大,呈强正相关性;锥度效应力减小,存在一定负相关性;动不平衡量增大,呈显著正相关性;径向跳动增大,... 研究硫化定型时间对全钢载重子午线轮胎均匀性及动平衡性能的影响。结果表明:随着硫化定型时间的延长,轮胎的径向力波动和侧向力波动增大,呈强正相关性;锥度效应力减小,存在一定负相关性;动不平衡量增大,呈显著正相关性;径向跳动增大,呈强正相关性;侧向跳动与硫化定型时间的相关性不明显。合理设定硫化定型时间,有利于提升轮胎的均匀性和动平衡性能。 展开更多
关键词 全钢载重子午线轮胎 硫化定型时间 均匀性 动平衡性能
下载PDF
全钢载重子午线轮胎氮气硫化工艺的有限元仿真优化
10
作者 张淦超 王小娟 +1 位作者 陈银香 续富琴 《橡胶科技》 CAS 2024年第7期397-401,共5页
对全钢载重子午线轮胎氮气硫化工艺进行有限元仿真优化。结果表明:通高温蒸汽时间对轮胎整体硫化程度变化影响力不足,保证高温蒸汽足够支撑后期硫化后,不需要再延长通高温蒸汽时间;可以加强硫化设备的保温效果,减小氮气保压阶段温度降... 对全钢载重子午线轮胎氮气硫化工艺进行有限元仿真优化。结果表明:通高温蒸汽时间对轮胎整体硫化程度变化影响力不足,保证高温蒸汽足够支撑后期硫化后,不需要再延长通高温蒸汽时间;可以加强硫化设备的保温效果,减小氮气保压阶段温度降幅以降低能源耗散,增大氮气硫化工艺优化的空间,更有利于实现节能降耗和提质增效。 展开更多
关键词 全钢载重子午线轮胎 氮气硫化工艺 有限元仿真
下载PDF
裂解炭黑G685在全钢载重子午线轮胎过渡层胶中的应用研究
11
作者 宋文涛 岳艳妮 +2 位作者 周静 辛远航 李超凡 《橡胶科技》 CAS 2024年第5期267-271,共5页
研究裂解炭黑G685在全钢载重子午线轮胎过渡层胶中的应用。结果表明:与炭黑N660相比,裂解炭黑G685粒径小,结构度高,硫含量高,但其所含硫主要为结合硫;将裂解炭黑G685替代炭黑N660用于轮胎过渡层胶,胶料的t90延长,交联密度、定伸应力、... 研究裂解炭黑G685在全钢载重子午线轮胎过渡层胶中的应用。结果表明:与炭黑N660相比,裂解炭黑G685粒径小,结构度高,硫含量高,但其所含硫主要为结合硫;将裂解炭黑G685替代炭黑N660用于轮胎过渡层胶,胶料的t90延长,交联密度、定伸应力、拉伸强度和生热降低,拉断伸长率增大;在过渡层胶中用裂解炭黑G685替代50%的炭黑N660,成品轮胎的耐久性能和高速性能提高。 展开更多
关键词 裂解炭黑 全钢载重子午线轮胎 过渡层胶
下载PDF
11R22.5全钢载重子午线轮胎胎圈轮廓设计
12
作者 战琪轩 于慧 +3 位作者 胡鸿 许美华 高建刚 杨万龙 《橡胶工业》 CAS 2024年第10期766-771,共6页
分析全钢载重子午线轮胎胎圈损坏问题,以轻量化11R22.5全钢载重子午线轮胎胎圈为例,设计轮胎胎圈仿生轮廓。该轮廓可以使胎圈与轮辋装配更加贴合,为轮胎负载提供支撑,还可以将胎体反包端点锚定,使胎圈损坏几率减小,有效提高轮胎耐久性... 分析全钢载重子午线轮胎胎圈损坏问题,以轻量化11R22.5全钢载重子午线轮胎胎圈为例,设计轮胎胎圈仿生轮廓。该轮廓可以使胎圈与轮辋装配更加贴合,为轮胎负载提供支撑,还可以将胎体反包端点锚定,使胎圈损坏几率减小,有效提高轮胎耐久性能和高速性能,延长轮胎使用寿命。 展开更多
关键词 全钢载重子午线轮胎 胎圈 仿生轮廓
下载PDF
全钢载重子午线轮胎稳态滚动下的接地印痕仿真分析
13
作者 尚永会 于慧 +4 位作者 胡鸿 战琪轩 许美华 高建刚 杨万龙 《橡胶工业》 CAS 2024年第11期869-873,共5页
以12R22.5全钢载重子午线轮胎为例,采用有限元分析软件建立轮胎的三维有限元模型,仿真分析静态加载、制动和驱动状态下轮胎的接地印痕。结果表明:自由滚动状态下轮胎的接地印痕面积小于静态加载状态下轮胎的接地印痕面积,且自由滚动状... 以12R22.5全钢载重子午线轮胎为例,采用有限元分析软件建立轮胎的三维有限元模型,仿真分析静态加载、制动和驱动状态下轮胎的接地印痕。结果表明:自由滚动状态下轮胎的接地印痕面积小于静态加载状态下轮胎的接地印痕面积,且自由滚动状态下轮胎的接地印痕压力区域更为集中,接地印痕压力的最大值大于静态加载状态下轮胎的接地印痕压力的最大值;自由滚动状态下,随着行驶速度的增大,轮胎的接地印痕面积逐渐减小,接地印痕压力逐渐增大;制动状态下,轮胎的接地印痕前端的接地面积小于后端的接地面积,而接地印痕前端的压力大于后端的压力;驱动状态下,轮胎的接地印痕前端凸出,后端趋近为水平线,而接地印痕前端的压力小于后端的压力。 展开更多
关键词 全钢载重子午线轮胎 接地印痕 静态加载 制动 驱动 仿真分析
下载PDF
全钢载重子午线轮胎均匀性和动平衡性能的前置管理研究
14
作者 张春生 张明 +3 位作者 王志博 纪雪华 钟声远 王啸 《橡胶工业》 CAS 2024年第10期783-788,共6页
针对12R22.5全钢载重子午线轮胎,对轮胎成型设备进行数字化升级,对轮胎均匀性和动平衡性能进行前置管理研究。将轮胎均匀性和动平衡性能管理从轮胎硫化后提前至轮胎成型时,采用胎面测长系统及其自动调节功能来控制胎面供料结构,保证胎... 针对12R22.5全钢载重子午线轮胎,对轮胎成型设备进行数字化升级,对轮胎均匀性和动平衡性能进行前置管理研究。将轮胎均匀性和动平衡性能管理从轮胎硫化后提前至轮胎成型时,采用胎面测长系统及其自动调节功能来控制胎面供料结构,保证胎面长度,并利用在线激光扫描装置扫描胎坯轮廓,控制胎坯中心径向跳动、接头质量和胎坯周长等,提高了轮胎均匀性和动平衡性能。 展开更多
关键词 全钢载重子午线轮胎 均匀性 动平衡性能 成型设备 前置管理
下载PDF
0.22+18×0.20CCST钢丝帘线在全钢载重子午线轮胎胎体中的应用
15
作者 刘勇 李光亭 +5 位作者 李明 陈立强 任淑琴 孙福忠 潘雷 安晓青 《橡胶工业》 CAS 2024年第11期844-847,共4页
研究0.22+18×0.20CCST钢丝帘线在全钢载重子午线轮胎胎体中的应用。结果表明,以0.22+18×0.20CCST钢丝帘线替代3+9+15×0.175+0.15钢丝帘线用于295/80R22.518PR全钢载重子午线轮胎胎体中,可在满足轮胎承载性能的前提下有... 研究0.22+18×0.20CCST钢丝帘线在全钢载重子午线轮胎胎体中的应用。结果表明,以0.22+18×0.20CCST钢丝帘线替代3+9+15×0.175+0.15钢丝帘线用于295/80R22.518PR全钢载重子午线轮胎胎体中,可在满足轮胎承载性能的前提下有效提高轮胎的高速性能和耐久性能,同时还能减小轮胎的质量和降低成本。 展开更多
关键词 全钢载重子午线轮胎 胎体 0.22+18×0.20CCST钢丝帘线 高速性能 耐久性能
下载PDF
全钢载重子午线轮胎肩空脱层原因分析与解决措施
16
作者 张志坚 李永建 +3 位作者 孟凡迪 李易 张思喜 刘金龙 《橡胶科技》 CAS 2024年第2期98-100,共3页
分析全钢载重子午线轮胎肩空脱层现象的原因并提出相应的解决措施。结果表明,轮胎半成品部件界面污染、部分部件厚度超差、胎肩垫胶移位、易生热、帘布渗胶性能差、轮胎选用不当等是造成全钢载重子午线轮胎肩空脱层的主要原因,通过改进... 分析全钢载重子午线轮胎肩空脱层现象的原因并提出相应的解决措施。结果表明,轮胎半成品部件界面污染、部分部件厚度超差、胎肩垫胶移位、易生热、帘布渗胶性能差、轮胎选用不当等是造成全钢载重子午线轮胎肩空脱层的主要原因,通过改进配方、优化工艺控制流程等措施,肩空脱层轮胎理赔率降低74.39%。 展开更多
关键词 全钢载重子午线轮胎 肩空 脱层
下载PDF
全钢载重子午线轮胎胎侧蛇形弯曲原因分析及解决措施
17
作者 张鹏 张建新 +1 位作者 张超 张志坚 《橡胶科技》 CAS 2024年第1期45-47,共3页
对全钢载重子午线轮胎胎侧蛇形弯曲的产生原因进行分析,并提出相应解决措施。通过采取胎侧在恒温恒湿环境下停放、调整挤出机温度匹配性、合理设定混炼胶门尼粘度标准、优化耐磨胶配方及改进胎侧终口型开型比等措施,有效解决了胎侧蛇形... 对全钢载重子午线轮胎胎侧蛇形弯曲的产生原因进行分析,并提出相应解决措施。通过采取胎侧在恒温恒湿环境下停放、调整挤出机温度匹配性、合理设定混炼胶门尼粘度标准、优化耐磨胶配方及改进胎侧终口型开型比等措施,有效解决了胎侧蛇形弯曲问题,降低了胎侧部件返工率,使成品轮胎胎圈类质量缺陷的理赔率由0.66%下降至0.21%。 展开更多
关键词 全钢载重子午线轮胎 胎侧 蛇形弯曲 胎圈
下载PDF
全钢载重子午线轮胎胎圈耐久性能试验方法的研究
18
作者 牛飞 丁纪龙 +5 位作者 高明 张乐乐 陈绪飞 王丁 郑嵩嵩 袁桂真 《橡胶科技》 CAS 2024年第4期230-232,共3页
开发一种全钢载重子午线轮胎胎圈耐久性能试验方法,并与目前应用较为普遍的2种常规试验方法进行对比分析。结果表明:采用本试验方法测试全钢载重子午线轮胎胎圈耐久性能时,对胎面进行打磨至花纹沟底0~1 mm,可有效提升轮胎肩部散热效率,... 开发一种全钢载重子午线轮胎胎圈耐久性能试验方法,并与目前应用较为普遍的2种常规试验方法进行对比分析。结果表明:采用本试验方法测试全钢载重子午线轮胎胎圈耐久性能时,对胎面进行打磨至花纹沟底0~1 mm,可有效提升轮胎肩部散热效率,试验速度和充气压力更接近目前国内载重轮胎在实际路况下的真实使用状态;与2种常规试验方法相比,本试验方法中轮胎累计行驶时间较长,试验周期较短,试验成本较低,可参考性更好。 展开更多
关键词 全钢载重子午线轮胎 胎圈 耐久性能 试验方法
下载PDF
全钢载重子午线轮胎垫胶4条挤出工艺问题原因分析及解决措施
19
作者 李光亭 李明 +3 位作者 刘勇 王三妮 赵淑霞 苟增亮 《轮胎工业》 CAS 2024年第6期370-372,共3页
分析全钢载重子午线轮胎垫胶由2条挤出变为4条挤出产生的工艺问题,并提出相应的解决措施。通过采取改造口型板、预口型及调整胶料配方适当减小垫胶粘性等措施,解决了挤出垫胶破边、宽度不一致和粘连等问题,大幅提高了垫胶半成品的尺寸... 分析全钢载重子午线轮胎垫胶由2条挤出变为4条挤出产生的工艺问题,并提出相应的解决措施。通过采取改造口型板、预口型及调整胶料配方适当减小垫胶粘性等措施,解决了挤出垫胶破边、宽度不一致和粘连等问题,大幅提高了垫胶半成品的尺寸合格率和生产效率,降低了轮胎生产成本和水电消耗。 展开更多
关键词 全钢载重子午线轮胎 垫胶 挤出机 口型 预口型
下载PDF
全钢载重子午线轮胎胎冠全息气泡的原因分析与解决措施
20
作者 柳青 杨文强 龚超 《轮胎工业》 CAS 2024年第4期242-244,共3页
分析全钢载重子午线轮胎胎冠全息气泡的产生原因,并提出相应的解决措施。成品轮胎胎冠全息气泡产生于带束层之间及胎面与带束层之间,主要原因是半成品粘性波动,滚压轨迹不合理会加剧此病象产生。通过调整胶料粘性以及优化成型装备结构... 分析全钢载重子午线轮胎胎冠全息气泡的产生原因,并提出相应的解决措施。成品轮胎胎冠全息气泡产生于带束层之间及胎面与带束层之间,主要原因是半成品粘性波动,滚压轨迹不合理会加剧此病象产生。通过调整胶料粘性以及优化成型装备结构和压合轨迹,基本可以解决此类问题。 展开更多
关键词 全钢载重子午线轮胎 胎冠 全息气泡 胎面 带束层
下载PDF