The zeta potential measurements show that the flotation separation of diaspore from kaolinite, illite and pyrophyllite could be achieved in the range of pH 46.5 with cationic collectors. A special quaternary ammonium ...The zeta potential measurements show that the flotation separation of diaspore from kaolinite, illite and pyrophyllite could be achieved in the range of pH 46.5 with cationic collectors. A special quaternary ammonium salts(DTAL) shows better selectivity than that the dodecyl amine(DDA) does for the flotation of three silicates. The closed circuit flotation results show that the reverse flotation de silicate can be achieved with DTAL as collector, a new inorganic reagent(SFL) as depressant and MIBC as frother to obtain a bauxite concentrate m (Al 2O 3)/ m (SiO 2) >10, Al 2O 3 recovery>86%).展开更多
The technological mineralogy of the potash feldspar was investigated and a new collector named Yb105 was adopted to remove iron from potash feldspar ores.The technological mineralogy results indicate that the main com...The technological mineralogy of the potash feldspar was investigated and a new collector named Yb105 was adopted to remove iron from potash feldspar ores.The technological mineralogy results indicate that the main components of the ore were feldspar,sericite,quartz and kaolinite,and iron mainly existed in limonite and hematite,most of which can be removed by beneficiation.The results show the benzohydroxamic acid can not only increase the recovery of iron and reduce the consumption of oleic acid collector,but also enhance the collecting performance of oleic acid at low temperature,which can realize the flotation of the ores at a low temperature and play an important role in saving energy to some extent.Compared with oleic oil,the benzohydroxamic acid had a great advantage in removing iron from potash feldspar,a potash feldspar concentrate with Fe grade of 0.23%,K2O grade of 12.59%and Na2O grade of 0.26%was obtained by flotation with Yb105 as collector,and the yield of the concentrate was 82.55%.展开更多
Using cetyl trimethylammonium bromide (CTAB) as collector, the flotation de-silicating from diasporic-bauxite was investigated. And the Zeta potentials and contact-angles of silicate minerals and diaspore were also ...Using cetyl trimethylammonium bromide (CTAB) as collector, the flotation de-silicating from diasporic-bauxite was investigated. And the Zeta potentials and contact-angles of silicate minerals and diaspore were also stu-(died.)The results show that in the presence of 2×10-4 mol·L-1CTAB, the surface charges of pyrophyllite, kaolinite and illite become more positive, and the contact angles of these three silicates also increase evidently in the pH range of 2-8, but the Zeta potentials and contact angles of diaspore change little. So, the floatability of the four minerals is in the following order: pyrophyllite>kaolinite≈illite>diaspore. The open-circuit flotation results also show that a bauxite concentrate with m(Al2O3)/m(SiO2) over 9.3 and Al2O3 recovery over 76% can be obtained from diasporic-bauxite ore. The result of XRD of the bauxite concentrate shows that pyrophyllite is easier to be removed from diasporic-bauxite than illite and kaolinite due to its better floatability.展开更多
文摘The zeta potential measurements show that the flotation separation of diaspore from kaolinite, illite and pyrophyllite could be achieved in the range of pH 46.5 with cationic collectors. A special quaternary ammonium salts(DTAL) shows better selectivity than that the dodecyl amine(DDA) does for the flotation of three silicates. The closed circuit flotation results show that the reverse flotation de silicate can be achieved with DTAL as collector, a new inorganic reagent(SFL) as depressant and MIBC as frother to obtain a bauxite concentrate m (Al 2O 3)/ m (SiO 2) >10, Al 2O 3 recovery>86%).
基金Project(21776320)supported by the National Natural Science Foundation of ChinaProject(2016TP1007)supported by the Hunan Provincial Science and Technology Plan Project,China
文摘The technological mineralogy of the potash feldspar was investigated and a new collector named Yb105 was adopted to remove iron from potash feldspar ores.The technological mineralogy results indicate that the main components of the ore were feldspar,sericite,quartz and kaolinite,and iron mainly existed in limonite and hematite,most of which can be removed by beneficiation.The results show the benzohydroxamic acid can not only increase the recovery of iron and reduce the consumption of oleic acid collector,but also enhance the collecting performance of oleic acid at low temperature,which can realize the flotation of the ores at a low temperature and play an important role in saving energy to some extent.Compared with oleic oil,the benzohydroxamic acid had a great advantage in removing iron from potash feldspar,a potash feldspar concentrate with Fe grade of 0.23%,K2O grade of 12.59%and Na2O grade of 0.26%was obtained by flotation with Yb105 as collector,and the yield of the concentrate was 82.55%.
文摘Using cetyl trimethylammonium bromide (CTAB) as collector, the flotation de-silicating from diasporic-bauxite was investigated. And the Zeta potentials and contact-angles of silicate minerals and diaspore were also stu-(died.)The results show that in the presence of 2×10-4 mol·L-1CTAB, the surface charges of pyrophyllite, kaolinite and illite become more positive, and the contact angles of these three silicates also increase evidently in the pH range of 2-8, but the Zeta potentials and contact angles of diaspore change little. So, the floatability of the four minerals is in the following order: pyrophyllite>kaolinite≈illite>diaspore. The open-circuit flotation results also show that a bauxite concentrate with m(Al2O3)/m(SiO2) over 9.3 and Al2O3 recovery over 76% can be obtained from diasporic-bauxite ore. The result of XRD of the bauxite concentrate shows that pyrophyllite is easier to be removed from diasporic-bauxite than illite and kaolinite due to its better floatability.