In this work,we initially synthesized Sb2S3 with uniform flower-like structures via a facile hydrothermal method through the modification of the Sb source and pH value.Afterward,Sb2S3 with a nanosheet structure was su...In this work,we initially synthesized Sb2S3 with uniform flower-like structures via a facile hydrothermal method through the modification of the Sb source and pH value.Afterward,Sb2S3 with a nanosheet structure was successfully synthesized on reduced graphene oxide(Sb2S3@RGO).The flower-like Sb2S3 and the Sb2S3@RGO nanosheets were tested as the counter electrode(CE)of dye-sensitized solar cells,and the latter exhibited a higher electrocatalytic property than the former owing to the introduction of graphene.The results from electrochemical tests indicated that the as-prepared Sb2S3@RGO nanosheets possess higher catalytic activity,charge-transfer ability,and electrochemical stability than Sb2S3,RGO,and Pt CEs.More notably,the power conversion efficiency of Sb2S3@RGO reached 8.17%,which was higher than that of the standard Pt CE(7.75%).展开更多
基金funded by the Tianjin science and technology support key projects(18YFZCSF00500)the National Science Fund for Distinguished Young Scholars(21425729)the National Natural Science Foundation of China
文摘In this work,we initially synthesized Sb2S3 with uniform flower-like structures via a facile hydrothermal method through the modification of the Sb source and pH value.Afterward,Sb2S3 with a nanosheet structure was successfully synthesized on reduced graphene oxide(Sb2S3@RGO).The flower-like Sb2S3 and the Sb2S3@RGO nanosheets were tested as the counter electrode(CE)of dye-sensitized solar cells,and the latter exhibited a higher electrocatalytic property than the former owing to the introduction of graphene.The results from electrochemical tests indicated that the as-prepared Sb2S3@RGO nanosheets possess higher catalytic activity,charge-transfer ability,and electrochemical stability than Sb2S3,RGO,and Pt CEs.More notably,the power conversion efficiency of Sb2S3@RGO reached 8.17%,which was higher than that of the standard Pt CE(7.75%).